ER317L – wire and rod for 317L stainless

Austenitic filler metal with 3–4 % molybdenum, indicated for 317L stainless and for welding 316L when more margin against pitting is wanted.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER317L
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS31783
GroupAustenitic stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER317L
Solid MIG/MAG wire (GMAW) ER317L
Covered electrode (SMAW) E317L-16/-17 – AWS A5.4
Flux-cored wire (FCAW) E317LT0-1/-4 – AWS A5.22
Submerged arc wire (SAW) ER317L + flux
Designations and equivalents
DesignationValue
AWS ER317L
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S31783
Others EN ISO 14343-A: W/G 18 15 3 L (aproximado)*

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.03
Cr 18.5 – 20.5
Ni 13.0 – 15.0
Mo 3.0 – 4.0
Mn 1.0 – 2.5
Si 0.30 – 0.65
P ≤ 0.03
S ≤ 0.03
Cu ≤ 0.75

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 520 MPa (AWS A5.4 minimum for E317L, reference)
Elongation ≥ 30 % (AWS A5.4 minimum for E317L, reference)

Materials welded with ER317L

Why the composition differs from the base metal

Molybdenum segregates during solidification and leaves depleted regions between the dendrites. ER317L has the same Mo range as the base metal (3.0–4.0 %), so the bead may be slightly less pitting resistant than the plate. When that matters, an over-alloyed consumable is used, such as ER317LMn or a nickel alloy (ERNiCrMo-3).

Welding precautions

  • No preheating; interpass up to 150 °C.
  • Low to moderate heat input to limit Mo segregation.
  • TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes.

Frequently asked questions

What is ER317L used for?

Austenitic filler metal with 3–4 % molybdenum, indicated for 317L stainless and for welding 316L when more margin against pitting is wanted.

Why is the composition of ER317L different from the material it welds?

Molybdenum segregates during solidification and leaves depleted regions between the dendrites. ER317L has the same Mo range as the base metal (3.0–4.0 %), so the bead may be slightly less pitting resistant than the plate. When that matters, an over-alloyed consumable is used, such as ER317LMn or a nickel alloy (ERNiCrMo-3).

Which covered electrode corresponds to ER317L?

E317L-16/-17 – AWS A5.4.

What precautions apply when welding with ER317L?

No preheating; interpass up to 150 °C. Low to moderate heat input to limit Mo segregation. TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes.

Need ER317L?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)