Dustre
EN
Customer area

Virgin PTFE (Teflon®) – polytetrafluoroethylene

Fluoropolymer with minimal friction and near-total chemical inertness, from −200 to 260 °C

Download data sheet (PDF)

PTFE is the plastic with the lowest friction and the highest chemical resistance available: only molten alkali metals and fluorine attack it. It works from about −200 to 260 °C and does not absorb water. On the other hand, it is soft, has high cold flow (creep) and wears quickly under load; for this reason, parts that slide under load use filled PTFE (bronze, carbon, glass). Teflon® is the Chemours trademark that became the popular name for the material.

Technical review Oct 2026 · typical values from semi-finished stock manufacturers' catalogues (23 °C, ISO/ASTM methods stated), not specification minimums; values with * to be confirmed

FamilyFluoropolymer
Continuous temperature260 °C
Density2.15 g/cm³
Dynamic friction0.1

Designations and equivalents

Designations of Virgin PTFE (Teflon®) – polytetrafluoroethylene
SystemDesignation
Abbreviation (ISO 1043) PTFE
Trade names TECAFLON PTFE (Ensinger); Fibracon PTFE virgin (Roechling); Teflon PTFE (Chemours, resin); POLYFLON PTFE (Daikin, resin)

Standards by product form

Standards for Virgin PTFE (Teflon®) – polytetrafluoroethylene
FormStandard
Granular resin (raw material) ASTM D4894
Rod and extruded shapes ASTM D1710*
Sheet and molded shapes ASTM D3293 / ASTM D3294*
Food contact FDA 21 CFR 177.1550; EU 10/2011 (depending on grade and lot)
Machined part to drawing ISO 2768 tolerance or as per drawing

Composition and filler

Pure polymer, unfilled (virgin grade)

Composition of Virgin PTFE (Teflon®) – polytetrafluoroethylene
ComponentContent
PTFE (polytetrafluoroethylene) 100%
Filler none (virgin)

Mechanical properties

Typical values from the stock-shape manufacturer's catalog, 23 °C; ISO/ASTM methods as per the source

Mechanical properties of Virgin PTFE (Teflon®) – polytetrafluoroethylene
PropertyValue
Tensile strength 22 MPa
Elongation at break 220%
Compressive strength 5 MPa
Hardness Shore D 55
Notched impact 160 J/m

Typical physical and thermal properties

Typical values at 23 °C unless stated
PropertyValue
Density 2.15 g/cm³
Maximum continuous service temperature 260 °C
Maximum short-term temperature 260 °C
Minimum service temperature -200 °C
HDT (1.8 MPa) 45 °C
Melting point or glass transition 327 °C
Linear thermal expansion 130 µm/m·K
Thermal conductivity 0.2 W/m·K
Water absorption (24 h) <0.01%
Dielectric strength 24 kV/mm
Flammability (UL 94) V-0

Calculate the weight of Virgin PTFE (Teflon®) – polytetrafluoroethylene bar, plate or pipe →

Friction, wear and PV limit

Friction and wear of Virgin PTFE (Teflon®) – polytetrafluoroethylene
PropertyValue
Dynamic coefficient of friction against steel 0.1 (dynamic at 10 ft/min (0.05 m/s), PV 8,000-10,000 psi·ft/min)
PV limit (pressure × velocity) 0.042 MPa·m/s (at 0.05 m/s (10 ft/min), unlubricated, 21-27 °C; original 1,200 psi·ft/min); 0.063 MPa·m/s (at 0.5 m/s (100 ft/min); original 1,800 psi·ft/min); 0.088 MPa·m/s (at 5 m/s (1,000 ft/min); original 2,500 psi·ft/min); 0.04 MPa·m/s (at 0.05 m/s); 0.07 MPa·m/s (at 0.5 m/s); 0.095 MPa·m/s (at 5 m/s)
Deformation under load (creep) 10% (deformation under 14 MPa load, 24 h, 23 °C (ASTM D621))
Deformation under load (creep) 14.5% (total deformation under 14 MPa, 24 h (ASTM D621))

PV and friction depend on the test method, the mating surface (steel, stainless, roughness), lubrication and each manufacturer's safety factor: compare values from the same source and confirm by testing in critical applications.

Chemical resistance

Chemical resistance of Virgin PTFE (Teflon®) – polytetrafluoroethylene at room temperature (guidance only; check concentration and temperature)
MediumResistance
Acids Excellent
Bases (alkalis) Excellent
Solvents Excellent (practically inert)
Hydrocarbons and oils Excellent
Steam and hot water Excellent (limit 260 °C)
Caution Molten alkali metals (sodium, potassium), fluorine gas and some fluorinated compounds (ClF₃, OF₂)

Compare Virgin PTFE (Teflon®) – polytetrafluoroethylene with the other plastics by application, temperature and medium →

Stock forms and sizes

  • Rod (round bar)
  • Sheet (plate)
  • Tube and bushing
  • Skived film/tape
  • Raw material: rod (round bar), sheet (plate) and tube, cut to size
  • Machined part to drawing or sample, in the same order as the metal parts
  • Lot certificate of conformity; FDA/EU 10/2011 declaration when the grade allows

Service temperature, machining and assembly

ItemUsual practice
Service temperature Continuous service up to 260 °C; minimum -200 °C (unloaded; under load, limited by HDT and creep).
Annealing (stress relief) Stress-relief annealing before finish machining of tight-tolerance parts; PTFE does not harden by heat treatment.
Bonding and welding Cannot be welded or bonded without preparation: the surface needs chemical etching (sodium naphthalene) to accept adhesive. In sealing, it is fitted by interference or pressed in.
Machining Machines easily with a sharp tool and positive rake; its high thermal expansion (ten times that of steel) requires measuring the part at room temperature and allowing clearance.

Typical applications

  • Gaskets, packings and chemical seals
  • Valve seats
  • Electrical and high-frequency insulators
  • Sliding bearing plates for bridges and structures
  • Cryogenic components
  • Low-load, low-speed bearings
  • Pipe and tank linings

Alternatives: PTFE with bronze, carbon or glass when there is load or wear; PVDF when more stiffness with good chemical resistance is needed; PEEK for high load and temperature.

Frequently asked questions

Which standards cover Virgin PTFE (Teflon®)?

Granular resin (raw material): ASTM D4894. Rod and extruded shapes: ASTM D1710*. Sheet and molded shapes: ASTM D3293 / ASTM D3294*. Food contact: FDA 21 CFR 177.1550; EU 10/2011 (depending on grade and lot). Machined part to drawing: ISO 2768 tolerance or as per drawing.

Up to what temperature can Virgin PTFE (Teflon®) be used?

Continuous service up to 260 °C; minimum -200 °C (unloaded; under load, limited by HDT and creep).

Which materials can replace Virgin PTFE (Teflon®)?

PTFE with bronze, carbon or glass when there is load or wear; PVDF when more stiffness with good chemical resistance is needed; PEEK for high load and temperature.

Are Teflon and PTFE the same thing?

Yes. PTFE (polytetrafluoroethylene) is the polymer; Teflon® is the Chemours registered trademark that became the popular name. A Teflon rod is a PTFE rod.

Why does virgin PTFE deform over time?

Because of cold flow (creep): under constant load the part deforms slowly, even at room temperature. For loaded seals and rings, use filled PTFE (bronze, carbon or glass), which deforms much less.

Can PTFE be used in contact with food?

The virgin grade can, under FDA 21 CFR 177.1550 and EU 10/2011. Ask for the lot declaration of conformity with your order.

Where to buy Virgin PTFE (Teflon®) in Brazil?

Dustre supplies Virgin PTFE (Teflon®) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

Need Virgin PTFE (Teflon®)?Rods, sheets, tubes and parts machined to drawing, with lot certificate of conformity.

Forms and stock of Virgin PTFE (Teflon®)

Dustre supplies Virgin PTFE (Teflon®) as bar, plate and pipe and tube, cut to size, with forged and machined parts to drawing (shafts, discs, rings and blocks) and a 3.1 certificate.

Not in stock at the moment: supplied to order, with lead time in the quotation.

See the full ready-to-ship stock · Request a quote for Virgin PTFE (Teflon®)

Where to buy Virgin PTFE (Teflon®) in Brazil?

Dustre supplies Virgin PTFE (Teflon®) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

See also

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)