Alloy 20 (Carpenter 20) – UNS N08020

Niobium-stabilized Fe-Ni-Cr-Mo-Cu alloy

Download data sheet (PDF)

Austenitic Fe-Ni-Cr alloy with Mo, Cu and Nb, developed for sulfuric acid. The high Ni (32–38%) gives high resistance to chloride stress corrosion cracking; Nb stabilizes against intergranular corrosion. Classified by ASTM as a nickel alloy (B series).

Technical review Oct 2026 · minimum values per the cited standard; physical properties are typical; values marked * to be confirmed in the standard

FamilySuper austenitic stainless
UNSN08020
W.Nr. / EN2.4660 (NiCr20CuMo)
PREN≈ 26 – 31

Designations and equivalents

Designations of Alloy 20 (Carpenter 20) – UNS N08020
SystemDesignation
UNS N08020
W.Nr./EN 2.4660 (NiCr20CuMo)
DIN NiCr20CuMo
Trade names Carpenter 20Cb-3, Incoloy 020, Nicrofer 3620 Nb
Others Alloy 20

Standards by product form

Standards for Alloy 20 (Carpenter 20) – UNS N08020
FormStandard
Bar ASTM B473 / ASME SB-473
Forging/flange ASTM B462
Plate ASTM B463
Tube ASTM B464 / B468 / B729
Fittings ASTM B366

Tolerances and HS codes

  • Forged bars (round and square): machining allowance from 2 mm (Ø 6–16 mm) to 24 mm (Ø 400–500 mm) on the diameter. E.g. Ø 100–125 mm finished: +7 mm, tolerance +6 / −0 (length up to 3,500 mm).
  • Forged discs: allowance of 4 to 9 mm on the diameter and 3 to 11 mm on the height, plus-only tolerance.
  • Cutting and machining: band saw −0 / +5 to +15 mm on length; waterjet +10 % of thickness on the diameter (min. 2 mm); machined parts −0 / +2 to +5 mm on the diameter. See the full tables (INF 002 and INF 003, the same for every alloy).
Tariff classification of Alloy 20 (Carpenter 20): NCM, HS, HTS and CN by product form
FormNCM (Brazil, 8 digits)HS (international, 6 digits)HTS (USA, 10 digits)*CN (European Union, 8 digits)*
Forged bar7222.30.007222.307222.30.00247222 30 51
Hot-rolled bar7222.11.007222.117222.11.00597222 11 11
Plate (> 10 mm, width ≥ 600 mm)7219.21.007219.217219.21.00207219 21 10
Seamless pipe7304.41.907304.417304.41.60457304 41 00
Welded pipe7306.40.007306.407306.40.50857306 40 80
Flange and fitting7307.21.007307.217307.21.50007307 21 00

Tariff class: stainless steel (by chemical composition, under the Chapter 72 Notes and Section XV Note 5). Fe-Ni-Cr alloy in which iron predominates by weight: under Section XV Note 5 and Chapter 72 Note 1(e) it is classified as stainless steel (7219, 7222, 7304), not as a Chapter 75 nickel alloy.

*: US and EU codes for reference. NCM per current legislation (General Rules of Interpretation, Notes to Chapters 72, 74 and 75 and Section XV Note 5). Confirm the final code with your customs broker according to the item size and finish. HS = first 6 digits of the NCM.

Chemical composition (%)

ASTM B473

Chemical composition of Alloy 20 (Carpenter 20) – UNS N08020, per ASTM B473
ElementRange (%)
C ≤ 0.07
Mn ≤ 2.00
P ≤ 0.045
S ≤ 0.035
Si ≤ 1.00
Cr 19.0 – 21.0
Ni 32.0 – 38.0
Mo 2.00 – 3.00
Cu 3.00 – 4.00
Nb (+Ta) 8×C – 1.00
Fe balance

Calculate the PREN of Alloy 20 (Carpenter 20) in the PREN calculator →

Mechanical properties

Stabilize annealed (ASTM B473)

Mechanical properties of Alloy 20 (Carpenter 20) – UNS N08020
PropertyValue
Yield strength (0.2%) ≥ 241 MPa
Tensile strength ≥ 551 MPa
Elongation ≥ 30%
Reduction of area ≥ 50%
Cold worked (≤ 50.8 mm) Rm ≥ 620 MPa; Rp0.2 ≥ 414 MPa; A ≥ 15%

Typical physical properties

Typical values at 20 °C
PropertyValue
Density 8.08 g/cm³
Melting range ≈ 1,357 – 1,430 °C
Modulus of elasticity ≈ 193 GPa
Thermal conductivity (20 °C) ≈ 12 W/m·K
Thermal expansion (20–100 °C) ≈ 14.7 µm/m·K

Calculate the weight of Alloy 20 (Carpenter 20) bar, plate or pipe →

Heat treatment, welding and machining

ItemUsual practice
Service temperature Corrosion service up to ≈ 425 °C (usual ASME design limit for N08020).
Heat treatment Stabilizing anneal 927 – 1,010 °C (1,700 – 1,850 °F), ≈ 30 min per inch, water cooling. Forging between ≈ 1,150 and 1,230 °C, without working below ≈ 980 °C.
Welding Good. Consumable AWS ER320LR / E320LR; for joining to Ni alloys or 316, ERNiCrMo-3.
Machining Machinability lower than carbon steel: it work hardens quickly; use sharp tools, positive rake, constant feed without 'rubbing' and abundant coolant. Behavior similar to nickel alloys.

Plan an open-die forging in Alloy 20 (Carpenter 20): reduction, slenderness and how much material to send →Simulate the cutting plan of the ingot or bar →

Filler metal for welding

The wire composition is usually not identical to the material: each page explains why.

Typical applications

  • Sulfuric acid (production, pickling, mixers)
  • Fine chemicals, pharmaceuticals and solvents
  • Plastics, synthetic rubber and explosives
  • Gas scrubbers
  • Pumps, valves and shafts in acidic media
  • Food and dyes

Alternatives: 904L for dilute sulfuric acid at lower cost; Incoloy 825 with more Ni and Mo; C-276/Hastelloy for mixed acids with chlorides and reducing agents.

Compare alloys by corrosive medium, concentration and temperature →

Alloy 20 (Carpenter 20): complete guide

What Alloy 20 is

Alloy 20 was born in the 1950s as a super-austenitic stainless steel for sulfuric acid; today ASTM classifies it among the nickel alloys, in the UNS N080xx series, although iron is still the element present in the largest amount. The niobium-stabilized version, 20Cb-3, is the only one manufactured today and is the one covered by ASTM B473 (bar) and B462 (forgings).

Chemical composition and role of the elements

Copper (3 – 4%) is the element that gives resistance to sulfuric acid, a reducing medium in which chromium alone does not protect. The high nickel (32 – 38%) stabilizes the austenite and gives practical immunity to chloride stress corrosion cracking. Molybdenum improves pitting resistance and niobium, in an amount of at least eight times the carbon, ties up the carbon and prevents sensitization in welding.

Corrosion and limits of use

Alloy 20 resists sulfuric acid at all concentrations up to about 60 °C, phosphoric acid, nitric acid and media with moderate chlorides, with a PREN of 26 to 31. It is not a heat-resisting alloy: the usual design limit is about 425 °C. For hydrochloric acid and reducing sulfuric acid, nickel-molybdenum alloys such as Hastelloy B-2 are the choice.

Applications

Pumps, valves, shafts and agitators for sulfuric acid, tanks and heat exchangers for the chemical and fertilizer industries, desulfurization equipment, pharmaceutical and food processing, pulp plant components. For severe chlorides, 904L or 254 SMO.

Supply forms and Dustre services

Round bars and blocks forged in open die, cut to size on a band saw, with rough or finish machining, solution annealing in our own furnaces and hardness, tensile and impact testing. All material is supplied with a 3.1 inspection certificate and heat traceability.

Frequently asked questions

What is the chemical composition of Alloy 20 (Carpenter 20)?

Per ASTM B473: C ≤ 0.07; Mn ≤ 2.00; P ≤ 0.045; S ≤ 0.035; Si ≤ 1.00; Cr 19.0 – 21.0.

Which standards cover Alloy 20 (Carpenter 20)?

Bar: ASTM B473 / ASME SB-473. Forging/flange: ASTM B462. Plate: ASTM B463. Tube: ASTM B464 / B468 / B729. Fittings: ASTM B366.

Up to what temperature can Alloy 20 (Carpenter 20) be used?

Corrosion service up to ≈ 425 °C (usual ASME design limit for N08020).

Which materials can replace Alloy 20 (Carpenter 20)?

904L for dilute sulfuric acid at lower cost; Incoloy 825 with more Ni and Mo; C-276/Hastelloy for mixed acids with chlorides and reducing agents.

Is Alloy 20 a stainless steel?

It started as a super-austenitic stainless for sulfuric acid, but today ASTM classifies Alloy 20 among the nickel alloys (UNS N08020), because it has 32 to 38% nickel. Iron is still the element present in the largest amount.

What is Alloy 20 used for?

Mainly for sulfuric acid equipment: pumps, valves, tanks and piping. It is also used with phosphoric acid, nitric acid and media with moderate chlorides.

Are Carpenter 20 and Alloy 20 the same alloy?

Yes. Carpenter 20 (20Cb-3) is the original trade name; Alloy 20 and UNS N08020 are the generic designations of the same alloy.

Where to buy Alloy 20 (Carpenter 20) in Brazil?

Dustre supplies Alloy 20 (Carpenter 20) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

Need Alloy 20 (Carpenter 20)?Bars, forgings and parts with EN 10204 3.1 certificate.

Forms and stock of Alloy 20 (Carpenter 20)

Dustre supplies Alloy 20 (Carpenter 20) as bar, plate, pipe and tube, forgings and flanges and fittings, cut to size, with forged and machined parts to drawing (shafts, discs, rings and blocks) and a 3.1 certificate.

In stock in Osasco/SP, Brazil: round bar from Ø 25.4 to 101.6 mm. List updated on 11/13/2026.

See the full ready-to-ship stock · Request a quote for Alloy 20 (Carpenter 20)

Where to buy Alloy 20 (Carpenter 20) in Brazil?

Dustre supplies Alloy 20 (Carpenter 20) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

See also

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)