Dustre
EN
Customer area

ER385 – wire and rod for 904L stainless

Super-austenitic 20Cr-25Ni-4.5Mo-1.5Cu filler metal for 904L stainless, applied in sulfuric acid, phosphoric acid and chloride media.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER385
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSN08904
GroupAustenitic stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER385
Solid MIG/MAG wire (GMAW) ER385
Covered electrode (SMAW) E385-16/-17 – AWS A5.4
Submerged arc wire (SAW) ER385 + flux
Designations and equivalents
DesignationValue
AWS ER385
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS N08904
Others EN ISO 14343-A: W/G 20 25 5 Cu L; W.Nr. 1.4519

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.025
Cr 19.5 – 21.5
Ni 24.0 – 26.0
Mo 4.2 – 5.2
Cu 1.2 – 2.0
Mn 1.0 – 2.5
Si ≤ 0.50
P ≤ 0.02
S ≤ 0.03

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 520 MPa (AWS A5.4 minimum for E385, reference)
Elongation ≥ 30 % (AWS A5.4 minimum for E385, reference)

Materials welded with ER385

Dissimilar joints: For very aggressive chloride media, 904L joints are often also made with ERNiCrMo-3, which better compensates for molybdenum segregation.

Why the composition differs from the base metal

Phosphorus and silicon are limited more strictly than in the base metal because the bead is fully austenitic and those elements promote hot cracking. Molybdenum is slightly above 904L to compensate for segregation during solidification.

Welding precautions

  • No preheating; maximum interpass around 100 °C.
  • Low heat input and narrow beads; avoid wide weaving.
  • Shielding and purging with pure argon; pickle after welding to restore the passive layer.

Frequently asked questions

What is ER385 used for?

Super-austenitic 20Cr-25Ni-4.5Mo-1.5Cu filler metal for 904L stainless, applied in sulfuric acid, phosphoric acid and chloride media.

Why is the composition of ER385 different from the material it welds?

Phosphorus and silicon are limited more strictly than in the base metal because the bead is fully austenitic and those elements promote hot cracking. Molybdenum is slightly above 904L to compensate for segregation during solidification.

Which covered electrode corresponds to ER385?

E385-16/-17 – AWS A5.4.

What precautions apply when welding with ER385?

No preheating; maximum interpass around 100 °C. Low heat input and narrow beads; avoid wide weaving. Shielding and purging with pure argon; pickle after welding to restore the passive layer.

Need ER385?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)