ERNi-1 – wire and rod for nickel 200 and 201

Commercially pure nickel filler metal with titanium, for nickel 200/201 in caustic soda, food and electronics equipment, and for overlaying carbon steel.

Technical review Oct 2026 · composition per AWS A5.14/A5.14M; values marked * to be confirmed in the current edition of the standard

ClassificationERNi-1
StandardAWS A5.14/A5.14M / ASME SFA-5.14
UNSN02061
GroupNickel alloy

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ERNi-1
Solid MIG/MAG wire (GMAW) ERNi-1
Covered electrode (SMAW) ENi-1 – AWS A5.11
Submerged arc wire (SAW) ERNi-1 + flux
Designations and equivalents
DesignationValue
AWS ERNi-1
Specification AWS A5.14/A5.14M / ASME SFA-5.14
UNS N02061
Others EN ISO 18274: S Ni 2061 (NiTi3); W.Nr. 2.4155
Trade designation Níquel 61 (designação genérica)

Chemical composition (%)

AWS A5.14 (% by mass, filler metal)
Elementwt. %
C ≤ 0.15
Ni ≥ 93.0
Ti 2.0 – 3.5
Al ≤ 1.5
Mn ≤ 1.0
Fe ≤ 1.0
Si ≤ 0.75
Cu ≤ 0.25
P ≤ 0.03
S ≤ 0.015

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 410 MPa (AWS A5.11 minimum for ENi-1, reference)
Elongation ≥ 20 % (AWS A5.11 minimum for ENi-1, reference)

Materials welded with ERNi-1

Why the composition differs from the base metal

Nickel 200 has more than 99 % Ni, but the wire has only about 93–96 %, because it carries 2–3.5 % titanium and a little aluminum. These elements capture oxygen and nitrogen from the pool; without them, molten pure nickel produces a lot of porosity.

Welding precautions

  • No preheating.
  • Very rigorous cleaning: pure nickel is sensitive to sulfur and lead.
  • The nickel alloy pool is viscous and penetrates little: use a wider bevel, a smaller root face and place the wire at the edge of the pool.
  • TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Frequently asked questions

What is ERNi-1 used for?

Commercially pure nickel filler metal with titanium, for nickel 200/201 in caustic soda, food and electronics equipment, and for overlaying carbon steel.

Why is the composition of ERNi-1 different from the material it welds?

Nickel 200 has more than 99 % Ni, but the wire has only about 93–96 %, because it carries 2–3.5 % titanium and a little aluminum. These elements capture oxygen and nitrogen from the pool; without them, molten pure nickel produces a lot of porosity.

Which covered electrode corresponds to ERNi-1?

ENi-1 – AWS A5.11.

What precautions apply when welding with ERNi-1?

No preheating. Very rigorous cleaning: pure nickel is sensitive to sulfur and lead. The nickel alloy pool is viscous and penetrates little: use a wider bevel, a smaller root face and place the wire at the edge of the pool. TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Need ERNi-1?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)