ERNiCu-7 – wire and rod for Monel 400 and K-500

Nickel-copper filler metal (about 65Ni-30Cu) with titanium, for welding alloy 400 and making joints or repairs on K-500, in seawater, hydrofluoric acid and brines.

Technical review Oct 2026 · composition per AWS A5.14/A5.14M; values marked * to be confirmed in the current edition of the standard

ClassificationERNiCu-7
StandardAWS A5.14/A5.14M / ASME SFA-5.14
UNSN04060
GroupNickel alloy

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ERNiCu-7
Solid MIG/MAG wire (GMAW) ERNiCu-7
Covered electrode (SMAW) ENiCu-7 – AWS A5.11
Submerged arc wire (SAW) ERNiCu-7 + flux
Designations and equivalents
DesignationValue
AWS ERNiCu-7
Specification AWS A5.14/A5.14M / ASME SFA-5.14
UNS N04060
Others EN ISO 18274: S Ni 4060 (NiCu30Mn3Ti); W.Nr. 2.4377
Trade designation Liga 60 (arame para soldar Monel 400) (designação de material)

Chemical composition (%)

AWS A5.14 (% by mass, filler metal)
Elementwt. %
C ≤ 0.15
Ni 62.0 – 69.0
Cu Balance
Ti 1.5 – 3.0
Mn ≤ 4.0
Fe ≤ 2.5
Al ≤ 1.25
Si ≤ 1.25
P ≤ 0.02*
S ≤ 0.015

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 480 MPa (AWS A5.11 minimum for ENiCu-7, reference)
Elongation ≥ 30 % (AWS A5.11 minimum for ENiCu-7, reference)

Materials welded with ERNiCu-7

Dissimilar joints: Can join alloy 400 to carbon steel and to copper-nickel; for joints with stainless, ERNiCr-3 is usually preferred.

Why the composition differs from the base metal

The wire has about 2–3 % titanium, which alloy 400 does not have. Titanium deoxidizes and denitrifies the pool, preventing the porosity typical of Ni-Cu alloys. On K-500 the bead does not age like the base metal, so the joint ends up with the strength of alloy 400.

Welding precautions

  • No preheating; interpass below 150 °C.
  • On K-500, weld the solution-treated material and be aware that the weld does not reach the strength of the aged metal.
  • TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Frequently asked questions

What is ERNiCu-7 used for?

Nickel-copper filler metal (about 65Ni-30Cu) with titanium, for welding alloy 400 and making joints or repairs on K-500, in seawater, hydrofluoric acid and brines.

Why is the composition of ERNiCu-7 different from the material it welds?

The wire has about 2–3 % titanium, which alloy 400 does not have. Titanium deoxidizes and denitrifies the pool, preventing the porosity typical of Ni-Cu alloys. On K-500 the bead does not age like the base metal, so the joint ends up with the strength of alloy 400.

Which covered electrode corresponds to ERNiCu-7?

ENiCu-7 – AWS A5.11.

What precautions apply when welding with ERNiCu-7?

No preheating; interpass below 150 °C. On K-500, weld the solution-treated material and be aware that the weld does not reach the strength of the aged metal. TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Need ERNiCu-7?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)