ER309L – wire and rod for stainless-to-carbon steel joints

Low-carbon 23Cr-13Ni filler metal, used to join stainless to carbon or low-alloy steel and as a buttering layer before stainless overlay.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER309L
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS30983
GroupAustenitic stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER309L
Solid MIG/MAG wire (GMAW) ER309L / ER309LSi
Covered electrode (SMAW) E309L-16/-17 – AWS A5.4
Flux-cored wire (FCAW) E309LT0-1/-4 – AWS A5.22
Submerged arc wire (SAW) ER309L + flux
Designations and equivalents
DesignationValue
AWS ER309L
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S30983
Others EN ISO 14343-A: W/G 23 12 L; W.Nr. 1.4332

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.03
Cr 23.0 – 25.0
Ni 12.0 – 14.0
Mo ≤ 0.75
Mn 1.0 – 2.5
Si 0.30 – 0.65
P ≤ 0.03
S ≤ 0.03
Cu ≤ 0.75

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 520 MPa (AWS A5.4 minimum for E309L, reference)
Elongation ≥ 30 % (AWS A5.4 minimum for E309L, reference)

Materials welded with ER309L

Dissimilar joints: Typical joint: 304L/316L stainless with carbon steel (e.g. an A105 flange) or with Cr-Mo steel at moderate temperature. When a joint with 316L must keep molybdenum in the bead, for pitting resistance, ER309LMo is used. Also used on martensitic and ferritic stainless (416, 431, 446) when an austenitic bead, softer than the base metal, is acceptable.

Why the composition differs from the base metal

It is more highly alloyed than 304 on purpose. When the bead mixes with carbon steel, which has no Cr or Ni, dilution lowers the alloy content; starting from 23Cr-13Ni the result is still austenitic with a little ferrite, without brittle martensite or cracks.

Welding precautions

  • Control dilution: torch angle toward the stainless side and moderate heat input.
  • Preheat the carbon steel or martensitic side according to thickness and carbon equivalent.
  • Not indicated above about 370 °C in joints with carbon steel because of carbon migration; in that case prefer a nickel alloy.
  • TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes.

Frequently asked questions

What is ER309L used for?

Low-carbon 23Cr-13Ni filler metal, used to join stainless to carbon or low-alloy steel and as a buttering layer before stainless overlay.

Why is the composition of ER309L different from the material it welds?

It is more highly alloyed than 304 on purpose. When the bead mixes with carbon steel, which has no Cr or Ni, dilution lowers the alloy content; starting from 23Cr-13Ni the result is still austenitic with a little ferrite, without brittle martensite or cracks.

Which covered electrode corresponds to ER309L?

E309L-16/-17 – AWS A5.4.

What precautions apply when welding with ER309L?

Control dilution: torch angle toward the stainless side and moderate heat input. Preheat the carbon steel or martensitic side according to thickness and carbon equivalent. Not indicated above about 370 °C in joints with carbon steel because of carbon migration; in that case prefer a nickel alloy. TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes.

Need ER309L?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)