ER410NiMo – wire and rod for CA6NM (F6NM) martensitic stainless

Low-carbon martensitic 12Cr-4.5Ni-0.5Mo filler metal, for 13Cr-4Ni steels such as F6NM and CA6NM, used in hydraulic turbines, pumps and valves.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER410NiMo
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS41086
GroupMartensitic and PH stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER410NiMo
Solid MIG/MAG wire (GMAW) ER410NiMo
Covered electrode (SMAW) E410NiMo-15/-16 – AWS A5.4
Flux-cored wire (FCAW) E410NiMoT0-1/-4 – AWS A5.22
Submerged arc wire (SAW) ER410NiMo + flux
Designations and equivalents
DesignationValue
AWS ER410NiMo
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S41086
Others EN ISO 14343-A: W/G 13 4; W.Nr. 1.4351*

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.06
Cr 11.0 – 12.5
Ni 4.0 – 5.0
Mo 0.4 – 0.7
Mn ≤ 0.6
Si ≤ 0.5
P ≤ 0.03
S ≤ 0.03
Cu ≤ 0.75

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 760 MPa (AWS A5.4 minimum for E410NiMo, after PWHT, reference)
Elongation ≥ 15 % (AWS A5.4 minimum for E410NiMo, after PWHT, reference)

Materials welded with ER410NiMo

Dissimilar joints: Also used in repairs of 431 stainless when a martensitic bead with good toughness is wanted.

Why the composition differs from the base metal

Chromium is slightly below the base metal and carbon is limited to 0.06 %. With 4–5 % nickel, this avoids delta ferrite in the bead and produces soft low-carbon martensite, tougher and less prone to cracking than an ordinary 13Cr deposit.

Welding precautions

  • Preheat and interpass of about 100 to 150 °C (some sources indicate a 150 °C minimum on thick parts).
  • PWHT typically between 580 and 620 °C; do not exceed about 620 °C, since above that reverted martensite re-hardens.
  • Cool below about 100 °C before PWHT.

Frequently asked questions

What is ER410NiMo used for?

Low-carbon martensitic 12Cr-4.5Ni-0.5Mo filler metal, for 13Cr-4Ni steels such as F6NM and CA6NM, used in hydraulic turbines, pumps and valves.

Why is the composition of ER410NiMo different from the material it welds?

Chromium is slightly below the base metal and carbon is limited to 0.06 %. With 4–5 % nickel, this avoids delta ferrite in the bead and produces soft low-carbon martensite, tougher and less prone to cracking than an ordinary 13Cr deposit.

Which covered electrode corresponds to ER410NiMo?

E410NiMo-15/-16 – AWS A5.4.

What precautions apply when welding with ER410NiMo?

Preheat and interpass of about 100 to 150 °C (some sources indicate a 150 °C minimum on thick parts). PWHT typically between 580 and 620 °C; do not exceed about 620 °C, since above that reverted martensite re-hardens. Cool below about 100 °C before PWHT.

Need ER410NiMo?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)