Engineering plastics

Engineering plastics (also called technical, high-performance or engineered plastics) for sliding, sealing and insulating parts and for contact with chemicals and food, as rod, sheet and tube or machined to drawing by Dustre.

Engineering plastics: materials supplied by Dustre

Forms: Bar, Plate, Pipe, Casting, Machined part. Click a material to see properties, friction and PV, chemical resistance, standards and applications.

Engineering plastics: material, abbreviation, continuous temperature and forms
MaterialAbbreviationContinuous temp.Forms
Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filledPolyamide (nylon) · Cast polyamide 6 for large rods and sheets, bushings, sheaves and gearsPA6 G (nylon cast)100 °CBar, Plate, Pipe, Casting, Machined part
Extruded nylon PA6 and PA66 (polyamide)Polyamide (nylon) · Extruded polyamide for bushings, gears and general-purpose engineering partsPA6 / PA66100 °CBar, Plate, Pipe, Machined part
PAI (Torlon® 4301) – polyamide-imideHigh-performance polymer · The strongest thermoplastic up to 260 °C, bearing grade with PTFE and graphitePAI260 °CBar, Plate, Pipe, Machined part
PC – polycarbonatePolycarbonate · Transparent thermoplastic with high impact strength up to about 120 °CPC120 °CBar, Plate, Pipe, Machined part
HDPE – high-density polyethylene (PE 300 / PE 500)Polyolefin (PE and PP) · Light, weldable, chemical-resistant polyolefin for sheets, tanks and boardsPEAD (PE-HD, PE 300)80 °CBar, Plate, Pipe, Machined part
PEEK – polyether ether ketoneHigh-performance polymer · High-performance thermoplastic: mechanical, chemical and thermal resistance up…PEEK260 °CBar, Plate, Pipe, Machined part
Reinforced PEEK – GF30, CF30 and bearing gradeHigh-performance polymer · PEEK with glass fiber, carbon fiber or a sliding filler package…PEEK GF30 / CF30 / mancal260 °CBar, Plate, Pipe, Machined part
PEI (Ultem®) – polyetherimideHigh-performance polymer · Amber amorphous thermoplastic, stiff and flame retardant up to 170 °CPEI170 °CBar, Plate, Pipe, Machined part
PET-C (Ertalyte®) – semi-crystalline polyester, natural and PTFE-filledThermoplastic polyester · The engineering plastic with the highest dimensional stability and low wear in…PET-C / PET + PTFE115 / 100 °CBar, Plate, Pipe, Machined part
PI – polyimide (Vespel®, TECASINT, Duratron PI)High-performance polymer · The highest-temperature plastic: continuous use near 290 °C, no meltingPI290 °CBar, Plate, Pipe, Machined part
Polyacetal (POM, Delrin®) – copolymer and homopolymerPolyacetal (POM) · Precision engineering plastic: stiff, stable and low-friction up to about 100 °CPOM-C / POM-H100 °CBar, Plate, Pipe, Machined part
PP – polypropylene homopolymerPolyolefin (PE and PP) · Weldable, chemical-resistant polyolefin up to about 100 °CPP-H100 °CBar, Plate, Pipe, Machined part
PPS – polyphenylene sulfideHigh-performance polymer · High-performance plastic with dimensional stability and chemical resistance up…PPS220 °CBar, Plate, Pipe, Machined part
PTFE with 25% glass fiberFluoropolymer · Glass-filled PTFE: less creep and wear, keeping its chemical resistancePTFE + 25 % vidro260 °CBar, Plate, Pipe, Machined part
Bronze-filled PTFE (40% and 60%) – bronze TeflonFluoropolymer · Bronze-filled PTFE for guide rings, bushings and loaded hydraulic sealsPTFE + bronze260 °CBar, Plate, Pipe, Machined part
Carbon- and graphite-filled PTFE (25% C and 15% graphite)Fluoropolymer · Carbon- or graphite-filled PTFE for sliding in water, steam and chemicalsPTFE + carbono / grafite260 °CBar, Plate, Pipe, Machined part
Virgin PTFE (Teflon®) – polytetrafluoroethyleneFluoropolymer · Fluoropolymer with minimal friction and near-total chemical inertness, from −200…PTFE260 °CBar, Plate, Pipe, Machined part
PVDF – polyvinylidene fluorideFluoropolymer · Stiff, weldable fluoropolymer for the chemical industry up to 140 °CPVDF140 °CBar, Plate, Pipe, Machined part
UHMW – ultra-high molecular weight polyethylene (PE 1000)Polyolefin (PE and PP) · The plastic with the highest abrasion and impact resistance, up to 80 °CPE-UHMW (PE 1000)80 °CBar, Plate, Pipe, Machined part

Did not find the material? See all materials or ask the technical team.

About engineering plastics

Each engineering plastic covers a range of temperature and load. General-purpose grades (UHMW, nylon, acetal and PET) work up to about 80 to 110 °C and solve most guides, rollers, bushings and gears. High-performance grades (PTFE, PVDF, PEEK) go from 150 to 260 °C and resist almost all chemicals; PEEK adds mechanical strength close to that of light alloys.

Fillers change the behavior: bronze, carbon, graphite and glass fiber reduce the cold flow of PTFE and raise its wear resistance; oil and MoS₂ lower the friction of cast nylon; carbon fiber and PTFE make the bearing grades of PEEK. So the right material depends on load (P), speed (V), temperature and medium more than on the trade name.

Dustre supplies the raw material (rod, sheet, tube and bushing stock) and the machined part to drawing: guide and seal rings, bushings, valve seats, scrapers, rollers and gears, in the same order as the metal parts.

See also

Frequently asked questions

Are Teflon and PTFE the same thing?

Yes. PTFE (polytetrafluoroethylene) is the polymer; Teflon® is the Chemours trademark that became the common name. Teflon rod is PTFE rod.

Which plastic replaces bronze in bushings and rings?

It depends on load, speed and temperature. PTFE with 40 to 60% bronze accepts poor lubrication and up to about 260 °C; bearing-grade PEEK takes higher load and temperature; oil-filled cast nylon solves general-purpose bushings at lower cost. Compare the PV limit on each data sheet.

Cast or extruded nylon?

Cast nylon (PA6 G) comes in large rods and plates, with less internal stress and better stability in machining. Extruded nylon (PA6 and PA66) is usual in smaller diameters. Both absorb water and change dimensions in humid environments.

Does Dustre sell only raw material or also the part?

Both: rod, sheet, tube and bushing stock cut to size, or the part machined to drawing or sample.

Other families

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)