ER410 – wire and rod for 410/403 martensitic stainless

Martensitic 12–13 % Cr filler metal for welding and repairing 403 and 410 stainless steels, for example turbine blades, shafts and components.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER410
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS41080
GroupMartensitic and PH stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER410
Solid MIG/MAG wire (GMAW) ER410
Covered electrode (SMAW) E410-15/-16 – AWS A5.4
Flux-cored wire (FCAW) E410T0-1/-4 – AWS A5.22
Submerged arc wire (SAW) ER410 + flux
Designations and equivalents
DesignationValue
AWS ER410
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S41080
Others EN ISO 14343-A: W/G 13; W.Nr. 1.4009*

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.12
Cr 11.5 – 13.5
Ni ≤ 0.6
Mo ≤ 0.75
Mn ≤ 0.6
Si ≤ 0.5
P ≤ 0.03
S ≤ 0.03
Cu ≤ 0.75

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 520 MPa (AWS A5.4 minimum for E410, after PWHT, reference)
Elongation ≥ 20 % (AWS A5.4 minimum for E410, after PWHT, reference)

Materials welded with ER410

Dissimilar joints: On 416 (free-machining, with sulfur) weldability is limited; ER410 serves when a hardenable bead is wanted, and ER309L when an austenitic bead is acceptable.

Why the composition differs from the base metal

The chemistry follows the base metal so that the bead also hardens and responds to tempering. The difference lies in the tighter limits for Mn, Si, P and S, which reduce cracking and improve toughness; in the case of 416, the wire does not carry the sulfur of the base metal.

Welding precautions

  • Preheat and interpass of 200 to 300 °C, according to thickness.
  • Tempering PWHT (typically 650–760 °C) right after welding.
  • Let the part cool slowly to about 100 °C before PWHT to complete the martensitic transformation.

Frequently asked questions

What is ER410 used for?

Martensitic 12–13 % Cr filler metal for welding and repairing 403 and 410 stainless steels, for example turbine blades, shafts and components.

Why is the composition of ER410 different from the material it welds?

The chemistry follows the base metal so that the bead also hardens and responds to tempering. The difference lies in the tighter limits for Mn, Si, P and S, which reduce cracking and improve toughness; in the case of 416, the wire does not carry the sulfur of the base metal.

Which covered electrode corresponds to ER410?

E410-15/-16 – AWS A5.4.

What precautions apply when welding with ER410?

Preheat and interpass of 200 to 300 °C, according to thickness. Tempering PWHT (typically 650–760 °C) right after welding. Let the part cool slowly to about 100 °C before PWHT to complete the martensitic transformation.

Need ER410?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)