ER347 – wire and rod for 321 and 347 stainless

Niobium-stabilized austenitic filler metal, used on 347 and 321 stainless that work in the sensitization range (about 425 to 850 °C).

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER347
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS34780
GroupAustenitic stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER347
Solid MIG/MAG wire (GMAW) ER347 / ER347Si
Covered electrode (SMAW) E347-16/-17 – AWS A5.4
Flux-cored wire (FCAW) E347T0-1/-4 – AWS A5.22
Submerged arc wire (SAW) ER347 + flux
Designations and equivalents
DesignationValue
AWS ER347
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S34780
Others EN ISO 14343-A: W/G 19 9 Nb; W.Nr. 1.4551

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.08
Cr 19.0 – 21.5
Ni 9.0 – 11.0
Mo ≤ 0.75
Mn 1.0 – 2.5
Si 0.30 – 0.65
P ≤ 0.03
S ≤ 0.03
Cu ≤ 0.75
Nb 10 × C min. – 1.0

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 520 MPa (AWS A5.4 minimum for E347, reference)
Elongation ≥ 30 % (AWS A5.4 minimum for E347, reference)

Materials welded with ER347

Why the composition differs from the base metal

321 stainless is stabilized with titanium, but titanium oxidizes and is lost in the electric arc. That is why the wire uses niobium, which crosses the arc and keeps tying up the carbon as niobium carbides, keeping the bead stabilized.

Welding precautions

  • No preheating; interpass up to 150 °C.
  • Keep the bead ferrite within the recommended range to avoid hot cracking, to which Nb is sensitive.
  • TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes.

Frequently asked questions

What is ER347 used for?

Niobium-stabilized austenitic filler metal, used on 347 and 321 stainless that work in the sensitization range (about 425 to 850 °C).

Why is the composition of ER347 different from the material it welds?

321 stainless is stabilized with titanium, but titanium oxidizes and is lost in the electric arc. That is why the wire uses niobium, which crosses the arc and keeps tying up the carbon as niobium carbides, keeping the bead stabilized.

Which covered electrode corresponds to ER347?

E347-16/-17 – AWS A5.4.

What precautions apply when welding with ER347?

No preheating; interpass up to 150 °C. Keep the bead ferrite within the recommended range to avoid hot cracking, to which Nb is sensitive. TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes.

Need ER347?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)