Super austenitic stainless steels

Austenitics with much more nickel, molybdenum and nitrogen than 316L, for acids, chlorides and seawater where 316L suffers pitting or stress corrosion cracking. PREN ranges from about 28 (Alloy 20) to over 42 (254 SMO).

Super austenitic stainless steels: alloys supplied by Dustre

Forms: Bar, Plate, Pipe, Forging and flange, Fitting. Click an alloy to see standards by form, composition, properties and equivalents.

Super austenitic stainless steels: material, UNS, W.Nr./EN and forms
MaterialUNSW.Nr. / ENForms
254 SMO / F44Super austenitic stainless · 6Mo super-austenitic stainless steel with nitrogenS312541.4547Bar, Plate, Pipe, Forging and flange, Fitting
904L stainless steelSuper austenitic stainless · Low-carbon Ni-Cr-Mo-Cu super-austenitic stainless steelN089041.4539Bar, Plate, Pipe, Forging and flange
Alloy 20 (Carpenter 20)Super austenitic stainless · Niobium-stabilized Fe-Ni-Cr-Mo-Cu alloyN080202.4660Bar, Plate, Pipe, Forging and flange, Fitting
Alloy 28Super austenitic stainless · 27Cr-31Ni-3.5Mo-Cu super-austenitic stainless steelN080281.4563Bar, Plate, Pipe

Did not find the alloy? See all materials or ask the technical team.

Which alloy resists each environment

Indicative summary from the corrosive media calculator, under typical conditions. For your medium, concentration and temperature, use the calculator.

Super austenitic stainless steels: resistance in fresh water, seawater, sulfuric acid and hot air
MaterialFresh water (200 ppm Cl⁻, 25 °C)Seawater (20,000 ppm Cl⁻, 25 °C)Sulfuric acid 20 %, 40 °CAir at 800 °C
254 SMO / F44very goodvery goodvery goodnot recommended
904L stainless steelvery goodlimitedvery goodnot recommended
Alloy 20 (Carpenter 20)very goodlimitedvery good—

About super austenitic stainless steels

904L (N08904) and Alloy 20 (N08020) add copper to 20–38 % nickel and resist sulfuric and phosphoric acid. 254 SMO (S31254, forging F44) is the classic 6Mo grade, with nitrogen, for seawater and pulp bleaching. Alloy 28 (N08028) has more chromium and nickel for phosphoric acid and well tubing with H₂S. 6Mo alloys such as Alloy 926 and Alloy 31 follow the same logic, with even more molybdenum and nitrogen.

Like ordinary austenitics, they do not harden by heat treatment and are supplied solution annealed. Welding calls for overalloyed filler metal (ER385, ER320LR, ER383 or ERNiCrMo-3), so that the weld bead is not below the base metal in corrosion resistance.

See also

Frequently asked questions

904L or 254 SMO?

904L is better in sulfuric and phosphoric acid, thanks to copper. 254 SMO, with 6 % Mo and nitrogen, is better in chlorides and seawater: PREN of about 43, against about 35 for 904L.

Is a super austenitic a nickel alloy?

No. 904L, Alloy 20 and Alloy 28 get N-series UNS numbers because of their high nickel content, but they are iron based and classified as highly alloyed austenitic stainless steels.

Other families

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)