Inconel 600 – UNS N06600

Solid-solution-strengthened nickel-chromium-iron alloy

Download data sheet (PDF)

Ni-Cr-Fe alloy with at least 72% nickel, for general use at high temperature and in moderately corrosive media. It combines good resistance to oxidation, alkaline media (caustic soda) and chloride stress corrosion cracking. Not hardenable by heat treatment: strength increases only by cold work.

Technical review Oct 2026 · minimum values per the cited standard; physical properties are typical; values marked * to be confirmed in the standard

FamilyNickel alloy
UNSN06600
W.Nr. / EN2.4816 – NiCr15Fe

Designations and equivalents

Designations of Inconel 600 – UNS N06600
SystemDesignation
UNS N06600
W.Nr./EN 2.4816 – NiCr15Fe
DIN NiCr15Fe (DIN 17742)
JIS NCF 600
Trade names Inconel 600 (Special Metals), Nicrofer 7216 (VDM), Alloy 600
Others AMS 5540 (plate), AMS 5665 (bar)

Standards by product form

Standards for Inconel 600 – UNS N06600
FormStandard
Bar ASTM B166
Forging ASTM B564
Plate ASTM B168
Tube ASTM B167 (seamless), B163 (heat exchanger)

Tolerances and HS codes

  • Forged bars (round and square): machining allowance from 2 mm (Ø 6–16 mm) to 24 mm (Ø 400–500 mm) on the diameter. E.g. Ø 100–125 mm finished: +7 mm, tolerance +6 / −0 (length up to 3,500 mm).
  • Forged discs: allowance of 4 to 9 mm on the diameter and 3 to 11 mm on the height, plus-only tolerance.
  • Cutting and machining: band saw −0 / +5 to +15 mm on length; waterjet +10 % of thickness on the diameter (min. 2 mm); machined parts −0 / +2 to +5 mm on the diameter. See the full tables (INF 002 and INF 003, the same for every alloy).
Tariff classification of Inconel 600: NCM, HS, HTS and CN by product form
FormNCM (Brazil, 8 digits)HS (international, 6 digits)HTS (USA, 10 digits)*CN (European Union, 8 digits)*
Forged bar7505.12.107505.127505.12.30007505 12 00
Hot-rolled bar7505.12.107505.127505.12.30007505 12 00
Plate (> 10 mm, width ≥ 600 mm)7506.20.007506.207506.20.30007506 20 00
Seamless pipe7507.12.007507.127507.12.00007507 12 00
Welded pipe7507.12.007507.127507.12.00007507 12 00
Flange and fitting7507.20.007507.207507.20.00007507 20 00

Tariff class: nickel alloy (by chemical composition, under the Chapter 72 Notes and Section XV Note 5).

*: US and EU codes for reference. NCM per current legislation (General Rules of Interpretation, Notes to Chapters 72, 74 and 75 and Section XV Note 5). Confirm the final code with your customs broker according to the item size and finish. HS = first 6 digits of the NCM.

Chemical composition (%)

ASTM B166 / B564 (UNS N06600)

Chemical composition of Inconel 600 – UNS N06600, per ASTM B166 / B564 (UNS N06600)
ElementRange (%)
Ni (+Co) ≥ 72.0
Cr 14.0 – 17.0
Fe 6.0 – 10.0
C ≤ 0.15
Mn ≤ 1.00
Si ≤ 0.50
Cu ≤ 0.50
S ≤ 0.015

Calculate the PREN of Inconel 600 in the PREN calculator →

Mechanical properties

annealed (ASTM B564 / B166 hot rolled and annealed)

Mechanical properties of Inconel 600 – UNS N06600
PropertyValue
Yield strength (0.2%) ≥ 241 MPa
Tensile strength ≥ 552 MPa
Elongation ≥ 30%
Hardness (typical, annealed) ≈ 75 – 95 HRB

Typical physical properties

Typical values at 20 °C
PropertyValue
Density 8.47 g/cm³
Melting range 1,354 – 1,413 °C
Modulus of elasticity 207 GPa
Thermal conductivity (20 °C) 14.9 W/m·K
Thermal expansion (20–100 °C) 13.3 µm/m·K
Electrical resistivity 103 µΩ·cm

Calculate the weight of Inconel 600 bar, plate or pipe →

Heat treatment, welding and machining

ItemUsual practice
Service temperature Oxidation resistance up to ~1,100 °C; creep design typically up to ~650 °C. In sulfur-bearing atmospheres the limit drops considerably (typically ~550 °C).
Heat treatment Supplied annealed (≈ 980 – 1,040 °C) or solution annealed (≈ 1,120 °C, when creep resistance is sought), with rapid cooling. Avoid long solution-annealing times (grain growth). Not age hardenable.
Welding Good weldability by GTAW, GMAW and SMAW. Consumables: AWS A5.14 ERNiCr-3 (FM 82 type) and AWS A5.11 ENiCrFe-3 (182 type). Normally without preheat or PWHT.
Machining Low machinability: work hardens quickly; use sharp carbide, constant feed (no 'rubbing') and abundant coolant.

Plan an open-die forging in Inconel 600: reduction, slenderness and how much material to send →Simulate the cutting plan of the ingot or bar →

Filler metal for welding

The wire composition is usually not identical to the material: each page explains why.

Typical applications

  • Muffles, retorts and fixtures for heat treatment furnaces
  • Heat exchangers and heaters in the chemical industry
  • Evaporators and caustic soda equipment
  • Fatty acid and food processing
  • Thermocouple sheaths and heating elements
  • Nuclear components (replaced by 690 in primary water)

Alternatives: Inconel 601 for cyclic oxidation above ~1,050 °C; Incoloy 800H/HT when cost and creep weigh more; Inconel 690 in pressurized water (nuclear); Nickel 201 for hot concentrated caustic soda.

Compare alloys by corrosive medium, concentration and temperature →

Inconel 600: complete guide

What Inconel 600 is

Inconel 600 belongs to the family of nickel alloys, in the solid-solution nickel-chromium-iron group. With a minimum of 72% nickel, it resists reducing media, caustics and chloride stress corrosion cracking; with 14 to 17% chromium, it resists oxidation in air up to about 1,100 °C. It does not harden by heat treatment: its strength comes from solid solution and cold work.

Mechanical properties

In annealed bar and forgings, ASTM B166 / B564 requires a minimum yield strength of 241 MPa, minimum tensile strength of 552 MPa and minimum elongation of 30%. Under load at temperature, design is based on creep allowable stresses, typically up to about 650 °C; oxidation resistance, up to 1,100 °C, applies to lightly loaded components.

Welding

Good weldability by TIG, MIG and covered electrode with ERNiCr-3 and ENiCrFe-3 consumables, without preheat or post-weld heat treatment.

Corrosion and limits of use

600 is the classic alloy for caustic soda and alkaline media, magnesium chloride and reducing processes, and resists chloride stress corrosion cracking well.

Applications

Muffles, retorts, baskets and heat treatment furnace components, caustic soda production and concentration equipment, exchangers and vessels for reducing chemical processes, turbine and engine components at moderate temperature, glass furnace parts and food equipment.

Supply forms and Dustre services

Round bars and blocks forged in open die, cut to size on a band saw, with rough or finish machining, solution annealing or annealing in our own furnaces and hardness, tensile and impact testing. All material is supplied with a 3.1 inspection certificate and heat traceability.

Frequently asked questions

What is the chemical composition of Inconel 600?

Per ASTM B166 / B564 (UNS N06600): Ni (+Co) ≥ 72.0; Cr 14.0 – 17.0; Fe 6.0 – 10.0; C ≤ 0.15; Mn ≤ 1.00; Si ≤ 0.50.

Which standards cover Inconel 600?

Bar: ASTM B166. Forging: ASTM B564. Plate: ASTM B168. Tube: ASTM B167 (seamless), B163 (heat exchanger).

Up to what temperature can Inconel 600 be used?

Oxidation resistance up to ~1,100 °C; creep design typically up to ~650 °C. In sulfur-bearing atmospheres the limit drops considerably (typically ~550 °C).

Which materials can replace Inconel 600?

Inconel 601 for cyclic oxidation above ~1,050 °C; Incoloy 800H/HT when cost and creep weigh more; Inconel 690 in pressurized water (nuclear); Nickel 201 for hot concentrated caustic soda.

Where to buy Inconel 600 in Brazil?

Dustre supplies Inconel 600 as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

Need Inconel 600?Bars, forgings and parts with EN 10204 3.1 certificate.

Forms and stock of Inconel 600

Dustre supplies Inconel 600 as bar, plate, pipe and tube and forgings and flanges, cut to size, with forged and machined parts to drawing (shafts, discs, rings and blocks) and a 3.1 certificate.

In stock in Osasco/SP, Brazil: plate from 8 mm and round bar from Ø 6 to 160 mm. List updated on 11/13/2026.

See the full ready-to-ship stock · Request a quote for Inconel 600

Where to buy Inconel 600 in Brazil?

Dustre supplies Inconel 600 as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

See also

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)