Dustre
EN
Customer area

Forging and testing standards: NDT, mechanical and corrosion

The forging standard sets the composition, treatment and properties. The testing standards say how to verify: NDT looks for internal and surface defects; mechanical and corrosion tests confirm the properties.

Technical review Oct 2026 · Sources: ASTM A105, A182, A262, A350, A370, A388, A694, A788, A923, B381, B564, E10, E165, E709, G48, EN 10222, EN 10228, EN 10250, ISO 6892-1, ISO 148-1

Forging standards

Product standards for forgings
StandardScope
ASTM A788General requirements for steel forgings
ASTM A105Carbon steel forgings for piping components
ASTM A182Alloy and stainless steel forgings for piping: F11, F22, F91, F316L, F51, F53, F55
ASTM A350Carbon and alloy steel forgings with Charpy for low temperature (LF2, LF3)
ASTM A694High-strength forgings for transmission service (F42 to F70)
ASTM B564Nickel alloy forgings (625, 718, 825, C-276)
ASTM B381Titanium forgings
EN 10250Open-die steel forgings for general use (parts 1 to 4)
EN 10222Steel forgings for pressure equipment (parts 1 to 5)

Non-destructive testing (NDT)

NDT standards applied to forgings
StandardTest
ASTM A388Ultrasonic examination of steel forgings
EN 10228-1 / -2Magnetic particle / liquid penetrant on forgings
EN 10228-3 / -4Ultrasonic testing of ferritic and martensitic / austenitic and duplex forgings
ASTM E709 / E1444Magnetic particle
ASTM E165 / E1417Liquid penetrant

Mechanical and corrosion tests

Destructive and corrosion testing standards
StandardTest
ASTM A370 / E8 / ISO 6892-1Tensile: yield strength, tensile strength and elongation
ASTM A370 / E23 / ISO 148-1Charpy impact, including at low temperature
ASTM E10, E18, E92Brinell, Rockwell and Vickers hardness
ASTM A923Intermetallic phases in duplex and super duplex
ASTM G48Pitting and crevice corrosion in ferric chloride (CPT/CCT)
ASTM A262Intergranular corrosion in austenitic stainless
ASTM E1476 / E1916Positive material identification (PMI)

In practice

  • Forging reduction: starting from cast material (ingot), the usual minimum is 3:1. Starting from already rolled or forged bar, the new forging only changes the shape. See the forging calculator.
  • Ultrasonic testing: define the standard and the quality class in the order; without that there is no acceptance criterion.
  • Dustre laboratory: PMI, tensile, hardness and Charpy. See the testing laboratory.

Frequently asked questions

What is the difference between ASTM A182 and A105?

A105 is for carbon steel only. A182 covers alloy steels (F11, F22, F91), stainless (F304L, F316L) and duplex (F51, F53, F55) for the same piping applications.

Does every forging need ultrasonic testing?

No. Ultrasonic testing is required by the customer specification, by the equipment standard or on critical parts. When requested, the standard (e.g. ASTM A388) and the acceptance criterion must be stated in the order.

Certified forgingsWe forge stainless, duplex, nickel, titanium and alloy steels with testing.
Request a quote
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)