PREN calculator

PREN tells how well stainless steels, duplex and nickel alloys resist pitting in chlorides. Pick the material from the catalog or enter the composition from the certificate.

1You enter (wt. %)

2Result

PREN (Cr + 3.3 Mo + 16 N)
–
Per this material's standard
–
Talk to engineering

Typical composition = middle of the standard's ranges, taken from each material's data sheet. Use the certificate composition for the actual value.

PREN of the catalog materials

PREN from the standard composition (minimum and typical)
MaterialGroupMinimum PRENTypical PREN
Hastelloy C-276Nickel alloys68.974.5 (with W)
Hastelloy C-22Nickel alloys65.470.8 (with W)
Hastelloy C-4Nickel alloys60.267.2
Inconel 625 / Alloy 625Nickel alloys46.451.2
254 SMO / F44Stainless steels42.244.1
Super duplex 2507 / F53 / S32750Duplex37.742.7
Super duplex Zeron 100 / F55 / S32760Duplex37.941.8 (with W)
required ≥ 40 (NORSOK M-630 and manufacturer)
Ferralium 255 / F61Duplex35.239.5
Alloy 28Stainless steels35.938.6
904L stainless steelStainless steels32.236.7
Duplex S32205 / F60Duplex34.135.9
Nitronic 50 (XM-19)Stainless steels28.734.2
Duplex 2205 (F51 / S31803)Duplex30.534.1
Incoloy 825Nickel alloys27.831.4
317L stainless steelStainless steels27.931.3
Incoloy 925Nickel alloys27.830.9
329 stainless steelDuplex26.330.5
Inconel 718Nickel alloys26.229.1
Alloy 20 (Carpenter 20)Stainless steels25.628.3
AISI 446Stainless steels24.627.8
F138 stainless steel (316LVM)Stainless steels24.427.5
required ≥ 26 (Cr + 3.3 Mo, ASTM F138)
316Ti stainless steelStainless steels22.626.1
316 / 316L stainlessStainless steels22.625.3
310S stainless steelStainless steels24.025.0
Inconel 601Nickel alloys21.023.0
Incoloy 800HTNickel alloys19.021.0
Nitronic 60Stainless steels17.320.3
304L stainless steelStainless steels18.019.8
A-286 / Alloy 660Stainless steels16.818.9
321 stainless steelStainless steels17.018.8
347 stainless steelStainless steels17.018.0
17-7PH – UNS S17700 (Type 631)Stainless steels16.017.0
17-4PH stainless steel – UNS S17400 (ASTM A564 Type 630)Stainless steels15.016.3
AISI 431Stainless steels15.016.0
Inconel 600Nickel alloys14.015.5
ASTM A182 F6NMStainless steels13.215.2
15-5PH – UNS S15500 (XM-12)Stainless steels14.014.8
AISI 416Stainless steels12.014.0
AISI 403Stainless steels11.512.3

Minimum = lowest Cr, Mo, N (and W) contents of the standard; typical = middle of the ranges. Materials without chromium (Monel, nickel 200, Hastelloy B-2, copper, titanium) do not use PREN.

How to interpret

PREN: reference ranges for pitting corrosion
PRENTypical use
below 20Atmosphere and fresh water without chlorides
20 to 30Water with little chloride, mild chemicals
30 to 40Moderate chlorides, cold brine
40 or moreSeawater, hot chlorides

To choose the alloy by medium, temperature and concentration, see steel by corrosive medium. For carbon and low-alloy steel, use the carbon equivalent calculator.

Frequently asked questions

What is PREN?

PREN (Pitting Resistance Equivalent Number) estimates the resistance of stainless steels and nickel alloys to pitting corrosion in chlorides: PREN = %Cr + 3.3 × %Mo + 16 × %N. With tungsten, PRENw = %Cr + 3.3 × (%Mo + 0.5 × %W) + 16 × %N is used. The higher, the better.

What PREN is needed for seawater?

For natural seawater the usual reference is a PREN of 40 or more, such as super duplex, 6Mo and nickel alloys. Below that there is a risk of pitting and crevice corrosion, especially above 20 to 30 °C.

Minimum or typical PREN: which one to use?

The minimum comes from the lowest Cr, Mo and N contents of the standard and is what the material guarantees. The typical value uses the middle of the ranges. When the project requires a minimum PREN (for example ≥ 40 for super duplex), the value must be calculated from the heat analysis and stated on the certificate.

Does PREN apply to carbon steel?

No. PREN only makes sense for passive alloys containing chromium (stainless, duplex and nickel alloys with Cr). For carbon and low-alloy steel the useful index is the carbon equivalent, which measures weldability.

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)