PEI (Ultem®) – polyetherimide

Amber amorphous thermoplastic, stiff and flame retardant up to 170 °C

Download data sheet (PDF)

Polyetherimide is an amorphous, amber-colored thermoplastic that is stiff and inherently flame retardant. It keeps its properties up to about 170 °C, withstands repeated steam sterilization and has good dielectric strength. Being amorphous, it is less solvent resistant than PEEK and is not recommended for sliding applications.

Technical review Oct 2026 · typical values from semi-finished stock manufacturers' catalogues (23 °C, ISO/ASTM methods stated), not specification minimums; values with * to be confirmed

FamilyHigh-performance polymer
Continuous temperature170 °C
Density1.28 g/cm³

Designations and equivalents

Designations of PEI (Ultem®) – polyetherimide
SystemDesignation
Abbreviation (ISO 1043) PEI
Trade names TECAPEI natural (Ensinger); Duratron U1000 PEI (MCAM); ULTEM 1000 (SABIC, resin)

Standards by product form

Standards for PEI (Ultem®) – polyetherimide
FormStandard
Rod, sheet and tube Manufacturer's specification (SABIC Ultem 1000 or equivalent)
Food contact FDA/EU compliant grades; confirm for the lot
Machined part to drawing ISO 2768 tolerance or as per drawing

Composition and filler

Nominal composition

Composition of PEI (Ultem®) – polyetherimide
ComponentContent
PEI (polyetherimide) 100% (Ultem 1000)

Mechanical properties

Typical values from the stock-shape manufacturer's catalog, 23 °C; ISO/ASTM methods as per the source

Mechanical properties of PEI (Ultem®) – polyetherimide
PropertyValue
Tensile strength 127 MPa
Modulus of elasticity (tensile) 3,200 MPa
Elongation at break 35%
Compressive strength 92 MPa
Hardness Shore D 88
Notched impact 3.5 kJ/m²

Typical physical and thermal properties

Typical values at 23 °C unless stated
PropertyValue
Density 1.28 g/cm³
Maximum continuous service temperature 170 °C
Maximum short-term temperature 200 °C
Minimum service temperature -50 °C
HDT (1.8 MPa) 195 °C
Melting point or glass transition 216 °C
Linear thermal expansion 50 µm/m·K
Thermal conductivity 0.21 W/m·K
Water absorption (24 h) 0.05-0.10%
Water absorption (saturation) 1.25%
Dielectric strength 27 kV/mm
Flammability (UL 94) V-0

Calculate the weight of PEI (Ultem®) – polyetherimide bar, plate or pipe →

Chemical resistance

Chemical resistance of PEI (Ultem®) – polyetherimide at room temperature (guidance only; check concentration and temperature)
MediumResistance
Acids Good in dilute acids
Bases (alkalis) Limited (Ensinger: resistance to hot water/bases rated negative)
Solvents Limited in chlorinated and some polar solvents (amorphous, prone to stress cracking)
Hydrocarbons and oils Good
Steam and hot water Limited under long exposure

Compare PEI (Ultem®) – polyetherimide with the other plastics by application, temperature and medium →

Stock forms and sizes

  • Rod (round bar)
  • Sheet (plate)
  • Tube and bushing
  • Film
  • Raw material: rod (round bar), sheet (plate) and tube, cut to size
  • Machined part to drawing or sample, in the same order as the metal parts
  • Lot certificate of conformity; FDA/EU 10/2011 declaration when the grade allows

Service temperature, machining and assembly

ItemUsual practice
Service temperature Continuous service up to 170 °C, short peaks up to 200 °C; minimum -50 °C (unloaded; under load, limited by HDT and creep).
Annealing (stress relief) Stress-relief annealing before precision machining.
Bonding and welding Bonding with epoxy or cyanoacrylate; ultrasonic welding.
Machining Machines well; use a compatible coolant (no chlorinated solvents).

Typical applications

  • Medical and sterilization equipment parts
  • Electrical insulators and connectors
  • Aircraft parts with flammability requirements
  • Food equipment components

Alternatives: PEEK for chemical service and sliding; PPSU when there is impact and frequent sterilization.

Frequently asked questions

Which standards cover PEI (Ultem®)?

Rod, sheet and tube: Manufacturer's specification (SABIC Ultem 1000 or equivalent). Food contact: FDA/EU compliant grades; confirm for the lot. Machined part to drawing: ISO 2768 tolerance or as per drawing.

Up to what temperature can PEI (Ultem®) be used?

Continuous service up to 170 °C, short peaks up to 200 °C; minimum -50 °C (unloaded; under load, limited by HDT and creep).

Which materials can replace PEI (Ultem®)?

PEEK for chemical service and sliding; PPSU when there is impact and frequent sterilization.

Is PEI suitable for bearings?

It is not the best choice: amorphous PEI has high wear. For sliding at high temperature, use bearing-grade PEEK or PAI.

Where to buy PEI (Ultem®) in Brazil?

Dustre supplies PEI (Ultem®) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

Need PEI (Ultem®)?Rods, sheets, tubes and parts machined to drawing, with lot certificate of conformity.

Forms and stock of PEI (Ultem®)

Dustre supplies PEI (Ultem®) as bar, plate and pipe and tube, cut to size, with forged and machined parts to drawing (shafts, discs, rings and blocks) and a 3.1 certificate.

Not in stock at the moment: supplied to order, with lead time in the quotation.

See the full ready-to-ship stock · Request a quote for PEI (Ultem®)

Where to buy PEI (Ultem®) in Brazil?

Dustre supplies PEI (Ultem®) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

See also

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)