ERNiCrMo-3 – wire and rod for Inconel 625 and corrosion-resistant alloys

Ni-22Cr-9Mo-3.5Nb filler metal, one of the most versatile on the market: it welds alloy 625, 6 % Mo super-austenitics, Alloy 825, 9 % Ni steel and dissimilar joints in general.

Technical review Oct 2026 · composition per AWS A5.14/A5.14M; values marked * to be confirmed in the current edition of the standard

ClassificationERNiCrMo-3
StandardAWS A5.14/A5.14M / ASME SFA-5.14
UNSN06625
GroupNickel alloy

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ERNiCrMo-3
Solid MIG/MAG wire (GMAW) ERNiCrMo-3
Covered electrode (SMAW) ENiCrMo-3 – AWS A5.11
Flux-cored wire (FCAW) ENiCrMo3T1-1/-4 – AWS A5.34
Submerged arc wire (SAW) ERNiCrMo-3 + flux
Designations and equivalents
DesignationValue
AWS ERNiCrMo-3
Specification AWS A5.14/A5.14M / ASME SFA-5.14
UNS N06625
Others EN ISO 18274: S Ni 6625 (NiCr22Mo9Nb); W.Nr. 2.4831
Trade designation Liga 625 / Inconel 625 (designação de material)

Chemical composition (%)

AWS A5.14 (% by mass, filler metal)
Elementwt. %
C ≤ 0.10
Cr 20.0 – 23.0
Mo 8.0 – 10.0
Nb + Ta 3.15 – 4.15
Fe ≤ 5.0
Ni ≥ 58.0
Mn ≤ 0.50
Si ≤ 0.50
Al ≤ 0.40
Ti ≤ 0.40
Cu ≤ 0.50
P ≤ 0.02
S ≤ 0.015

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 760 MPa (AWS A5.11 minimum for ENiCrMo-3, reference)
Elongation ≥ 30 % (AWS A5.11 minimum for ENiCrMo-3, reference)

Materials welded with ERNiCrMo-3

Dissimilar joints: Widely used in joints of carbon or Cr-Mo steel with stainless, of stainless with nickel alloys, in cladding of carbon steel and on super-austenitics and super duplex when a bead nobler than the base metal is required.

Why the composition differs from the base metal

To weld 6 % Mo super-austenitics (such as 254) and Alloy 825, a filler metal much more highly alloyed than the plate is used. Molybdenum segregates in the bead and would leave depleted zones; starting from 9 % Mo in a nickel matrix, the bead is at least as pitting resistant as the base metal. On 9 % Ni steel, the choice is due to cryogenic toughness and a thermal expansion close to that of steel.

Welding precautions

  • No preheating for nickel alloys and stainless; maximum interpass around 150 °C.
  • The nickel alloy pool is viscous and penetrates little: use a wider bevel, a smaller root face and place the wire at the edge of the pool.
  • TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.
  • On 9 % Ni steel, control the residual magnetism of the part (arc blow) and keep the heat input low.

Frequently asked questions

What is ERNiCrMo-3 used for?

Ni-22Cr-9Mo-3.5Nb filler metal, one of the most versatile on the market: it welds alloy 625, 6 % Mo super-austenitics, Alloy 825, 9 % Ni steel and dissimilar joints in general.

Why is the composition of ERNiCrMo-3 different from the material it welds?

To weld 6 % Mo super-austenitics (such as 254) and Alloy 825, a filler metal much more highly alloyed than the plate is used. Molybdenum segregates in the bead and would leave depleted zones; starting from 9 % Mo in a nickel matrix, the bead is at least as pitting resistant as the base metal. On 9 % Ni steel, the choice is due to cryogenic toughness and a thermal expansion close to that of steel.

Which covered electrode corresponds to ERNiCrMo-3?

ENiCrMo-3 – AWS A5.11.

What precautions apply when welding with ERNiCrMo-3?

No preheating for nickel alloys and stainless; maximum interpass around 150 °C. The nickel alloy pool is viscous and penetrates little: use a wider bevel, a smaller root face and place the wire at the edge of the pool. TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead. On 9 % Ni steel, control the residual magnetism of the part (arc blow) and keep the heat input low.

Need ERNiCrMo-3?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)