ERNiCrMo-4 – wire and rod for Hastelloy C-276

Ni-16Cr-16Mo-4W filler metal for alloy C-276, with high resistance to reducing and oxidizing acids, chlorides and mixed media in chemical and pollution control plants.

Technical review Oct 2026 · composition per AWS A5.14/A5.14M; values marked * to be confirmed in the current edition of the standard

ClassificationERNiCrMo-4
StandardAWS A5.14/A5.14M / ASME SFA-5.14
UNSN10276
GroupNickel alloy

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ERNiCrMo-4
Solid MIG/MAG wire (GMAW) ERNiCrMo-4
Covered electrode (SMAW) ENiCrMo-4 – AWS A5.11
Submerged arc wire (SAW) ERNiCrMo-4 + flux
Designations and equivalents
DesignationValue
AWS ERNiCrMo-4
Specification AWS A5.14/A5.14M / ASME SFA-5.14
UNS N10276
Others EN ISO 18274: S Ni 6276 (NiCr15Mo16Fe6W4); W.Nr. 2.4886
Trade designation Liga C-276 / Hastelloy C-276 (designação de material)

Chemical composition (%)

AWS A5.14 (% by mass, filler metal)
Elementwt. %
C ≤ 0.02
Cr 14.5 – 16.5
Mo 15.0 – 17.0
W 3.0 – 4.5
Fe 4.0 – 7.0
Co ≤ 2.5
V ≤ 0.35
Ni Balance
Mn ≤ 1.0
Si ≤ 0.08
Cu ≤ 0.50
P ≤ 0.04
S ≤ 0.03

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 690 MPa (AWS A5.11 minimum for ENiCrMo-4, reference)
Elongation ≥ 25 % (AWS A5.11 minimum for ENiCrMo-4, reference)

Materials welded with ERNiCrMo-4

Dissimilar joints: Also employed to join C-276 to stainless and to carbon steel, and in overlays on carbon steel exposed to aggressive media.

Why the composition differs from the base metal

Here the composition is practically that of the base metal, with very low carbon and silicon. Those limits are the key point: they reduce the precipitation of carbides and intermetallic phases in the fusion zone, which would strip the bead of its corrosion resistance.

Welding precautions

  • No preheating; interpass below 100–150 °C.
  • Low heat input and stringer beads, without wide weaving.
  • TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Frequently asked questions

What is ERNiCrMo-4 used for?

Ni-16Cr-16Mo-4W filler metal for alloy C-276, with high resistance to reducing and oxidizing acids, chlorides and mixed media in chemical and pollution control plants.

Why is the composition of ERNiCrMo-4 different from the material it welds?

Here the composition is practically that of the base metal, with very low carbon and silicon. Those limits are the key point: they reduce the precipitation of carbides and intermetallic phases in the fusion zone, which would strip the bead of its corrosion resistance.

Which covered electrode corresponds to ERNiCrMo-4?

ENiCrMo-4 – AWS A5.11.

What precautions apply when welding with ERNiCrMo-4?

No preheating; interpass below 100–150 °C. Low heat input and stringer beads, without wide weaving. TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Need ERNiCrMo-4?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)