Enter the application, the temperatures and the medium. The selector removes what cannot take it and shows the simplest plastic that works first, with data from the datasheet.

1You enter

In contact with
Requirements

2Result

First choice
–
Also suitable
–
Quote this plastic

Indicative screening based on the semi-finished product makers' catalog data. Continuous temperature without load; under load, check HDT and creep. For critical parts, confirm with our engineering team and, if needed, with a test.

The plastics in the catalog side by side

Temperature, tensile strength, friction and water absorption of each plastic (datasheet values)
MaterialContinuous (°C)Minimum (°C)Tensile (MPa)Friction against steelWater (%)FDA / V-0
UHMW – ultra-high molecular weight polyethylene (PE 1000)80-200190.120.1FDA
HDPE – high-density polyethylene (PE 300 / PE 500)80-5025–0.01FDA
PP – polypropylene homopolymer100030–0.1FDA
Extruded nylon PA6 and PA66 (polyamide)100-30790.268FDA
Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filled93-30690.147FDA
PC – polycarbonate120-50690.380.35FDA
PET-C (Ertalyte®) – semi-crystalline polyester, natural and PTFE-filled100-20760.190.5FDA
Polyacetal (POM, Delrin®) – copolymer and homopolymer100-50670.20.8FDA
Virgin PTFE (Teflon®) – polytetrafluoroethylene260-200220.10.01FDA · V-0
PTFE with 25% glass fiber260-200180.070.02V-0
Bronze-filled PTFE (40% and 60%) – bronze Teflon260-200120.06––
Carbon- and graphite-filled PTFE (25% C and 15% graphite)260-200130.060.05V-0
PVDF – polyvinylidene fluoride140–62–0.02FDA · V-0
PAI (Torlon® 4301) – polyamide-imide260-201030.21.5V-0
PEEK – polyether ether ketone260-501160.250.45FDA · V-0
Reinforced PEEK – GF30, CF30 and bearing grade260-20840.130.35V-0
PEI (Ultem®) – polyetherimide170-50127–1.25FDA · V-0
PI – polyimide (Vespel®, TECASINT, Duratron PI)290-50130–4V-0
PPS – polyphenylene sulfide220-301020.240.1FDA · V-0

Where the datasheet lists several grades, the table shows the worst case (lowest temperature and tensile strength, highest absorption) and the lowest friction.

Frequently asked questions

How does the selector choose the plastic?

It removes the materials that cannot take the maximum and minimum temperature, the chemical medium or the requirements you tick (food contact, flame, humidity, dry running). Among those that pass, it first shows the ones already used in the chosen application and then the simplest one that works: polyolefin, engineering plastic, fluoropolymer and, last, high performance.

Where do the values come from?

From each technical datasheet in the catalog, which cites the semi-finished product makers' catalogs (Ensinger, Mitsubishi Chemical Group, Daikin, Victrex and others). Where a datasheet lists several grades, the selector uses the weakest grade for temperature, tensile strength and water absorption.

Does the continuous temperature apply under load?

Not necessarily. The maximum continuous temperature is the material's ageing limit without load. Under load the limit is usually lower: check the HDT (heat deflection temperature) and creep in the material datasheet.

Which plastic for a bushing without lubrication?

Up to 100 °C, POM, PET-C with PTFE and oil-filled nylon solve most cases. Above that, PTFE with bronze or carbon and, under high load, bearing-grade PEEK or PAI (Torlon). Check the PV limit in each datasheet.

Which plastic resists almost every chemical?

PTFE (Teflon) resists practically every chemical up to 260 °C. When more stiffness is needed, PVDF (up to 140 °C) and PPS (up to 220 °C) are the usual alternatives; for acids and bases at low temperature, PP and HDPE.

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)