Dustre
EN
Customer area

300M steel (modified 4340) – UNS K44220

Ultra-high-strength low-alloy steel: 4340 with silicon and vanadium

Download data sheet (PDF)

Ni-Cr-Mo low-alloy steel derived from SAE 4340, with added silicon (1.45 – 1.80%) and vanadium (0.05 – 0.10%), vacuum melted. Oil quenched and tempered at ≈ 300 °C, it reaches 1,900 – 2,100 MPa tensile strength with better toughness, ductility and fatigue strength than 4340 at the same level. It is the classic landing gear steel. It is not a carbon steel: it contains about 5% total alloying elements.

Technical review Oct 2026 · minimum values per the cited standard; physical properties are typical; values marked * to be confirmed in the standard

FamilyAlloy steel
UNSK44220
W.Nr. / ENNo direct EN equivalent (BS S155 in the UK)
Tensile strength1,900 – 2,100 MPa

Designations and equivalents

Designations of 300M steel (modified 4340) – UNS K44220
SystemDesignation
UNS K44220
W.Nr./EN No direct EN equivalent (BS S155 in the UK)
Trade names 300M, modified 4340 (4340 Mod, E4340 Mod), 434M, Lescalloy 300M VAC-ARC
Others AMS 6257, AMS 6417, AMS 6419; MIL-S-8844 Class 3 and MIL-S-83135 (superseded by the AMS); BMS 7-26; ASTM A646

Standards by product form

Standards for 300M steel (modified 4340) – UNS K44220
FormStandard
Bar and forging (normalized and tempered) AMS 6257 (supersedes MIL-S-8844 Class 3)
Vacuum-melted bar, forging and tube (VAR) AMS 6417 (supersedes MIL-S-83135)
Bar, forging and tube AMS 6419
Aircraft-quality cleanliness AMS 2300
Bloom and billet for aerospace forgings ASTM A646

Tolerances and HS codes

  • Forged bars (round and square): machining allowance from 2 mm (Ø 6–16 mm) to 24 mm (Ø 400–500 mm) on the diameter. E.g. Ø 100–125 mm finished: +7 mm, tolerance +6 / −0 (length up to 3,500 mm).
  • Forged discs: allowance of 4 to 9 mm on the diameter and 3 to 11 mm on the height, plus-only tolerance.
  • Cutting and machining: band saw −0 / +5 to +15 mm on length; waterjet +10 % of thickness on the diameter (min. 2 mm); machined parts −0 / +2 to +5 mm on the diameter. See the full tables (INF 002 and INF 003, the same for every alloy).
Tariff classification of 300M steel (modified 4340): NCM, HS, HTS and CN by product form
FormNCM (Brazil, 8 digits)HS (international, 6 digits)HTS (USA, 10 digits)*CN (European Union, 8 digits)*
Forged bar7228.40.007228.407228.40.00007228 40 90
Hot-rolled bar7228.30.007228.307228.30.80417228 30 61
Seamless pipe7304.19.007304.197304.19.50507304 19 10
Welded pipe7306.19.007306.197306.19.51507306 19 00
Flange and fitting7307.91.007307.917307.91.50307307 91 00

Tariff class: alloy steel (by chemical composition, under the Chapter 72 Notes and Section XV Note 5).

Pipe: 7304.19 and 7306.19 are line pipe for oil and gas pipelines; boiler, heat exchanger or process tubes go under 7304.39/7304.59 (seamless) and 7306.30/7306.50 (welded).

*: US and EU codes for reference. NCM per current legislation (General Rules of Interpretation, Notes to Chapters 72, 74 and 75 and Section XV Note 5). Confirm the final code with your customs broker according to the item size and finish. HS = first 6 digits of the NCM.

Chemical composition (%)

AMS 6417 (UNS K44220); AMS 6257 requires C 0.40 – 0.44 and AMS 6419 requires C 0.40 – 0.45

Chemical composition of 300M steel (modified 4340) – UNS K44220, per AMS 6417 (UNS K44220); AMS 6257 requires C 0.40 – 0.44 and AMS 6419 requires C 0.40 – 0.45
ElementRange (%)
C 0.38 – 0.43
Mn 0.65 – 0.90
Si 1.45 – 1.80
Ni 1.65 – 2.00
Cr 0.70 – 0.95
Mo 0.30 – 0.50
V 0.05 – 0.10
P ≤ 0.010
S ≤ 0.008
Cu ≤ 0.35
Fe balance

Calculate the carbon equivalent of 300M steel (modified 4340) for welding →

Mechanical properties

Oil quenched from 871 °C and double tempered at ≈ 302 °C (575 °F) – AMS 6417 minimums (longitudinal) and AMS 6257 range

Mechanical properties of 300M steel (modified 4340) – UNS K44220
PropertyValue
Tensile strength 1,900 – 2,100 MPa (AMS 6257); ≥ 1,862 MPa (270 ksi, AMS 6417)
Yield strength (0.2%) ≥ 1,555 MPa (AMS 6257); ≥ 1,517 MPa (220 ksi, AMS 6417)
Elongation ≥ 8% longitudinal; ≥ 5% transverse
Reduction of area ≥ 30% longitudinal; ≥ 20% transverse
Hardness, quenched and tempered ≥ 52 HRC at the core (sections up to 89 mm)
Delivery hardness (normalized and tempered) ≤ 311 HB

Typical physical properties

Typical values at 20 °C
PropertyValue
Density 7.85 g/cm³
Modulus of elasticity ≈ 205 GPa*
Thermal expansion (mean) ≈ 11.5 µm/m·K*

Calculate the weight of 300M steel (modified 4340) bar, plate or pipe →

Heat treatment, welding and machining

ItemUsual practice
Service temperature Structural use at room and moderate temperature, always well below the tempering temperature (≈ 300 °C); above it the part loses strength. It is not stainless: it needs corrosion protection (cadmium or zinc-nickel plus paint).
Heat treatment Normalize at 927 °C (1,700 °F), air cool. Harden: austenitize at 871 °C (1,600 °F) and oil quench. Double temper 2 h + 2 h at ≈ 302 °C (575 °F) for the 1,900 – 2,100 MPa range; tempering can range from 204 to 649 °C depending on the strength required. For machining, normalize and temper at ≈ 649 °C (1,200 °F). Forge between 1,066 and 1,232 °C, finishing no lower than 927 °C. Sections up to 89 mm through-harden (≥ 52 HRC).
Welding Weldable by arc or gas processes, but rarely welded in critical parts: high carbon and hardenability bring a risk of cold cracking. When unavoidable, weld with preheat and a low-hydrogen consumable and repeat the full heat treatment afterwards, under a qualified procedure*.
Machining Machine in the normalized and tempered condition (≤ 311 HB), leave stock and only then harden and temper. After hardening (≥ 52 HRC), grinding only, with parameters that avoid burns: grinding burns create untempered martensite and surface cracks*.

Plan an open-die forging in 300M steel (modified 4340): reduction, slenderness and how much material to send →Simulate the cutting plan of the ingot or bar →

Typical applications

  • Aircraft landing gear (cylinders, axles and links)
  • Aircraft structural components such as flap tracks
  • Ultra-high-strength drive shafts
  • High-strength bolts and fasteners
  • Highly loaded gears
  • Missile and defense components
  • Motorsport suspension and driveline parts

Alternatives: SAE 4340 when 1,000 – 1,400 MPa is enough and cost matters; AerMet 100 (Ni-Co, UNS K92580) when fracture toughness and stress corrosion resistance are critical at the same strength; Maraging 250 to harden without quenching, with almost no distortion and easier welding; 17-4PH or 15-5PH when corrosion matters more than strength.

300M steel (modified 4340): complete guide

What 300M steel is

300M is a modified SAE 4340: it keeps the nickel, chromium and molybdenum of 4340, raises silicon to 1.45 – 1.80% and adds vanadium. It is vacuum arc remelted (VAR), with aircraft-quality cleanliness (AMS 2300), and delivered normalized and tempered for machining. After quenching and tempering it reaches 1,900 – 2,100 MPa tensile strength without higher carbon.

By classification it is a low-alloy steel, not a carbon steel. It sits in the carbon and low-alloy steels group of the Dustre catalog.

Why silicon and vanadium

Silicon allows tempering at ≈ 300 °C while keeping very high strength and shifts tempered martensite embrittlement to higher temperatures*. Vanadium refines the grain. The result is better fatigue strength, ductility, impact strength and fracture toughness than 4340 at the same strength level.

Hydrogen embrittlement, plating and finishing

The higher the strength of the steel, the smaller the amount of hydrogen that causes delayed cracking under load. On 300M landing gear, cadmium plating protects against corrosion, but cleaning and plating must be controlled to reduce the risk of hydrogen embrittlement, followed by a relief bake.

Shot peening introduces compressive residual stresses at the surface and improves fatigue life; grit blasting, on the other hand, roughens the surface and can reduce fatigue strength.

300M, 4340, AerMet 100 and Maraging 250

4340 costs less and covers shafts and gears up to ≈ 1,400 MPa. Maraging 250 reaches ≥ 1,724 MPa yield by aging, without quenching and with almost no distortion, but at a much higher cost. AerMet 100* (Ni-Co) trades cost for more toughness and stress corrosion resistance. When corrosion is the main problem, the choice moves to precipitation-hardening stainless steels such as 17-4PH and 15-5PH.

Supply forms and Dustre services

Round bars and blocks forged in open die, cut to size on a band saw, with rough or finish machining, heat treatment in our own furnaces and hardness, tensile and impact testing. All material is supplied with a 3.1 inspection certificate and heat traceability.

Frequently asked questions

What is the chemical composition of 300M steel (modified 4340)?

Per AMS 6417 (UNS K44220); AMS 6257 requires C 0.40 – 0.44 and AMS 6419 requires C 0.40 – 0.45: C 0.38 – 0.43; Mn 0.65 – 0.90; Si 1.45 – 1.80; Ni 1.65 – 2.00; Cr 0.70 – 0.95; Mo 0.30 – 0.50.

Which standards cover 300M steel (modified 4340)?

Bar and forging (normalized and tempered): AMS 6257 (supersedes MIL-S-8844 Class 3). Vacuum-melted bar, forging and tube (VAR): AMS 6417 (supersedes MIL-S-83135). Bar, forging and tube: AMS 6419. Aircraft-quality cleanliness: AMS 2300. Bloom and billet for aerospace forgings: ASTM A646.

Up to what temperature can 300M steel (modified 4340) be used?

Structural use at room and moderate temperature, always well below the tempering temperature (≈ 300 °C); above it the part loses strength. It is not stainless: it needs corrosion protection (cadmium or zinc-nickel plus paint).

Which materials can replace 300M steel (modified 4340)?

SAE 4340 when 1,000 – 1,400 MPa is enough and cost matters; AerMet 100 (Ni-Co, UNS K92580) when fracture toughness and stress corrosion resistance are critical at the same strength; Maraging 250 to harden without quenching, with almost no distortion and easier welding; 17-4PH or 15-5PH when corrosion matters more than strength.

Is 300M a carbon steel?

No. It is a low-alloy steel: besides ≈ 0.40% carbon, it contains about 5% total alloying elements (Ni 1.65 – 2.00%, Si 1.45 – 1.80%, Cr, Mo, Mn and V). In the catalog it sits in the carbon and low-alloy steels group, next to 4340.

What is the difference between 300M and 4340?

300M is 4340 with silicon (1.45 – 1.80% versus 0.15 – 0.35%), vanadium (0.05 – 0.10%) and slightly more molybdenum, vacuum melted. Tempered at ≈ 300 °C, it reaches 1,900 – 2,100 MPa tensile strength with better toughness and fatigue strength. Commercial quenched and tempered 4340 works in the 930 – 1,080 MPa range.

Why does 300M need care when plated?

At around 1,900 MPa, tiny amounts of hydrogen (less than 0.1 ppm mobile hydrogen in 4340 at 1,790 – 1,930 MPa) can crack the part under load. After pickling and cadmium or zinc-nickel plating, the part goes to a hydrogen relief bake; the practice cited by the US Navy is 24 h at 190 °C for the highest-strength steels. Always follow the customer's process specification.

What is the tempering temperature of 300M?

Double temper 2 h + 2 h at ≈ 302 °C (575 °F), after oil quenching from 871 °C. This cycle gives 1,900 – 2,100 MPa tensile strength. Higher tempering temperatures (up to 649 °C) lower the strength.

Where to buy 300M steel (modified 4340) in Brazil?

Dustre supplies 300M steel (modified 4340) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

Need 300M steel (modified 4340)?Bars, forgings and parts with EN 10204 3.1 certificate.

Forms and stock of 300M steel (modified 4340)

Dustre supplies 300M steel (modified 4340) as bar, pipe and tube, forgings and flanges and castings, cut to size, with forged and machined parts to drawing (shafts, discs, rings and blocks) and a 3.1 certificate.

Not in stock at the moment: supplied to order, with lead time in the quotation.

See the full ready-to-ship stock · Request a quote for 300M steel (modified 4340)

Where to buy 300M steel (modified 4340) in Brazil?

Dustre supplies 300M steel (modified 4340) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

See also

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)