Carbon equivalent calculator

The carbon equivalent tells whether a carbon or low-alloy steel needs preheat for welding. Pick the steel from the catalog or enter the composition from the certificate.

1You enter (wt. %)

2Result

CE (IIW)
–
Pcm (Ito-Bessyo)
–
Per this steel's standard
–
Talk to engineering

Typical composition = middle of the standard's ranges; for residuals with only a maximum (Cr, Ni, Cu in A105), half the maximum. Use the certificate composition for the actual value.

Carbon equivalent of the catalog steels

CE (IIW) from the standard composition
SteelWorst-case CETypical CETypical PcmNote
ASTM A182 F10.560.370.222Good weldability
ASTM A694 F65 – High-yield steel forging0.570.280.198Good weldability
ASTM A105 – Forged carbon steel for piping0.680.390.253With supplementary S4: heat CE ≤ 0.47 (section up to 2 in) · Good weldability
ASTM A182 F11 Class 20.760.600.301High preheat and post-weld heat treatment
SAE 9315 – AMS 62630.830.730.313High preheat and post-weld heat treatment
SAE 41400.870.780.518High preheat and post-weld heat treatment
ASTM A522 Type I – 9% Ni steel0.910.740.245Outside IIW CE validity: preheat per code (P-No.)
SAE 43400.940.850.535High preheat and post-weld heat treatment
8550 steel – 34CrAlNi7-10 (W.Nr. 1.8550)0.970.860.482High preheat and post-weld heat treatment
ASTM A182 F22 / P22 (2¼Cr-1Mo)0.980.830.310High preheat and post-weld heat treatment
300M steel (modified 4340)1.050.930.612High preheat and post-weld heat treatment
ASTM A182 F51.611.280.396Outside IIW CE validity: preheat per code (P-No.)
ASTM A182 F91 Type 12.412.170.660Outside IIW CE validity: preheat per code (P-No.)
ASTM A182 F92.472.150.639Outside IIW CE validity: preheat per code (P-No.)
Maraging 2502.492.270.671Outside IIW CE validity: preheat per code (P-No.)

* Values to be confirmed in the current edition of the standard or of the applicable welding code.

Worst-case CE = all elements at the standard maximum at the same time (in practice the heat is well below); typical = middle of the ranges. Stainless, duplex, nickel alloys, titanium and copper do not use carbon equivalent: for them see the PREN calculator.

How to interpret

Carbon equivalent (IIW): weldability
CEWeldabilityPrecaution
up to 0.40GoodUsually no preheat needed
0.40 to 0.45FairPreheat depending on thickness
0.45 to 0.60Needs controlPreheat, low-hydrogen electrode
above 0.60DifficultHigh preheat and post-weld heat treatment

Reference ranges. The preheat temperature also depends on thickness, consumable hydrogen and joint restraint (AWS D1.1 Annex H, EN 1011-2).

Frequently asked questions

What is carbon equivalent?

It is a weldability index for carbon and low-alloy steel: it adds up the effect of carbon and alloying elements on hardening of the heat-affected zone. IIW formula: CE = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15. Up to 0.40 welding usually needs no preheat; above 0.45 preheat and hydrogen control are required.

Which materials use carbon equivalent?

Carbon steel (A105, A350 LF2), hardenable low-alloy steels (4140, 4340, 9315) and low-chromium Cr-Mo (F1, F11, F22). For 5Cr, 9Cr, F91 and 9 % Ni steels the IIW CE falls outside its validity range: preheat follows the code (ASME B31.3 and Section VIII) by P-Number. Stainless, duplex and nickel alloys do not use CE.

Does A105 have a carbon equivalent limit?

When the purchaser orders supplementary requirement S4 (Carbon Equivalent) of ASTM A105 / ASME SA-105, the heat analysis CE, by the IIW formula, is limited to 0.47 for sections up to 2 in (50.8 mm) and to 0.48 above that. A lower limit, such as 0.43, may be agreed between purchaser and supplier (S4.3). Without S4 in the order, the standard does not limit CE.

When to use Pcm instead of CE?

For steels with carbon up to about 0.12 %, such as modern pipeline and structural steels. Pcm (Ito-Bessyo) gives more weight to carbon and boron. Usual limit: up to 0.20 to 0.25*.

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)