Dustre
EN
Customer area

Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filled

Cast polyamide 6 for large rods and sheets, bushings, sheaves and gears

Download data sheet (PDF)

Cast nylon (polyamide 6 G, "nylon cast") is polymerized directly in the mold, which allows large rods and sheets with little internal stress. It is tough and resistant to wear and impact, and it replaces bronze and steel in bushings, sheaves, gears and guides. Oil-filled and MoS₂-filled grades reduce friction and work better without lubrication. Like all nylons, it absorbs water and changes dimensions in humid environments.

Technical review Oct 2026 · typical values from semi-finished stock manufacturers' catalogues (23 °C, ISO/ASTM methods stated), not specification minimums; values with * to be confirmed

FamilyPolyamide (nylon)
Continuous temperature100 °C

Designations and equivalents

Designations of Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filled
SystemDesignation
Abbreviation (ISO 1043) PA6 G (nylon cast)
Trade names TECAST T (Ensinger); Ertalon 6 PLA (MCAM); TECAST L (Ensinger); Nylatron LIG (MCAM, USA); Nylatron GSM (MCAM); TECAST T MO black (Ensinger)

Standards by product form

Standards for Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filled
FormStandard
Cast rod, sheet and tube Manufacturer's specification (Ertalon 6 PLA, Nylatron, TECAST, Nylotec)
Food contact FDA 21 CFR 177.1500 (natural grade)
Machined part to drawing ISO 2768 tolerance or as per drawing

Composition and filler

Nominal composition

Composition of Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filled
ComponentContent
Polyamide 6 (cast) ≈ 100% (natural)
Oil-filled grade built-in lubricating oil
MoS₂-filled grade molybdenum disulfide (≈ 1–2%)*

Mechanical properties

Typical values from the stock-shape manufacturer's catalog, 23 °C (natural, oil-filled, MoS₂-filled); ISO/ASTM methods as per the source

Mechanical properties of Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filled
PropertyValue
Tensile strength natural: 83 MPa · oil-filled: 69 MPa · MoS₂-filled: 75.8 MPa
Modulus of elasticity (tensile) natural: 3,500 MPa · oil-filled: 2,900 MPa · MoS₂-filled: 2,760 MPa
Elongation at break natural: 40% · oil-filled: 50% · MoS₂-filled: 30%
Compressive strength natural: 83 MPa · oil-filled: 76 MPa · MoS₂-filled: 96.5 MPa
Hardness natural: Shore D 83 · oil-filled: Shore D 80 · MoS₂-filled: Shore D 85
Notched impact natural: 4 kJ/m² · oil-filled: 5 kJ/m² · MoS₂-filled: 26.7 J/m

Typical physical and thermal properties

Typical values at 23 °C unless stated
PropertyValue
Density natural: 1.15 g/cm³ · oil-filled: 1.13 g/cm³ · MoS₂-filled: 1.16 g/cm³
Maximum continuous service temperature natural: 100 °C · oil-filled: 100 °C · MoS₂-filled: 93.3 °C
Maximum short-term temperature 170 °C
Minimum service temperature natural: -30 °C · MoS₂-filled: -30 °C
HDT (1.8 MPa) natural: 80 °C · oil-filled: 93.3 °C · MoS₂-filled: 93.3 °C
Melting point or glass transition natural: 215 °C · oil-filled: 218 °C · MoS₂-filled: 216 °C
Linear thermal expansion natural: 120 µm/m·K · oil-filled: 130 µm/m·K · MoS₂-filled: 90 µm/m·K
Thermal conductivity natural: 0.38 W/m·K · oil-filled: 0.37 W/m·K · MoS₂-filled: 0.3 W/m·K
Water absorption (24 h) natural: 0.2-0.4% · oil-filled: 0.2-0.4% · MoS₂-filled: 0.6%
Water absorption (saturation) natural: 6.5% · oil-filled: 6% · MoS₂-filled: 7%
Dielectric strength natural: 25 / 17 kV/mm · MoS₂-filled: 15.7 kV/mm
Flammability (UL 94) HB

Calculate the weight of Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filled bar, plate or pipe →

Friction, wear and PV limit

Friction and wear of Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filled
PropertyValue
Dynamic coefficient of friction against steel natural: 0.26 (dynamic, ASTM D3702, 40 psi (0.28 MPa), 50 ft/min (0.25 m/s)) · oil-filled: 0.14 (dynamic, dry against steel (MCAM QTM 55007)) · MoS₂-filled: 0.2 (dynamic, dry against steel (MCAM QTM 55007))
PV limit (pressure × velocity) oil-filled: 0.21 MPa·m/s (MCAM QTM 55007, dry against steel, safety factor 4:1 already applied; original 6,000 psi·ft/min) · MoS₂-filled: 0.105 MPa·m/s (MCAM QTM 55007, dry against steel, safety factor 4:1 already applied; original 3,000 psi·ft/min)

PV and friction depend on the test method, the mating surface (steel, stainless, roughness), lubrication and each manufacturer's safety factor: compare values from the same source and confirm by testing in critical applications.

Chemical resistance

Chemical resistance of Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filled at room temperature (guidance only; check concentration and temperature)
MediumResistance
Acids Limited: mineral acids attack polyamide
Bases (alkalis) Limited
Solvents Good; chlorinated solvents limited
Hydrocarbons and oils Very good (hydraulic oil OK)
Steam and hot water Limited

Compare Cast nylon (PA6 G) – natural, oil-filled and MoS₂-filled with the other plastics by application, temperature and medium →

Stock forms and sizes

  • Rod (round bar)
  • Sheet (plate)
  • Tube and bushing
  • Custom cast bushings
  • Raw material: rod (round bar), sheet (plate) and tube, cut to size
  • Machined part to drawing or sample, in the same order as the metal parts
  • Lot certificate of conformity; FDA/EU 10/2011 declaration when the grade allows

Service temperature, machining and assembly

ItemUsual practice
Service temperature Continuous service up to 100 °C, short peaks up to 170 °C; minimum -30 °C (unloaded; under load, limited by HDT and creep).
Annealing (stress relief) Stress-relief annealing of large parts before machining; condition to the service humidity when the tolerance is tight.
Bonding and welding Does not weld well; bonding is possible with specific adhesives.
Machining Machines very well; allow for swelling from moisture in bushing clearances.

Typical applications

  • Machine bushings and bearings
  • Sheaves, pulleys and wheels
  • Gears and crown wheels
  • Guides and wear strips
  • Wear plates and hammers for light crushing

Alternatives: UHMW for abrasion and humidity; POM for small precision parts; bronze-filled PTFE or PEEK for higher temperature.

Frequently asked questions

Which standards cover Cast nylon (PA6 G)?

Cast rod, sheet and tube: Manufacturer's specification (Ertalon 6 PLA, Nylatron, TECAST, Nylotec). Food contact: FDA 21 CFR 177.1500 (natural grade). Machined part to drawing: ISO 2768 tolerance or as per drawing.

Up to what temperature can Cast nylon (PA6 G) be used?

Continuous service up to 100 °C, short peaks up to 170 °C; minimum -30 °C (unloaded; under load, limited by HDT and creep).

Which materials can replace Cast nylon (PA6 G)?

UHMW for abrasion and humidity; POM for small precision parts; bronze-filled PTFE or PEEK for higher temperature.

Cast or extruded nylon?

Cast nylon (PA6 G) allows large parts and rods with less internal stress; extruded nylon (PA6 and PA66) is usual in smaller diameters.

Why did the nylon bushing seize on the shaft?

Most likely because of water absorption: nylon swells in humid environments. Calculate the clearance for the service humidity or switch to POM, PET or UHMW, which absorb almost no water.

Oil-filled or MoS₂-filled nylon?

The oil-filled grade has the lowest friction and suits bushings without lubrication; the MoS₂-filled grade improves wear and surface hardness and is common in gears and sheaves.

Where to buy Cast nylon (PA6 G) in Brazil?

Dustre supplies Cast nylon (PA6 G) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

Need Cast nylon (PA6 G)?Rods, sheets, tubes and parts machined to drawing, with lot certificate of conformity.

Forms and stock of Cast nylon (PA6 G)

Dustre supplies Cast nylon (PA6 G) as bar, plate, pipe and tube and castings, cut to size, with forged and machined parts to drawing (shafts, discs, rings and blocks) and a 3.1 certificate.

Not in stock at the moment: supplied to order, with lead time in the quotation.

See the full ready-to-ship stock · Request a quote for Cast nylon (PA6 G)

Where to buy Cast nylon (PA6 G) in Brazil?

Dustre supplies Cast nylon (PA6 G) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

See also

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)