ER90S-B3 – wire and rod for 2¼Cr-1Mo steel (F22)

2¼Cr-1Mo filler metal for ASTM A182 F22 and equivalent forgings and tubes, in pressure vessels, reactors and high-temperature steam lines.

Technical review Oct 2026 · composition per AWS A5.28/A5.28M; values marked * to be confirmed in the current edition of the standard

ClassificationER90S-B3
StandardAWS A5.28/A5.28M / ASME SFA-5.28
UNSK30960
GroupCr-Mo steel

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER90S-B3
Solid MIG/MAG wire (GMAW) ER90S-B3
Covered electrode (SMAW) E9018-B3 – AWS A5.5
Flux-cored wire (FCAW) E91T1-B3 – AWS A5.29
Submerged arc wire (SAW) EB3 + flux – AWS A5.23
Designations and equivalents
DesignationValue
AWS ER90S-B3
Specification AWS A5.28/A5.28M / ASME SFA-5.28
UNS K30960
Others EN ISO 21952-A: W/G CrMo2Si*; AWS A5.28M: ER62S-B3

Chemical composition (%)

AWS A5.28 (% by mass, filler metal)
Elementwt. %
C 0.07 – 0.12
Mn 0.40 – 0.70
Si 0.40 – 0.70
Cr 2.30 – 2.70
Mo 0.90 – 1.20
Ni ≤ 0.20
P ≤ 0.025
S ≤ 0.025
Cu ≤ 0.35

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 620 MPa (AWS minimum, after PWHT)
Yield strength ≥ 540 MPa (AWS minimum, after PWHT)*
Elongation ≥ 17 % (AWS minimum, after PWHT)*

Materials welded with ER90S-B3

Why the composition differs from the base metal

The alloy is the same as F22, but the wire has carbon controlled within a narrow range and higher silicon for deoxidation. This balances hot strength after PWHT with a lower tendency to solidification and reheat cracking.

Welding precautions

  • Preheat and interpass of about 200 to 300 °C.
  • PWHT typically between 690 and 750 °C.
  • For high-pressure hydrogen service, require control of residuals (Bruscato X factor) on the certificate.
  • TIG with pure argon; MIG/MAG with argon and 2–5 % O2 or up to 20 % CO2*. Clean, dry wire and bevel to limit hydrogen.

Frequently asked questions

What is ER90S-B3 used for?

2¼Cr-1Mo filler metal for ASTM A182 F22 and equivalent forgings and tubes, in pressure vessels, reactors and high-temperature steam lines.

Why is the composition of ER90S-B3 different from the material it welds?

The alloy is the same as F22, but the wire has carbon controlled within a narrow range and higher silicon for deoxidation. This balances hot strength after PWHT with a lower tendency to solidification and reheat cracking.

Which covered electrode corresponds to ER90S-B3?

E9018-B3 – AWS A5.5.

What precautions apply when welding with ER90S-B3?

Preheat and interpass of about 200 to 300 °C. PWHT typically between 690 and 750 °C. For high-pressure hydrogen service, require control of residuals (Bruscato X factor) on the certificate. TIG with pure argon; MIG/MAG with argon and 2–5 % O2 or up to 20 % CO2*. Clean, dry wire and bevel to limit hydrogen.

Need ER90S-B3?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)