Dustre
EN
Customer area

Carbon- and graphite-filled PTFE (25% C and 15% graphite)

Carbon- or graphite-filled PTFE for sliding in water, steam and chemicals

Download data sheet (PDF)

Carbon and graphite give PTFE compressive strength, heat conduction and low wear, including in water and steam, where bronze corrodes. These fillers are almost as chemically inert as PTFE itself and less abrasive than glass fiber. Carbon and graphite combinations are common in piston rings for oil-free compressors.

Technical review Oct 2026 · typical values from semi-finished stock manufacturers' catalogues (23 °C, ISO/ASTM methods stated), not specification minimums; values with * to be confirmed

FamilyFluoropolymer
Continuous temperature260 °C
Dynamic friction25% carbon: 0.06

Designations and equivalents

Designations of Carbon- and graphite-filled PTFE (25% C and 15% graphite)
SystemDesignation
Abbreviation (ISO 1043) PTFE + carbon / graphite
Trade names Fibracon PTFE + 25% Carbon (Roechling); POLYFLON 25CAR (Daikin); Fibracon PTFE + 15% Graphite (Roechling); POLYFLON 15GR (Daikin)

Standards by product form

Standards for Carbon- and graphite-filled PTFE (25% C and 15% graphite)
FormStandard
Filled PTFE compound ASTM D4745*
Molded rod, tube and sheet Stock-shape manufacturer's specification
Machined part to drawing ISO 2768 tolerance or as per drawing

Composition and filler

Nominal composition by mass

Composition of Carbon- and graphite-filled PTFE (25% C and 15% graphite)
ComponentContent
PTFE 75% (carbon grade) or 85% (graphite grade)
Carbon (coke/fiber) 25% by mass
Graphite 15% by mass

Mechanical properties

Typical values from the stock-shape manufacturer's catalog, 23 °C (25% carbon, 15% graphite); ISO/ASTM methods as per the source

Mechanical properties of Carbon- and graphite-filled PTFE (25% C and 15% graphite)
PropertyValue
Tensile strength 25% carbon: min. 15 MPa · 15% graphite: >13 MPa
Elongation at break 25% carbon: min. 90% · 15% graphite: >180%
Compressive strength 25% carbon: 10 MPa
Hardness 25% carbon: Shore D 63 · 15% graphite: Shore D 55-59

Typical physical and thermal properties

Typical values at 23 °C unless stated
PropertyValue
Density 25% carbon: 2.10 ± 0.03 g/cm³ · 15% graphite: 2.05-2.25 g/cm³
Maximum continuous service temperature 260 °C
Minimum service temperature -200 °C
HDT (1.8 MPa) 25% carbon: 65 °C
Melting point or glass transition 327 °C
Linear thermal expansion 25% carbon: 95 µm/m·K
Thermal conductivity 25% carbon: 0.64 W/m·K
Water absorption (24 h) 25% carbon: 0.05%
Flammability (UL 94) 25% carbon: V-0

Calculate the weight of Carbon- and graphite-filled PTFE (25% C and 15% graphite) bar, plate or pipe →

Friction, wear and PV limit

Friction and wear of Carbon- and graphite-filled PTFE (25% C and 15% graphite)
PropertyValue
Dynamic coefficient of friction against steel 25% carbon: 0.06 (dynamic, 0.8 m/s, 1 MPa, against stainless steel Ra 0.5 µm)
PV limit (pressure × velocity) 25% carbon: 0.365 MPa·m/s (at 0.05 m/s); 0.46 MPa·m/s (at 0.5 m/s); 0.545 MPa·m/s (at 5 m/s)
Deformation under load (creep) 25% carbon: 5-7% (deformation under load, ASTM D621)
Deformation under load (creep) 25% carbon: 6.5% (total deformation under 14 MPa, 24 h)

PV and friction depend on the test method, the mating surface (steel, stainless, roughness), lubrication and each manufacturer's safety factor: compare values from the same source and confirm by testing in critical applications.

Chemical resistance

Chemical resistance of Carbon- and graphite-filled PTFE (25% C and 15% graphite) at room temperature (guidance only; check concentration and temperature)
MediumResistance
Acids Very good (Daikin cites resistance to hydrochloric acid)
Bases (alkalis) Very good
Solvents Very good
Hydrocarbons and oils Very good
Steam and hot water Very good; recommended for water applications (Daikin)

Compare Carbon- and graphite-filled PTFE (25% C and 15% graphite) with the other plastics by application, temperature and medium →

Stock forms and sizes

  • Rod (round bar)
  • Sheet (plate)
  • Tube and bushing
  • Molded bushings and rings
  • Raw material: rod (round bar), sheet (plate) and tube, cut to size
  • Machined part to drawing or sample, in the same order as the metal parts
  • Lot certificate of conformity; FDA/EU 10/2011 declaration when the grade allows

Service temperature, machining and assembly

ItemUsual practice
Service temperature Continuous service up to 260 °C; minimum -200 °C (unloaded; under load, limited by HDT and creep).
Annealing (stress relief) Stress-relief annealing before finish machining.
Bonding and welding Cannot be welded; bonding only after chemical etching of the surface.
Machining Machines well with carbide; carbon dust is conductive, so clean the machine.

Typical applications

  • Piston rings for oil-free compressors
  • Bushings and bearings in water, steam and chemical media
  • Pump seals
  • Guide rings in water and emulsions
  • Antistatic parts

Alternatives: Bronze-filled PTFE in oil hydraulics with high load; carbon-filled PEEK when load and temperature exceed the limits of PTFE.

Frequently asked questions

Which standards cover Carbon- and graphite-filled PTFE (25% C and 15% graphite)?

Filled PTFE compound: ASTM D4745*. Molded rod, tube and sheet: Stock-shape manufacturer's specification. Machined part to drawing: ISO 2768 tolerance or as per drawing.

Up to what temperature can Carbon- and graphite-filled PTFE (25% C and 15% graphite) be used?

Continuous service up to 260 °C; minimum -200 °C (unloaded; under load, limited by HDT and creep).

Which materials can replace Carbon- and graphite-filled PTFE (25% C and 15% graphite)?

Bronze-filled PTFE in oil hydraulics with high load; carbon-filled PEEK when load and temperature exceed the limits of PTFE.

Carbon or bronze in PTFE?

Carbon in water, steam, acids and media where bronze corrodes; bronze in hydraulic oil, with higher load and better heat conduction.

Does carbon-filled PTFE conduct electricity?

Partially: carbon fillers make PTFE dissipative, which is useful in antistatic parts. It is not an insulator like virgin PTFE.

Where to buy Carbon- and graphite-filled PTFE (25% C and 15% graphite) in Brazil?

Dustre supplies Carbon- and graphite-filled PTFE (25% C and 15% graphite) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

Need Carbon- and graphite-filled PTFE (25% C and 15% graphite)?Rods, sheets, tubes and parts machined to drawing, with lot certificate of conformity.

Forms and stock of Carbon- and graphite-filled PTFE (25% C and 15% graphite)

Dustre supplies Carbon- and graphite-filled PTFE (25% C and 15% graphite) as bar, plate and pipe and tube, cut to size, with forged and machined parts to drawing (shafts, discs, rings and blocks) and a 3.1 certificate.

Not in stock at the moment: supplied to order, with lead time in the quotation.

See the full ready-to-ship stock · Request a quote for Carbon- and graphite-filled PTFE (25% C and 15% graphite)

Where to buy Carbon- and graphite-filled PTFE (25% C and 15% graphite) in Brazil?

Dustre supplies Carbon- and graphite-filled PTFE (25% C and 15% graphite) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

See also

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)