Steel by corrosive medium and equivalence table

Enter the medium the part works in, the concentration and the temperature. The table ranks the steels and alloys from best resistance down to "not recommended", with the standard equivalents.

1You enter

Aeration and oxidizing ions (Fe³⁺, Cu²⁺) worsen nickel-molybdenum alloys (B-2) and Monel; chlorides worsen stainless steels. B-2 values assume aerated acid; deaerated and free of Fe³⁺/Cu²⁺ it goes much further.

Source: Alleima, corrosion table: sulphuric acid; Haynes, HASTELLOY B-3 (datasheet), 2024

2Result

Most economical option with very good resistance
Duplex S32205 / F60
Alloys with good or very good resistance
10 of 15
See all options ↓

Caution: information based on various studies and literature. For a reliable answer, consult Dustre's engineering team. Small changes in the environment, such as aeration and the influence of other elements, among others, can completely change the analysis.

Resistance by alloy, with equivalents

Corrosion resistance in the chosen medium, from best to worst; within the same level, from most economical to most expensive
AlloyResistanceUNSW.Nr.ENOther namesOptions
Duplex S32205 / F60Very goodS32205 / S318031.4462X2CrNiMoN22-5-3F60, SAF 2205 (F51 = S31803)
904L stainless steelVery goodN089041.4539X1NiCrMoCu25-20-5Alloy 904L, F904L
Super duplex 2507 / F53 / S32750Very goodS327501.4410X2CrNiMoN25-7-4F53, SAF 2507
254 SMO / F44Very goodS312541.4547X1CrNiMoCuN20-18-7F44, 254 SMO
Alloy 20 (Carpenter 20)Very goodN080202.4660NiCr20CuMoCarpenter 20Cb-3, B462 N08020
Inconel 625 / Alloy 625Very goodN066252.4856NiCr22Mo9NbAlloy 625, B564 N06625
Hastelloy C-276Very goodN102762.4819NiMo16Cr15WAlloy C-276
Hastelloy B-2Very goodN106652.4617NiMo28Alloy B-2
317L stainless steelGoodS317031.4438X2CrNiMo18-15-4AISI 317L, F317L
Monel 400GoodN044002.4360NiCu30FeAlloy 400
316 / 316L stainlessLimitedS316031.4404X2CrNiMo17-12-2AISI 316L, F316L
Nickel 200LimitedN022002.4066Ni99,2Alloy 200
ASTM A105 – Forged carbon steel for pipingNot recommendedK035041.0460C22.8A105 / A350 LF2
304L stainless steelNot recommendedS304031.4307X2CrNi18-9AISI 304L, F304L
Titanium Grade 2Not recommendedR504003.7035Ti 2ASTM B348 Gr2, CP Ti

* Guidance only, based on published isocorrosion curves for pure media and reviewed in Oct 2026 medium by medium against technical literature (Nickel Institute, AMPP/NACE, TIMET, Haynes, Alleima, conference papers and journals); the source for each medium appears below the note. Within each concentration range the most aggressive condition applies. Contaminants (chlorides, fluorides, oxidizers), aeration, velocity, crevices and welds change the result. Confirm with Dustre engineering or by testing in the real medium before specifying.

Frequently asked questions

How do I read the rating?

Very good: corrosion below about 0.1 mm/year. Good: up to about 0.5 mm/year, acceptable with corrosion allowance. Limited: only for short use or with monitoring. Not recommended: rapid attack or risk of pitting and cracking.

Does pressure change the material choice?

Little, directly. It matters because it allows operation above the boiling point and because, with dissolved gases (H₂S, CO₂, O₂), it increases aggressiveness. Enter the actual operating temperature.

What is a steel equivalence table?

It is the correspondence between the designations of the same material in each system: UNS (USA), W.Nr. and EN name (Europe) and trade names. For example, 316L stainless = UNS S31603 = 1.4404 = X2CrNiMo17-12-2.

Need help choosing the alloy?Tell us the medium, the temperature and the concentration. We recommend the alloy and quote it with 3.1 certificate.
Request a quoteWhatsApp
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)