ER2594 – wire and rod for super duplex 2507

Super duplex 25Cr-9.5Ni-4Mo-N filler metal, for super duplex 2507 steels (UNS S32750/S32760) and for alloy S32550, with PREN above 40.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER2594
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS32594*
GroupDuplex stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER2594
Solid MIG/MAG wire (GMAW) ER2594
Covered electrode (SMAW) E2594-16 – AWS A5.4
Flux-cored wire (FCAW) E2594T0-1/-4 – AWS A5.22*
Submerged arc wire (SAW) ER2594 + flux
Designations and equivalents
DesignationValue
AWS ER2594
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S32594*
Others EN ISO 14343-A: W/G 25 9 4 N L; W.Nr. 1.4501*

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.03
Cr 24.0 – 27.0
Ni 8.0 – 10.5
Mo 2.5 – 4.5
N 0.20 – 0.30
W ≤ 1.0
Cu ≤ 1.5
Mn ≤ 2.5
Si ≤ 1.0
P ≤ 0.03
S ≤ 0.02

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 760 MPa (AWS A5.4 minimum for E2594, reference)
Elongation ≥ 15 % (AWS A5.4 minimum for E2594, reference)

Materials welded with ER2594

Dissimilar joints: Can be used on duplex 2205 when a bead with higher pitting resistance than the base metal is wanted.

Why the composition differs from the base metal

As with 2209, the nickel is raised (about 9–10 %, versus 6–8 % in 2507) so that the rapidly cooled bead forms enough austenite. The high nitrogen keeps the PREN of the deposit at the same level as the base metal.

Welding precautions

  • Typical heat input of 0.5 to 1.5 kJ/mm and maximum interpass of 100 °C.
  • TIG with argon and 1–2 % N2 helps keep the nitrogen in the bead; purge with argon or argon-nitrogen.
  • Avoid repeated reheating of the same region (risk of sigma phase).
  • Do not weld the root without wire.

Frequently asked questions

What is ER2594 used for?

Super duplex 25Cr-9.5Ni-4Mo-N filler metal, for super duplex 2507 steels (UNS S32750/S32760) and for alloy S32550, with PREN above 40.

Why is the composition of ER2594 different from the material it welds?

As with 2209, the nickel is raised (about 9–10 %, versus 6–8 % in 2507) so that the rapidly cooled bead forms enough austenite. The high nitrogen keeps the PREN of the deposit at the same level as the base metal.

Which covered electrode corresponds to ER2594?

E2594-16 – AWS A5.4.

What precautions apply when welding with ER2594?

Typical heat input of 0.5 to 1.5 kJ/mm and maximum interpass of 100 °C. TIG with argon and 1–2 % N2 helps keep the nitrogen in the bead; purge with argon or argon-nitrogen. Avoid repeated reheating of the same region (risk of sigma phase). Do not weld the root without wire.

Need ER2594?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)