ERNiCrMo-10 – wire and rod for Hastelloy C-22

Ni-21Cr-13Mo-3W filler metal for alloy C-22, also used as an over-alloyed option for welding C-276, alloy 625 and super-austenitics.

Technical review Oct 2026 · composition per AWS A5.14/A5.14M; values marked * to be confirmed in the current edition of the standard

ClassificationERNiCrMo-10
StandardAWS A5.14/A5.14M / ASME SFA-5.14
UNSN06022
GroupNickel alloy

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ERNiCrMo-10
Solid MIG/MAG wire (GMAW) ERNiCrMo-10
Covered electrode (SMAW) ENiCrMo-10 – AWS A5.11
Submerged arc wire (SAW) ERNiCrMo-10 + flux
Designations and equivalents
DesignationValue
AWS ERNiCrMo-10
Specification AWS A5.14/A5.14M / ASME SFA-5.14
UNS N06022
Others EN ISO 18274: S Ni 6022 (NiCr21Mo13Fe4W3); W.Nr. 2.4635
Trade designation Liga C-22 / Hastelloy C-22 (designação de material)

Chemical composition (%)

AWS A5.14 (% by mass, filler metal)
Elementwt. %
C ≤ 0.015
Cr 20.0 – 22.5
Mo 12.5 – 14.5
W 2.5 – 3.5
Fe 2.0 – 6.0
Co ≤ 2.5
V ≤ 0.35
Ni Balance
Mn ≤ 0.50
Si ≤ 0.08
Cu ≤ 0.50
P ≤ 0.02
S ≤ 0.010

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 690 MPa (AWS A5.11 minimum for ENiCrMo-10, reference)
Elongation ≥ 25 % (AWS A5.11 minimum for ENiCrMo-10, reference)

Materials welded with ERNiCrMo-10

Dissimilar joints: A good choice for joints between different Ni-Cr-Mo alloys and between those alloys and stainless, since the higher chromium tolerates dilution with iron well.

Why the composition differs from the base metal

For alloy C-22 itself the chemistry is practically identical, with very low carbon and silicon. On C-276 and super-austenitics it serves as over-alloyed metal: 21 % chromium and 13 % molybdenum give the bead corrosion resistance equal to or higher than the base metal even after segregation.

Welding precautions

  • No preheating; interpass below 100–150 °C.
  • Low heat input; avoid repeatedly reheating the same region.
  • TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Frequently asked questions

What is ERNiCrMo-10 used for?

Ni-21Cr-13Mo-3W filler metal for alloy C-22, also used as an over-alloyed option for welding C-276, alloy 625 and super-austenitics.

Why is the composition of ERNiCrMo-10 different from the material it welds?

For alloy C-22 itself the chemistry is practically identical, with very low carbon and silicon. On C-276 and super-austenitics it serves as over-alloyed metal: 21 % chromium and 13 % molybdenum give the bead corrosion resistance equal to or higher than the base metal even after segregation.

Which covered electrode corresponds to ERNiCrMo-10?

ENiCrMo-10 – AWS A5.11.

What precautions apply when welding with ERNiCrMo-10?

No preheating; interpass below 100–150 °C. Low heat input; avoid repeatedly reheating the same region. TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Need ERNiCrMo-10?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)