ER630 – wire and rod for 17-4PH and 15-5PH

Precipitation-hardenable 16Cr-4.8Ni-3.6Cu-Nb filler metal, for welding 17-4PH and 15-5PH steels with an aging response.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER630
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS17480
GroupMartensitic and PH stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER630
Solid MIG/MAG wire (GMAW) ER630
Covered electrode (SMAW) E630-15/-16 – AWS A5.4
Designations and equivalents
DesignationValue
AWS ER630
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S17480
Others EN ISO 14343-A: W/G Z 17 4 Cu Nb*; W.Nr. 1.4542*
Trade designation 17-4PH (designação de material)

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.05
Cr 16.00 – 16.75
Ni 4.5 – 5.0
Cu 3.25 – 4.00
Nb 0.15 – 0.30
Mo ≤ 0.75
Mn 0.25 – 0.75
Si ≤ 0.75
P ≤ 0.03
S ≤ 0.03

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 930 MPa (AWS A5.4 minimum for E630, after solution treatment and aging, reference)
Elongation ≥ 7 % (AWS A5.4 minimum for E630, reference)*

Materials welded with ER630

Why the composition differs from the base metal

The niobium in the wire is much lower than in 17-4PH (0.15–0.30 % versus up to about 0.45 %) and the Cr and Ni ranges are narrow. This reduces hot cracking and adjusts the ferrite content of the bead, which solidifies without the hot working of the bar.

Welding precautions

  • Preheating is normally not needed in thin sections; in thick sections, 100–150 °C.
  • To recover strength, solution treat (about 1040 °C) and age (e.g. H1150 or H1025) after welding; aging alone already improves it considerably.
  • Preferably weld the material in the solution-annealed (Cond. A) or overaged condition.

Frequently asked questions

What is ER630 used for?

Precipitation-hardenable 16Cr-4.8Ni-3.6Cu-Nb filler metal, for welding 17-4PH and 15-5PH steels with an aging response.

Why is the composition of ER630 different from the material it welds?

The niobium in the wire is much lower than in 17-4PH (0.15–0.30 % versus up to about 0.45 %) and the Cr and Ni ranges are narrow. This reduces hot cracking and adjusts the ferrite content of the bead, which solidifies without the hot working of the bar.

Which covered electrode corresponds to ER630?

E630-15/-16 – AWS A5.4.

What precautions apply when welding with ER630?

Preheating is normally not needed in thin sections; in thick sections, 100–150 °C. To recover strength, solution treat (about 1040 °C) and age (e.g. H1150 or H1025) after welding; aging alone already improves it considerably. Preferably weld the material in the solution-annealed (Cond. A) or overaged condition.

Need ER630?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)