ERNiFeCr-1 – wire and rod for Incoloy 825

Ni-Fe-Cr-Mo-Cu filler metal with titanium, with a composition close to alloy 825, for sulfuric and phosphoric acid equipment and piping with acidic media.

Technical review Oct 2026 · composition per AWS A5.14/A5.14M; values marked * to be confirmed in the current edition of the standard

ClassificationERNiFeCr-1
StandardAWS A5.14/A5.14M / ASME SFA-5.14
UNSN08065
GroupNickel alloy

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ERNiFeCr-1
Solid MIG/MAG wire (GMAW) ERNiFeCr-1
Submerged arc wire (SAW) ERNiFeCr-1 + flux
Designations and equivalents
DesignationValue
AWS ERNiFeCr-1
Specification AWS A5.14/A5.14M / ASME SFA-5.14
UNS N08065
Others EN ISO 18274: S Ni 8065 (NiFe30Cr21Mo3); W.Nr. 2.4858*
Trade designation Liga 825 / Incoloy 825 (designação de material)

Chemical composition (%)

AWS A5.14 (% by mass, filler metal)
Elementwt. %
C ≤ 0.05
Ni 38.0 – 46.0
Cr 19.5 – 23.5
Mo 2.5 – 3.5
Cu 1.50 – 3.0
Ti 0.60 – 1.2
Al ≤ 0.20
Fe ≥ 22.0
Mn ≤ 1.0
Si ≤ 0.50
P ≤ 0.03
S ≤ 0.03

Materials welded with ERNiFeCr-1

Dissimilar joints: When an 825 joint will work with aggressive chlorides, it is common to switch to ERNiCrMo-3, which has more molybdenum.

Why the composition differs from the base metal

It closely follows the chemistry of alloy 825, including the titanium that ties up the carbon. The chemistry of the wire is practically the same as alloy 825 (C ≤ 0.05 %, Ni 38–46 %); the bead is fully austenitic, like the base metal.

Welding precautions

  • No preheating; interpass below 150 °C.
  • The nickel alloy pool is viscous and penetrates little: use a wider bevel, a smaller root face and place the wire at the edge of the pool.
  • TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Frequently asked questions

What is ERNiFeCr-1 used for?

Ni-Fe-Cr-Mo-Cu filler metal with titanium, with a composition close to alloy 825, for sulfuric and phosphoric acid equipment and piping with acidic media.

Why is the composition of ERNiFeCr-1 different from the material it welds?

It closely follows the chemistry of alloy 825, including the titanium that ties up the carbon. The chemistry of the wire is practically the same as alloy 825 (C ≤ 0.05 %, Ni 38–46 %); the bead is fully austenitic, like the base metal.

What precautions apply when welding with ERNiFeCr-1?

No preheating; interpass below 150 °C. The nickel alloy pool is viscous and penetrates little: use a wider bevel, a smaller root face and place the wire at the edge of the pool. TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Need ERNiFeCr-1?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)