HDPE – high-density polyethylene (PE 300 / PE 500)

Light, weldable, chemical-resistant polyolefin for sheets, tanks and boards

Download data sheet (PDF)

High-density polyethylene is light and tough, does not absorb water and resists acids, bases and salt solutions. It is weldable, so it is the basis for tanks, vats and ducts, and it is widely used for cutting boards and parts with low mechanical demands. It is not recommended for heavy wear (use UHMW) or above 80 °C.

Technical review Oct 2026 · typical values from semi-finished stock manufacturers' catalogues (23 °C, ISO/ASTM methods stated), not specification minimums; values with * to be confirmed

FamilyPolyolefin (PE and PP)
Continuous temperature80 °C
Density0.95 g/cm³

Designations and equivalents

Designations of HDPE – high-density polyethylene (PE 300 / PE 500)
SystemDesignation
Abbreviation (ISO 1043) HDPE (PE-HD, PE 300)
Trade names Polystone G (Roechling, PE-HD 300); TECAFINE HDPE (Ensinger)

Standards by product form

Standards for HDPE – high-density polyethylene (PE 300 / PE 500)
FormStandard
Sheets and rods (PE-HD and PE-UHMW) ISO 15527*
Food contact FDA 21 CFR 177.1520 (depending on grade)
Machined part to drawing ISO 2768 tolerance or as per drawing

Composition and filler

Pure polymer

Composition of HDPE – high-density polyethylene (PE 300 / PE 500)
ComponentContent
HDPE 100%

Mechanical properties

Typical values from the stock-shape manufacturer's catalog, 23 °C; ISO/ASTM methods as per the source

Mechanical properties of HDPE – high-density polyethylene (PE 300 / PE 500)
PropertyValue
Tensile strength 25 MPa
Modulus of elasticity (tensile) 1,000 MPa
Elongation at break >50%
Hardness Shore D 62
Notched impact 20 kJ/m²

Typical physical and thermal properties

Typical values at 23 °C unless stated
PropertyValue
Density 0.95 g/cm³
Maximum continuous service temperature 80 °C
Maximum short-term temperature 100 °C
Minimum service temperature -50 °C
Melting point or glass transition 131 °C
Linear thermal expansion 150-230 µm/m·K
Thermal conductivity 0.4 W/m·K
Water absorption (24 h) <0.01%
Dielectric strength >40 kV/mm
Flammability (UL 94) HB

Calculate the weight of HDPE – high-density polyethylene (PE 300 / PE 500) bar, plate or pipe →

Chemical resistance

Chemical resistance of HDPE – high-density polyethylene (PE 300 / PE 500) at room temperature (guidance only; check concentration and temperature)
MediumResistance
Acids Excellent (except strong oxidizers)
Bases (alkalis) Excellent
Solvents Good at room temperature
Hydrocarbons and oils Limited (aromatics and chlorinated solvents cause swelling)
Steam and hot water No (temperature)

Compare HDPE – high-density polyethylene (PE 300 / PE 500) with the other plastics by application, temperature and medium →

Stock forms and sizes

  • Sheet (plate)
  • Rod (round bar)
  • Weldable sheet
  • Profiles
  • Raw material: rod (round bar), sheet (plate) and tube, cut to size
  • Machined part to drawing or sample, in the same order as the metal parts
  • Lot certificate of conformity; FDA/EU 10/2011 declaration when the grade allows

Service temperature, machining and assembly

ItemUsual practice
Service temperature Continuous service up to 80 °C, short peaks up to 100 °C; minimum -50 °C (unloaded; under load, limited by HDT and creep).
Annealing (stress relief) Not usual.
Bonding and welding Welds very well by hot plate, extrusion and hot air welding.
Machining Machines easily; allow clearance for thermal expansion.

Typical applications

  • Welded tanks, vats and reservoirs
  • Cutting boards
  • Linings and chutes
  • Low-load parts in chemical or wet environments

Alternatives: UHMW for wear; PP for somewhat higher temperature and stiffness.

Frequently asked questions

Which standards cover HDPE?

Sheets and rods (PE-HD and PE-UHMW): ISO 15527*. Food contact: FDA 21 CFR 177.1520 (depending on grade). Machined part to drawing: ISO 2768 tolerance or as per drawing.

Up to what temperature can HDPE be used?

Continuous service up to 80 °C, short peaks up to 100 °C; minimum -50 °C (unloaded; under load, limited by HDT and creep).

Which materials can replace HDPE?

UHMW for wear; PP for somewhat higher temperature and stiffness.

Is HDPE suitable for chain guides?

For light loads, yes; on conveyors with wear, use UHMW, which lasts several times longer.

Where to buy HDPE in Brazil?

Dustre supplies HDPE as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

Need HDPE?Rods, sheets, tubes and parts machined to drawing, with lot certificate of conformity.

Forms and stock of HDPE

Dustre supplies HDPE as bar, plate and pipe and tube, cut to size, with forged and machined parts to drawing (shafts, discs, rings and blocks) and a 3.1 certificate.

Not in stock at the moment: supplied to order, with lead time in the quotation.

See the full ready-to-ship stock · Request a quote for HDPE

Where to buy HDPE in Brazil?

Dustre supplies HDPE as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

See also

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)