Reinforced PEEK – GF30, CF30 and bearing grade

PEEK with glass fiber, carbon fiber or a sliding filler package (CF/PTFE/graphite)

Download data sheet (PDF)

Fillers take PEEK to another level: glass fiber (GF30) increases stiffness and stability; carbon fiber (CF30) gives even higher stiffness, better heat conduction and low wear; the bearing grade (carbon fiber, PTFE and graphite, such as TECAPEEK PVX and Ketron HPV) is designed to slide under load and at high speed without lubrication. This is the group of plastics with the highest PV limit.

Technical review Oct 2026 · typical values from semi-finished stock manufacturers' catalogues (23 °C, ISO/ASTM methods stated), not specification minimums; values with * to be confirmed

FamilyHigh-performance polymer
Continuous temperature260 °C

Designations and equivalents

Designations of Reinforced PEEK – GF30, CF30 and bearing grade
SystemDesignation
Abbreviation (ISO 1043) PEEK GF30 / CF30 / bearing grade
Trade names TECAPEEK GF30 natural (Ensinger); Ketron GF30 PEEK (MCAM); TECAPEEK CF30 black (Ensinger); Ketron CA30 PEEK (MCAM); TECAPEEK PVX black (Ensinger); Ketron HPV PEEK (MCAM)

Standards by product form

Standards for Reinforced PEEK – GF30, CF30 and bearing grade
FormStandard
Rod, sheet and tube Stock-shape manufacturer's specification
Machined part to drawing ISO 2768 tolerance or as per drawing

Composition and filler

Nominal composition by mass; the bearing grade varies by manufacturer

Composition of Reinforced PEEK – GF30, CF30 and bearing grade
ComponentContent
PEEK ≈ 70%
GF30: glass fiber 30%
CF30: carbon fiber 30%
Bearing grade: carbon fiber + PTFE + graphite ≈ 30% in total (10% each, depending on the manufacturer)

Mechanical properties

Typical values from the stock-shape manufacturer's catalog, 23 °C (GF30, CF30, bearing grade); ISO/ASTM methods as per the source

Mechanical properties of Reinforced PEEK – GF30, CF30 and bearing grade
PropertyValue
Tensile strength GF30: 113 MPa · CF30: 112 MPa · bearing grade: 84 MPa
Modulus of elasticity (tensile) GF30: 6,300 MPa · CF30: 6,000 MPa · bearing grade: 5,500 MPa
Elongation at break GF30: 5% · CF30: 10% · bearing grade: 3%
Compressive strength GF30: 120 MPa · CF30: 111 MPa · bearing grade: 102 MPa
Hardness GF30: Shore D 90 · CF30: Shore D 90 · bearing grade: Shore D 87
Notched impact GF30: 3 kJ/m² · CF30: 5 kJ/m² · bearing grade: 3 kJ/m²

Typical physical and thermal properties

Typical values at 23 °C unless stated
PropertyValue
Density GF30: 1.53 g/cm³ · CF30: 1.38 g/cm³ · bearing grade: 1.44 g/cm³
Maximum continuous service temperature 260 °C
Maximum short-term temperature 300 °C
Minimum service temperature -20 °C
HDT (1.8 MPa) GF30: 316 °C · CF30: 270 °C · bearing grade: 195 °C
Melting point or glass transition 341 °C
Linear thermal expansion GF30: 40 µm/m·K · CF30: 40 µm/m·K · bearing grade: 30 µm/m·K
Thermal conductivity GF30: 0.35 W/m·K · CF30: 0.66 W/m·K · bearing grade: 0.82 W/m·K
Water absorption (24 h) 0.02-0.03%
Water absorption (saturation) GF30: 0.35% · CF30: 0.3% · bearing grade: 0.3%
Dielectric strength GF30: 36 kV/mm
Flammability (UL 94) V-0

Calculate the weight of Reinforced PEEK – GF30, CF30 and bearing grade bar, plate or pipe →

Friction, wear and PV limit

Friction and wear of Reinforced PEEK – GF30, CF30 and bearing grade
PropertyValue
Dynamic coefficient of friction against steel GF30: 0.3 (dynamic, ASTM D3702, 40 psi (0.28 MPa), 50 ft/min (0.25 m/s)) · CF30: 0.13 (dynamic, ASTM D3702, 40 psi (0.28 MPa), 50 ft/min (0.25 m/s)) · bearing grade: 0.18-0.20 (ASTM D3702 (Ensinger USA))
PV limit (pressure × velocity) CF30: 0.876 MPa·m/s (MCAM QTM 55007, dry against steel, safety factor 4:1 already applied; original 25,000 psi·ft/min); 13.5 MPa·m/s (ASTM D3702 (Ensinger USA), no safety factor stated; original 385,000 psi·ft/min) · bearing grade: 0.701 MPa·m/s (MCAM QTM 55007, dry against steel, safety factor 4:1 already applied; original 20,000 psi·ft/min); 17.5 MPa·m/s (ASTM D3702 (Ensinger USA), no safety factor stated; original "500000" with no explicit unit, assumed psi·ft/min)

PV and friction depend on the test method, the mating surface (steel, stainless, roughness), lubrication and each manufacturer's safety factor: compare values from the same source and confirm by testing in critical applications.

Chemical resistance

Chemical resistance of Reinforced PEEK – GF30, CF30 and bearing grade at room temperature (guidance only; check concentration and temperature)
MediumResistance
Acids Good; limited in strong acids
Bases (alkalis) Good (hot alkalis can attack the glass fiber)
Solvents Very good
Hydrocarbons and oils Very good
Steam and hot water Very good

Compare Reinforced PEEK – GF30, CF30 and bearing grade with the other plastics by application, temperature and medium →

Stock forms and sizes

  • Rod (round bar)
  • Sheet (plate)
  • Tube and bushing
  • Raw material: rod (round bar), sheet (plate) and tube, cut to size
  • Machined part to drawing or sample, in the same order as the metal parts
  • Lot certificate of conformity; FDA/EU 10/2011 declaration when the grade allows

Service temperature, machining and assembly

ItemUsual practice
Service temperature Continuous service up to 260 °C, short peaks up to 300 °C; minimum -20 °C (unloaded; under load, limited by HDT and creep).
Annealing (stress relief) Stress-relief annealing before precision machining, as specified by the manufacturer.
Bonding and welding Bonding with epoxy after surface preparation; hot plate welding is possible in GF/CF grades.
Machining Fibers are abrasive: carbide or PCD tooling. CF30 and the bearing grade are conductive (dark powdery chips).

Typical applications

  • Guide rings, bushings and dry-running bearings under high load
  • Compressor piston rings and wear rings
  • Thrust washers and wear plates
  • Lightweight structural parts at high temperature
  • Replacement for bronze and babbitt in bearings

Alternatives: Bronze-filled PTFE when the load is moderate and cost matters; PAI (Torlon 4301) for even higher PV and temperature; SAE 660 bronze with good lubrication.

Frequently asked questions

Which standards cover Reinforced PEEK?

Rod, sheet and tube: Stock-shape manufacturer's specification. Machined part to drawing: ISO 2768 tolerance or as per drawing.

Up to what temperature can Reinforced PEEK be used?

Continuous service up to 260 °C, short peaks up to 300 °C; minimum -20 °C (unloaded; under load, limited by HDT and creep).

Which materials can replace Reinforced PEEK?

Bronze-filled PTFE when the load is moderate and cost matters; PAI (Torlon 4301) for even higher PV and temperature; SAE 660 bronze with good lubrication.

GF30, CF30 or bearing grade?

GF30 for stiffness and dimensional stability at lower cost; CF30 for maximum stiffness and low wear; bearing grade when the part slides under load and speed without lubrication.

Why does the PV of PEEK vary so much between catalogs?

Each manufacturer measures differently: some apply a safety factor (MCAM uses 4:1), others publish the test limit (ASTM D3702). Compare PV from the same source and confirm by testing when the application is critical.

Where to buy Reinforced PEEK in Brazil?

Dustre supplies Reinforced PEEK as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

Need Reinforced PEEK?Rods, sheets, tubes and parts machined to drawing, with lot certificate of conformity.

Forms and stock of Reinforced PEEK

Dustre supplies Reinforced PEEK as bar, plate and pipe and tube, cut to size, with forged and machined parts to drawing (shafts, discs, rings and blocks) and a 3.1 certificate.

Not in stock at the moment: supplied to order, with lead time in the quotation.

See the full ready-to-ship stock · Request a quote for Reinforced PEEK

Where to buy Reinforced PEEK in Brazil?

Dustre supplies Reinforced PEEK as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

See also

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)