Austenitic stainless steels

Austenitic stainless steels: material, UNS, W.Nr./EN and forms with standard
MaterialUNSW.Nr. / ENForms
304L stainless steelAustenitic stainless · Low-carbon Cr-Ni austenitic stainless steel S30403 1.4307 Bar, Plate, Pipe, Forging and flange, Fitting
310S stainless steelAustenitic stainless · Heat-resisting 25Cr-20Ni austenitic stainless steel S31008 1.4845 Bar, Plate, Pipe, Forging and flange
316Ti stainless steelAustenitic stainless · Titanium-stabilized Cr-Ni-Mo austenitic stainless steel S31635 1.4571 Bar, Plate, Pipe, Forging and flange
317L stainless steelAustenitic stainless · Low-carbon Cr-Ni-Mo (3–4% Mo) austenitic stainless steel S31703 ≈ 1.4438 Bar, Plate, Pipe, Forging and flange
321 stainless steelAustenitic stainless · Titanium-stabilized Cr-Ni austenitic stainless steel S32100 1.4541 Bar, Plate, Pipe, Forging and flange
347 stainless steelAustenitic stainless · Niobium-stabilized Cr-Ni austenitic stainless steel S34700 1.4550 Bar, Plate, Pipe, Forging and flange
F138 stainless steel (316LVM)Austenitic stainless · 18Cr-14Ni-2.5Mo austenitic stainless steel for surgical implants S31673 1.4441 Bar, Plate, Forging and flange, Wire
316 / 316L stainlessAustenitic stainless · All standards by product form S31600 1.4401, 1.4404… Bar, Plate, Pipe, Forging and flange, Fitting, Casting
Nitronic 50 (XM-19)Austenitic stainless · High-nitrogen, high-strength austenitic stainless steel S20910 Sem equivalente EN direto Bar, Plate, Pipe, Forging and flange
Nitronic 60Austenitic stainless · Galling- and wear-resistant austenitic stainless steel S21800 Sem equivalente EN direto Bar, Plate, Forging and flange, Casting, Wire

Super austenitic stainless

Super austenitic stainless: material, UNS, W.Nr./EN and forms with standard
MaterialUNSW.Nr. / ENForms
254 SMO / F44Super austenitic stainless · 6Mo super-austenitic stainless steel with nitrogen S31254 1.4547 Bar, Plate, Pipe, Forging and flange, Fitting
904L stainless steelSuper austenitic stainless · Low-carbon Ni-Cr-Mo-Cu super-austenitic stainless steel N08904 1.4539 Bar, Plate, Pipe, Forging and flange
Alloy 20 (Carpenter 20)Super austenitic stainless · Niobium-stabilized Fe-Ni-Cr-Mo-Cu alloy N08020 2.4660 Bar, Plate, Pipe, Forging and flange, Fitting
Alloy 28Super austenitic stainless · 27Cr-31Ni-3.5Mo-Cu super-austenitic stainless steel N08028 1.4563 Bar, Plate, Pipe

Duplex and super duplex

Duplex and super duplex: material, UNS, W.Nr./EN and forms with standard
MaterialUNSW.Nr. / ENForms
Duplex 2205 (F51 / S31803)Duplex · All standards by product form S31803 1.4462 X2CrNiMoN22-5-3 Bar, Plate, Pipe, Forging and flange, Fitting, Casting
Duplex S32205 / F60Duplex · All standards by product form S32205 1.4462 X2CrNiMoN22-5-3 Bar, Plate, Pipe, Forging and flange, Fitting, Casting
Ferralium 255 / F61Super duplex · 25Cr-6Ni-3.5Mo-2Cu-N super duplex stainless steel S32550 1.4507 Bar, Plate, Pipe, Forging and flange
329 stainless steelDuplex · First-generation 25Cr-4Ni-1.5Mo duplex stainless steel S32900 1.4460 Bar, Plate, Pipe, Forging and flange
Super duplex 2507 / F53 / S32750Super duplex · All standards by product form S32750 1.4410 X2CrNiMoN25-7-4 Bar, Plate, Pipe, Forging and flange, Fitting, Casting
Super duplex Zeron 100 / F55 / S32760Super duplex · All standards by product form S32760 1.4501 X2CrNiMoCuWN25-7-4 Bar, Plate, Pipe, Forging and flange, Fitting, Casting

Nickel alloys

Nickel alloys: material, UNS, W.Nr./EN and forms with standard
MaterialUNSW.Nr. / ENForms
Hastelloy B-2Nickel alloy · Nickel-molybdenum alloy for reducing acids N10665 2.4617 Bar, Plate, Pipe, Forging and flange
Hastelloy C-4Nickel alloy · Nickel-chromium-molybdenum alloy with high thermal stability N06455 2.4610 Bar, Plate, Pipe, Forging and flange
Hastelloy C-22Nickel alloy · Versatile nickel-chromium-molybdenum-tungsten alloy N06022 2.4602 Bar, Plate, Pipe, Forging and flange
Hastelloy C-276Nickel alloy · Low-carbon nickel-molybdenum-chromium-tungsten alloy N10276 2.4819 Bar, Plate, Pipe, Forging and flange
Incoloy 800HTNickel alloy · Iron-nickel-chromium alloy for creep and oxidation at high temperature N08811 1.4959 Bar, Plate, Pipe, Forging and flange
Incoloy 825Nickel alloy · Titanium-stabilized nickel-iron-chromium alloy with molybdenum and copper N08825 2.4858 Bar, Plate, Pipe, Forging and flange
Incoloy 925Nickel alloy · Precipitation-hardening Ni-Fe-Cr-Mo-Cu alloy for sour service N09925 — Bar, Pipe, Forging and flange
Inconel 600Nickel alloy · Solid-solution-strengthened nickel-chromium-iron alloy N06600 2.4816 Bar, Plate, Pipe, Forging and flange
Inconel 601Nickel alloy · Nickel-chromium-iron alloy with aluminum for high-temperature oxidation N06601 2.4851 Bar, Plate, Pipe, Forging and flange
Inconel 625 / Alloy 625Nickel alloy · All standards by product form N06625 2.4856 NiCr22Mo9Nb Bar, Plate, Pipe, Forging and flange, Fitting, Casting, Wire, Electrode
Inconel 718Nickel alloy · Precipitation-hardenable nickel-chromium superalloy N07718 2.4668 Bar, Plate, Pipe, Forging and flange
Nickel alloys – comparative overviewNickel alloy · Selection guide to the 13 nickel alloys in the Dustre portfolio N02200, N04400… 2.4066, 2.4360… Bar, Plate, Pipe, Forging and flange
Monel 400Nickel alloy · Solid-solution-strengthened nickel-copper alloy N04400 2.4360 Bar, Plate, Pipe, Forging and flange
Monel K-500Nickel alloy · Precipitation-hardenable nickel-copper alloy N05500 2.4375 Bar, Forging and flange
Nickel 200Nickel alloy · Commercially pure nickel (≥ 99.0% Ni) N02200 2.4066 Bar, Plate, Pipe, Forging and flange

Martensitic and ferritic stainless

Martensitic and ferritic stainless: material, UNS, W.Nr./EN and forms with standard
MaterialUNSW.Nr. / ENForms
AISI 403Martensitic stainless · Turbine-quality 12% Cr martensitic stainless steel S40300 ≈ 1.4006 Bar, Plate, Forging and flange, Wire
AISI 416Martensitic stainless · Free-machining (resulfurized) martensitic stainless steel S41600 1.4005 Bar, Forging and flange, Wire
AISI 431Martensitic stainless · High-strength Cr-Ni martensitic stainless steel S43100 1.4057 Bar, Plate, Forging and flange, Wire
AISI 446Ferritic stainless · Oxidation-resistant 25% Cr ferritic stainless steel S44600 ≈ 1.4749 Bar, Plate, Pipe, Forging and flange
ASTM A182 F6NMMartensitic stainless · Forged 13Cr-4Ni-Mo soft martensitic stainless steel (wrought equivalent of… S41500 1.4313 Bar, Plate, Pipe, Forging and flange, Casting

Precipitation hardening

Precipitation hardening: material, UNS, W.Nr./EN and forms with standard
MaterialUNSW.Nr. / ENForms
15-5PH – UNS S15500 (XM-12)Precipitation-hardening stainless · Martensitic precipitation-hardening stainless steel (Cr-Ni-Cu) S15500 1.4545 Bar, Plate, Forging and flange, Casting
17-7PH – UNS S17700 (Type 631)Precipitation-hardening stainless · Semi-austenitic precipitation-hardening stainless steel (Cr-Ni-Al) S17700 1.4568 Bar, Plate, Forging and flange, Wire
A-286 / Alloy 660Precipitation-hardening stainless · Precipitation-hardenable Fe-Ni-Cr superalloy S66286 1.4980 Bar, Plate, Forging and flange
17-4PH stainless steel – UNS S17400 (ASTM A564 Type 630)Precipitation-hardening stainless · Martensitic precipitation-hardening stainless steel (Cr-Ni-Cu-Nb) S17400 1.4542 Bar, Plate, Forging and flange, Casting
Maraging 250Alloy steel · Age-hardenable 18Ni(250) maraging steel K92890 1.6359 Bar, Plate, Forging and flange

Carbon and low-alloy steels

Carbon and low-alloy steels: material, UNS, W.Nr./EN and forms with standard
MaterialUNSW.Nr. / ENForms
300M steel (modified 4340)Alloy steel · Ultra-high-strength low-alloy steel: 4340 with silicon and vanadium K44220 Sem equivalente EN direto Bar, Pipe, Forging and flange, Casting
SAE 4140Alloy steel · Chromium-molybdenum low-alloy steel for quenching and tempering G41400 42CrMo4 Bar, Plate, Pipe, Forging and flange
SAE 4340Alloy steel · High-hardenability nickel-chromium-molybdenum low-alloy steel G43400 ≈ 34CrNiMo6 Bar, Plate, Pipe, Forging and flange
8550 steel – 34CrAlNi7-10 (W.Nr. 1.8550)Alloy steel · Cr-Al-Ni-Mo nitriding steel Sem UNS 1.8550 Bar, Forging and flange
ASTM A105 – Forged carbon steel for pipingCarbon steel · Carbon-manganese steel for forged flanges, fittings and valves K03504 ≈ P250GH Bar, Pipe, Forging and flange, Fitting
ASTM A182 F1Alloy steel · Forged carbon-molybdenum (C-½Mo) steel for elevated temperature K12822 ≈ 16Mo3 Plate, Pipe, Forging and flange, Fitting, Casting
ASTM A182 F5Alloy steel · Forged 5Cr-½Mo steel for high temperature and sulfidizing media K41545 X16CrMo5-1 Bar, Plate, Pipe, Forging and flange, Fitting, Casting
ASTM A182 F9Alloy steel · Forged 9Cr-1Mo steel for high temperature and sulfidizing media K90941 X11CrMo9-1 Plate, Pipe, Forging and flange, Fitting, Casting
ASTM A182 F11 Class 2Alloy steel · Forged 1¼Cr-½Mo steel for steam and elevated temperature K11572 ≈ 13CrMo4-5 Plate, Pipe, Forging and flange, Fitting, Casting
ASTM A182 F22 / P22 (2¼Cr-1Mo)Cr-Mo alloy steel · All standards by product form K21590 1.7380 10CrMo9-10 Bar, Plate, Pipe, Forging and flange, Fitting, Casting
ASTM A182 F91 Type 1Alloy steel · Modified 9Cr-1Mo-V-Nb ("P91") steel for creep K90901 X10CrMoVNb9-1 Plate, Pipe, Forging and flange, Fitting, Casting
ASTM A522 Type I – 9% Ni steelAlloy steel · Forged 9% nickel ferritic steel for cryogenic service down to −196 °C K81340 X8Ni9 Bar, Plate, Pipe, Forging and flange, Fitting
ASTM A694 F65 – High-yield steel forgingCarbon steel · Forged carbon steel for high-pressure pipeline flanges and fittings — — Pipe, Forging and flange, Fitting
SAE 9315 – AMS 6263Alloy steel · High-hardenability Ni-Cr-Mo carburizing steel G93150 ≈ 15NiCr13 Bar, Pipe, Forging and flange

Titanium

Titanium: material, UNS, W.Nr./EN and forms with standard
MaterialUNSW.Nr. / ENForms
Titanium Grade 2Titanium · Commercially pure (CP) titanium, general-purpose grade R50400 3.7035 Bar, Plate, Pipe, Forging and flange, Fitting
Titanium Grade 5 (Ti-6Al-4V)Titanium · High-strength alpha-beta titanium alloy R56400 3.7164 / 3.7165 Bar, Plate, Pipe, Forging and flange, Wire
Titanium Grade 7 (Ti-0.15Pd)Titanium · CP titanium with palladium, for reducing media and crevice corrosion R52400 3.7235 Bar, Plate, Pipe, Forging and flange, Fitting
Titanium Grade 9 (Ti-3Al-2.5V)Titanium · Medium-strength near-alpha titanium alloy, for tubing R56320 3.7194 / 3.7195 Bar, Plate, Pipe, Forging and flange, Wire

Copper and copper alloys

Copper and copper alloys: material, UNS, W.Nr./EN and forms with standard
MaterialUNSW.Nr. / ENForms
Cast aluminum bronze C95400Copper and copper alloys · Heat-treatable aluminum-iron bronze for casting C95400 Sem equivalente direto Casting
Nickel-aluminum bronze C63000Copper and copper alloys · Wrought aluminum bronze with nickel and iron (NAB) C63000 CW307G Bar, Plate, Forging and flange
SAE 660 bronzeCopper and copper alloys · High-leaded tin bronze (Cu-Sn-Pb-Zn ≈ 83-7-7-3) for bushings and bearings C93200 CuSn7Zn4Pb7-C Bar, Casting
TM23 bronze – high-lead bearing bronzeCopper and copper alloys · Cu-Pb-Zn-Sn leaded bronze (≈ 73-15-8-4) for bushings and bearing shells — — Bar, Casting
Beryllium copper C17200Copper and copper alloys · Precipitation-hardening copper alloy (≈ 2% Be) C17200 CW101C Bar, Plate, Forging and flange, Wire
Low-beryllium copper C17510Copper and copper alloys · High-conductivity precipitation-hardening copper-nickel-beryllium alloy C17510 CW110C Bar, Plate, Pipe, Forging and flange
Chromium copper C18200Copper and copper alloys · Precipitation-hardening copper with ≈ 1% Cr C18200 CW105C Bar, Forging and flange, Wire
Chromium-zirconium copper C18150Copper and copper alloys · High-conductivity precipitation-hardening copper C18150 CW106C Bar, Plate, Forging and flange
70/30 copper-nickel C71500Copper and copper alloys · Copper-nickel alloy with high marine corrosion resistance C71500 CW354H Bar, Plate, Pipe
90/10 copper-nickel C70600Copper and copper alloys · Copper-nickel alloy with iron for seawater C70600 CW352H Bar, Plate, Pipe
Naval brass C46400Copper and copper alloys · Alpha-beta brass with tin for marine use C46400 CW719R Bar, Plate, Forging and flange

Engineering plastics

Engineering plastics: material, UNS, W.Nr./EN and forms with standard
MaterialAbbreviationContinuous temp.Forms
Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filledPolyamide (nylon) · Cast polyamide 6 for large rods and sheets, bushings, sheaves and gears PA6 G (nylon cast) 100 °C Bar, Plate, Pipe, Casting, Machined part
Extruded nylon PA6 and PA66 (polyamide)Polyamide (nylon) · Extruded polyamide for bushings, gears and general-purpose engineering parts PA6 / PA66 100 °C Bar, Plate, Pipe, Machined part
PAI (Torlon® 4301) – polyamide-imideHigh-performance polymer · The strongest thermoplastic up to 260 °C, bearing grade with PTFE and graphite PAI 260 °C Bar, Plate, Pipe, Machined part
PC – polycarbonatePolycarbonate · Transparent thermoplastic with high impact strength up to about 120 °C PC 120 °C Bar, Plate, Pipe, Machined part
HDPE – high-density polyethylene (PE 300 / PE 500)Polyolefin (PE and PP) · Light, weldable, chemical-resistant polyolefin for sheets, tanks and boards PEAD (PE-HD, PE 300) 80 °C Bar, Plate, Pipe, Machined part
PEEK – polyether ether ketoneHigh-performance polymer · High-performance thermoplastic: mechanical, chemical and thermal resistance up… PEEK 260 °C Bar, Plate, Pipe, Machined part
Reinforced PEEK – GF30, CF30 and bearing gradeHigh-performance polymer · PEEK with glass fiber, carbon fiber or a sliding filler package… PEEK GF30 / CF30 / mancal 260 °C Bar, Plate, Pipe, Machined part
PEI (Ultem®) – polyetherimideHigh-performance polymer · Amber amorphous thermoplastic, stiff and flame retardant up to 170 °C PEI 170 °C Bar, Plate, Pipe, Machined part
PET-C (Ertalyte®) – semi-crystalline polyester, natural and PTFE-filledThermoplastic polyester · The engineering plastic with the highest dimensional stability and low wear in… PET-C / PET + PTFE 115 / 100 °C Bar, Plate, Pipe, Machined part
PI – polyimide (Vespel®, TECASINT, Duratron PI)High-performance polymer · The highest-temperature plastic: continuous use near 290 °C, no melting PI 290 °C Bar, Plate, Pipe, Machined part
Polyacetal (POM, Delrin®) – copolymer and homopolymerPolyacetal (POM) · Precision engineering plastic: stiff, stable and low-friction up to about 100 °C POM-C / POM-H 100 °C Bar, Plate, Pipe, Machined part
PP – polypropylene homopolymerPolyolefin (PE and PP) · Weldable, chemical-resistant polyolefin up to about 100 °C PP-H 100 °C Bar, Plate, Pipe, Machined part
PPS – polyphenylene sulfideHigh-performance polymer · High-performance plastic with dimensional stability and chemical resistance up… PPS 220 °C Bar, Plate, Pipe, Machined part
PTFE with 25% glass fiberFluoropolymer · Glass-filled PTFE: less creep and wear, keeping its chemical resistance PTFE + 25 % vidro 260 °C Bar, Plate, Pipe, Machined part
Bronze-filled PTFE (40% and 60%) – bronze TeflonFluoropolymer · Bronze-filled PTFE for guide rings, bushings and loaded hydraulic seals PTFE + bronze 260 °C Bar, Plate, Pipe, Machined part
Carbon- and graphite-filled PTFE (25% C and 15% graphite)Fluoropolymer · Carbon- or graphite-filled PTFE for sliding in water, steam and chemicals PTFE + carbono / grafite 260 °C Bar, Plate, Pipe, Machined part
Virgin PTFE (Teflon®) – polytetrafluoroethyleneFluoropolymer · Fluoropolymer with minimal friction and near-total chemical inertness, from −200… PTFE 260 °C Bar, Plate, Pipe, Machined part
PVDF – polyvinylidene fluorideFluoropolymer · Stiff, weldable fluoropolymer for the chemical industry up to 140 °C PVDF 140 °C Bar, Plate, Pipe, Machined part
UHMW – ultra-high molecular weight polyethylene (PE 1000)Polyolefin (PE and PP) · The plastic with the highest abrasion and impact resistance, up to 80 °C PE-UHMW (PE 1000) 80 °C Bar, Plate, Pipe, Machined part

Welding consumables

Welding consumables: material, UNS, W.Nr./EN and forms with standard
MaterialUNSW.Nr. / ENForms
ER70S-6Welding consumable · Wire and rod for A105 carbon steel K11140 EN ISO 14341-A: G 42 x x G3Si1 / G4Si1 Rod, Wire, Electrode
ER80S-B2Welding consumable · Wire and rod for 1¼Cr-½Mo steel (F11) K20900 EN ISO 21952-A: W/G CrMo1Si* Rod, Wire, Electrode
ER80S-B6Welding consumable · Wire and rod for 5Cr-½Mo steel (F5) S50280 EN ISO 21952-A: W/G CrMo5Si* Rod, Wire, Electrode
ER80S-B8Welding consumable · Wire and rod for 9Cr-1Mo steel (F9) S50480 EN ISO 21952-A: W/G CrMo9Si* Rod, Wire, Electrode
ER80S-D2Welding consumable · Mn-Mo wire and rod for 4140, 4340 and C-½Mo steels K10945 EN ISO 14341-A / 21952-A: G 4Mo / W 4Mo Rod, Wire, Electrode
ER90S-B3Welding consumable · Wire and rod for 2¼Cr-1Mo steel (F22) K30960 EN ISO 21952-A: W/G CrMo2Si* Rod, Wire, Electrode
ER90S-B9Welding consumable · Wire and rod for 9Cr-1Mo-V steel (F91) S50482 EN ISO 21952-A: W/G CrMo91* Rod, Wire, Electrode
ER209Welding consumable · Wire and rod for Nitronic 50 (XM-19) S20980 — Rod, Wire, Electrode
ER308LWelding consumable · Wire and rod for 304L stainless S30883 EN ISO 14343-A: W/G 19 9 L Rod, Wire, Electrode
ER309LWelding consumable · Wire and rod for stainless-to-carbon steel joints S30983 EN ISO 14343-A: W/G 23 12 L Rod, Wire, Electrode
ER310Welding consumable · Wire and rod for 310 stainless and high-temperature service S31080 EN ISO 14343-A: W/G 25 20 Rod, Wire, Electrode
ER316LWelding consumable · Wire and rod for 316L and 316Ti stainless S31683 EN ISO 14343-A: W/G 19 12 3 L Rod, Wire, Electrode
ER317LWelding consumable · Wire and rod for 317L stainless S31783 EN ISO 14343-A: W/G 18 15 3 L Rod, Wire, Electrode
ER320LRWelding consumable · Wire and rod for Alloy 20 N08022 — Rod, Wire, Electrode
ER347Welding consumable · Wire and rod for 321 and 347 stainless S34780 EN ISO 14343-A: W/G 19 9 Nb Rod, Wire, Electrode
ER383Welding consumable · Wire and rod for Alloy 28 (UNS N08028) N08028 EN ISO 14343-A: W/G 27 31 4 Cu L Rod, Wire, Electrode
ER385Welding consumable · Wire and rod for 904L stainless N08904 EN ISO 14343-A: W/G 20 25 5 Cu L Rod, Wire, Electrode
ER410Welding consumable · Wire and rod for 410/403 martensitic stainless S41080 EN ISO 14343-A: W/G 13 Rod, Wire, Electrode
ER410NiMoWelding consumable · Wire and rod for CA6NM (F6NM) martensitic stainless S41086 EN ISO 14343-A: W/G 13 4 Rod, Wire, Electrode
ER630Welding consumable · Wire and rod for 17-4PH and 15-5PH S17480 EN ISO 14343-A: W/G Z 17 4 Cu Nb* Rod, Wire, Electrode
ER2209Welding consumable · Wire and rod for duplex 2205 S39209 EN ISO 14343-A: W/G 22 9 3 N L Rod, Wire, Electrode
ER2594Welding consumable · Wire and rod for super duplex 2507 S32594* EN ISO 14343-A: W/G 25 9 4 N L Rod, Wire, Electrode
ERNi-1Welding consumable · Wire and rod for nickel 200 and 201 N02061 EN ISO 18274: S Ni 2061 Rod, Wire, Electrode
ERNiCr-3Welding consumable · Wire and rod for Inconel 600 and dissimilar joints N06082 EN ISO 18274: S Ni 6082 Rod, Wire, Electrode
ERNiCrCoMo-1Welding consumable · Wire and rod for Incoloy 800HT and Inconel 601 at high temperature N06617 EN ISO 18274: S Ni 6617 Rod, Wire, Electrode
ERNiCrMo-3Welding consumable · Wire and rod for Inconel 625 and corrosion-resistant alloys N06625 EN ISO 18274: S Ni 6625 Rod, Wire, Electrode
ERNiCrMo-4Welding consumable · Wire and rod for Hastelloy C-276 N10276 EN ISO 18274: S Ni 6276 Rod, Wire, Electrode
ERNiCrMo-7Welding consumable · Wire and rod for Hastelloy C-4 N06455 EN ISO 18274: S Ni 6455 Rod, Wire, Electrode
ERNiCrMo-10Welding consumable · Wire and rod for Hastelloy C-22 N06022 EN ISO 18274: S Ni 6022 Rod, Wire, Electrode
ERNiCu-7Welding consumable · Wire and rod for Monel 400 and K-500 N04060 EN ISO 18274: S Ni 4060 Rod, Wire, Electrode
ERNiFeCr-1Welding consumable · Wire and rod for Incoloy 825 N08065 EN ISO 18274: S Ni 8065 Rod, Wire
ERNiFeCr-2Welding consumable · Wire and rod for Inconel 718 N07718 EN ISO 18274: S Ni 7718 Rod, Wire
ERNiMo-7Welding consumable · Wire and rod for Hastelloy B-2 N10665 EN ISO 18274: S Ni 1066 Rod, Wire, Electrode
Titanium TIG filler rod – AWS A5.16 (ERTi-2 / ERTi-5 / ERTi-7 / ERTi-9)Welding consumable · Filler metal for GTAW welding of CP titanium and titanium alloys ERTi-2: R50120 ISO 24034 Wire, Rod

* Value or equivalent to be confirmed in the current edition of the standard.

About this list

Each material has a page with designations (UNS, W.Nr., EN, ABNT), ASTM/ASME standards by product form (bar, plate, pipe, forging and flange), chemical composition, mechanical and physical properties, heat treatment, welding and applications, plus the data sheet in PDF. Dustre supplies these materials as bar, plate, pipe and forging, with EN 10204 3.1 certificate.

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)