ASTM A182 F11 Class 2 – UNS K11572

Forged 1¼Cr-½Mo steel for steam and elevated temperature

Download data sheet (PDF)

Cr-Mo steel with 1.0–1.5% Cr and 0.5% Mo, forged to ASTM A182, in three strength classes (Cl.1, Cl.2 and Cl.3). Class 2 is the most traded for flanges and fittings of steam and refinery lines up to ≈ 550 °C.

Technical review Oct 2026 · minimum values per the cited standard; physical properties are typical; values marked * to be confirmed in the standard

FamilyAlloy steel
UNSK11572 (Cl.2/3); K11597 (Cl.1)
W.Nr. / EN≈ 13CrMo4-5 – 1.7335 (EN 10222-2)
Carbon equivalent (IIW)≈ 0.60 (Cl.2, nominal composition)

Designations and equivalents

Designations of ASTM A182 F11 Class 2 – UNS K11572
SystemDesignation
UNS K11572 (Cl.2/3); K11597 (Cl.1)
W.Nr./EN ≈ 13CrMo4-5 – 1.7335 (EN 10222-2)
DIN 13CrMo44 (old)
JIS SFVAF11A (JIS G3203)
Trade names 1¼Cr-½Mo, F11
Others Pipe A335 P11; plate A387 Gr 11; fittings A234 WP11; casting A217 WC6

Standards by product form

Standards for ASTM A182 F11 Class 2 – UNS K11572
FormStandard
Forging (flanges, fittings, valves) ASTM A182/A182M F11 Cl.1/2/3; ASME SA-182
Larger forgings ASTM A336 F11
Pipe/tube ASTM A335 P11 / A213 T11
Plate ASTM A387 Gr 11
Butt-welding fittings ASTM A234 WP11
Casting ASTM A217 WC6

Tolerances and HS codes

  • Forged bars (round and square): machining allowance from 2 mm (Ø 6–16 mm) to 24 mm (Ø 400–500 mm) on the diameter. E.g. Ø 100–125 mm finished: +7 mm, tolerance +6 / −0 (length up to 3,500 mm).
  • Forged discs: allowance of 4 to 9 mm on the diameter and 3 to 11 mm on the height, plus-only tolerance.
  • Cutting and machining: band saw −0 / +5 to +15 mm on length; waterjet +10 % of thickness on the diameter (min. 2 mm); machined parts −0 / +2 to +5 mm on the diameter. See the full tables (INF 002 and INF 003, the same for every alloy).
Tariff classification of ASTM A182 F11 Class 2: NCM, HS, HTS and CN by product form
FormNCM (Brazil, 8 digits)HS (international, 6 digits)HTS (USA, 10 digits)*CN (European Union, 8 digits)*
Forged bar7228.40.007228.407228.40.00007228 40 90
Plate (> 10 mm, width ≥ 600 mm)7225.40.907225.407225.40.30507225 40 40
Seamless pipe7304.19.007304.197304.19.50507304 19 10
Welded pipe7306.19.007306.197306.19.51507306 19 00
Flange and fitting7307.91.007307.917307.91.50307307 91 00

Tariff class: alloy steel (by chemical composition, under the Chapter 72 Notes and Section XV Note 5).

Pipe: 7304.19 and 7306.19 are line pipe for oil and gas pipelines; boiler, heat exchanger or process tubes go under 7304.39/7304.59 (seamless) and 7306.30/7306.50 (welded).

*: US and EU codes for reference. NCM per current legislation (General Rules of Interpretation, Notes to Chapters 72, 74 and 75 and Section XV Note 5). Confirm the final code with your customs broker according to the item size and finish. HS = first 6 digits of the NCM.

Chemical composition (%)

ASTM A182/A182M – F11 Class 2 (Cl.1: C 0.05–0.15; Mn 0.30–0.60; P, S ≤ 0.030)

Chemical composition of ASTM A182 F11 Class 2 – UNS K11572, per ASTM A182/A182M – F11 Class 2 (Cl.1: C 0.05–0.15; Mn 0.30–0.60; P, S ≤ 0.030)
ElementRange (%)
C 0.10 – 0.20
Mn 0.30 – 0.80
P ≤ 0.040
S ≤ 0.040
Si 0.50 – 1.00
Cr 1.00 – 1.50
Mo 0.44 – 0.65

Calculate the carbon equivalent of ASTM A182 F11 Class 2 for welding →

Mechanical properties

Normalized + tempered – ASTM A182 F11 (Cl.1 / Cl.2 / Cl.3)

Mechanical properties of ASTM A182 F11 Class 2 – UNS K11572
PropertyValue
Yield strength (0.2%) Cl.1 ≥ 205 / Cl.2 ≥ 275 / Cl.3 ≥ 310 MPa
Tensile strength Cl.1 ≥ 415 / Cl.2 ≥ 485 / Cl.3 ≥ 515 MPa
Elongation ≥ 20%
Reduction of area Cl.1 ≥ 45% / Cl.2 and 3 ≥ 30%
Hardness Cl.1 121–174 / Cl.2 143–207 / Cl.3 156–207 HBW

Typical physical properties

Typical values at 20 °C
PropertyValue
Density 7.85 g/cm³
Modulus of elasticity ≈ 205 GPa
Thermal conductivity (20 °C) ≈ 41 W/m·K (typical)
Thermal expansion (20–100 °C) ≈ 11.9 µm/m·K (typical)

Calculate the weight of ASTM A182 F11 Class 2 bar, plate or pipe →

Heat treatment, welding and machining

ItemUsual practice
Service temperature Up to ≈ 550–595 °C in continuous service (creep); ASME allows up to 649 °C with reduced stresses.
Heat treatment Annealing or normalizing (≈ 900–960 °C) + tempering ≥ 620 °C (usually 650–730 °C). Cl.3 may be quenched and tempered.
Welding Preheat ≈ 150 °C, consumable AWS E8018-B2 / E8015-B2 (A5.5), ER80S-B2 (A5.28); PWHT ≈ 650–730 °C according to thickness and code.
Machining Good in the normalized and tempered condition.

Plan an open-die forging in ASTM A182 F11 Class 2: reduction, slenderness and how much material to send →Simulate the cutting plan of the ingot or bar →

Filler metal for welding

The wire composition is usually not identical to the material: each page explains why.

Typical applications

  • Flanges and fittings for boiler and power plant steam lines
  • Hot refinery and petrochemical piping
  • Steam valve bodies
  • Vessel and exchanger nozzles in A387 Gr 11
  • Moderate hydrogen service (Nelson)

Alternatives: F22 for higher temperature/pressure; F1 is obsolete for the same use; A105 below ≈ 425 °C; F91 for supercritical power plants.

ASTM A182 F11 Class 2: complete guide

What ASTM A182 F11 steel is

F11 is the first chromium-molybdenum grade in the ASTM A182 series of high-temperature alloy steels, above F1 (C-½Mo) and below F22 (2¼Cr-1Mo). It is the forged version of A335 P11 pipe. It exists in three classes with the same chemical base and different strength levels; Class 2 is the most used.

Chemical composition and role of the elements

Chromium (1.00 – 1.50%) improves resistance to oxidation by steam and stabilizes the carbides; molybdenum (0.44 – 0.65%) increases creep resistance. There is no "sum of alloying elements up to 6%" rule: the 5% limit that separates low- and high-alloy steels is only a classification convention, with no normative value.

Mechanical properties

In the normalized and tempered condition Class 2 requires a minimum yield strength of 275 MPa, minimum tensile strength of 485 MPa, minimum elongation of 20%, minimum reduction of area of 30% and hardness between 143 and 207 HBW. Class 1 is softer (UTS ≥ 415 MPa) and Class 3 stronger (UTS ≥ 515 MPa).

Heat treatment

Normalizing and tempering, or quenching and tempering, with a minimum tempering temperature of 620 °C. Dustre performs the cycle in its own furnaces, with temperature records, as part of its heat treatment service.

Applications

Flanges, fittings, valves and headers for steam lines, boilers and low-temperature superheaters, refinery and petrochemical vessels and piping up to about 550 °C. It is not a material for surgical instruments, springs or automotive parts: those applications use other steels.

Supply forms and Dustre services

Round bars and blocks forged in open die, cut to size on a band saw, with rough or finish machining, heat treatment in our own furnaces and hardness, tensile and impact testing. All material is supplied with a 3.1 inspection certificate and heat traceability.

Frequently asked questions

What is the chemical composition of ASTM A182 F11 Class 2?

Per ASTM A182/A182M – F11 Class 2 (Cl.1: C 0.05–0.15; Mn 0.30–0.60; P, S ≤ 0.030): C 0.10 – 0.20; Mn 0.30 – 0.80; P ≤ 0.040; S ≤ 0.040; Si 0.50 – 1.00; Cr 1.00 – 1.50.

Which standards cover ASTM A182 F11 Class 2?

Forging (flanges, fittings, valves): ASTM A182/A182M F11 Cl.1/2/3; ASME SA-182. Larger forgings: ASTM A336 F11. Pipe/tube: ASTM A335 P11 / A213 T11. Plate: ASTM A387 Gr 11. Butt-welding fittings: ASTM A234 WP11. Casting: ASTM A217 WC6.

Up to what temperature can ASTM A182 F11 Class 2 be used?

Up to ≈ 550–595 °C in continuous service (creep); ASME allows up to 649 °C with reduced stresses.

Which materials can replace ASTM A182 F11 Class 2?

F22 for higher temperature/pressure; F1 is obsolete for the same use; A105 below ≈ 425 °C; F91 for supercritical power plants.

Where to buy ASTM A182 F11 Class 2 in Brazil?

Dustre supplies ASTM A182 F11 Class 2 as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

Need ASTM A182 F11 Class 2?Bars, forgings and parts with EN 10204 3.1 certificate.

Forms and stock of ASTM A182 F11 Class 2

Dustre supplies ASTM A182 F11 Class 2 as plate, pipe and tube, forgings and flanges, fittings and castings, cut to size, with forged and machined parts to drawing (shafts, discs, rings and blocks) and a 3.1 certificate.

In stock in Osasco/SP, Brazil: square bar from 485 mm and round bar from Ø 26 to 280 mm. List updated on 11/13/2026.

See the full ready-to-ship stock · Request a quote for ASTM A182 F11 Class 2

Where to buy ASTM A182 F11 Class 2 in Brazil?

Dustre supplies ASTM A182 F11 Class 2 as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

See also

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)