ER310 – wire and rod for 310 stainless and high-temperature service

Fully austenitic 25Cr-20Ni filler metal for 310 stainless and parts working under oxidation at elevated temperatures, such as furnaces and burners.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER310
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS31080
GroupAustenitic stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER310
Solid MIG/MAG wire (GMAW) ER310
Covered electrode (SMAW) E310-16/-15 – AWS A5.4
Flux-cored wire (FCAW) E310T0-1/-4 – AWS A5.22
Submerged arc wire (SAW) ER310 + flux
Designations and equivalents
DesignationValue
AWS ER310
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S31080
Others EN ISO 14343-A: W/G 25 20; W.Nr. 1.4842

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C 0.08 – 0.15
Cr 25.0 – 28.0
Ni 20.0 – 22.5
Mo ≤ 0.75
Mn 1.0 – 2.5
Si 0.30 – 0.65
P ≤ 0.03
S ≤ 0.03
Cu ≤ 0.75

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 550 MPa (AWS A5.4 minimum for E310, reference)
Elongation ≥ 30 % (AWS A5.4 minimum for E310, reference)

Materials welded with ER310

Dissimilar joints: Used in repairs of 446 ferritic stainless and in joints between heat-resisting stainless steels. For joining stainless to carbon steel, ER309L is indicated, or ERNiCr-3 in service above about 370 °C: the 100 % austenitic bead of ER310, diluted with carbon steel, tends to hot crack.

Why the composition differs from the base metal

Carbon is kept between 0.08 and 0.15 % to guarantee hot strength, and the bead comes out without ferrite. This avoids the sigma-phase embrittlement that ferrite would suffer in long exposures at 600–900 °C, but requires care against hot cracking.

Welding precautions

  • Fully austenitic deposit: use low heat input, stringer beads and well-filled craters to avoid hot cracking.
  • Interpass below 150 °C.
  • TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes.

Frequently asked questions

What is ER310 used for?

Fully austenitic 25Cr-20Ni filler metal for 310 stainless and parts working under oxidation at elevated temperatures, such as furnaces and burners.

Why is the composition of ER310 different from the material it welds?

Carbon is kept between 0.08 and 0.15 % to guarantee hot strength, and the bead comes out without ferrite. This avoids the sigma-phase embrittlement that ferrite would suffer in long exposures at 600–900 °C, but requires care against hot cracking.

Which covered electrode corresponds to ER310?

E310-16/-15 – AWS A5.4.

What precautions apply when welding with ER310?

Fully austenitic deposit: use low heat input, stringer beads and well-filled craters to avoid hot cracking. Interpass below 150 °C. TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes.

Need ER310?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)