ERNiCrMo-7 – wire and rod for Hastelloy C-4

Ni-16Cr-16Mo filler metal with titanium, for alloy C-4, chosen when the equipment spends long periods at temperatures of 650 to 1040 °C without losing corrosion resistance.

Technical review Oct 2026 · composition per AWS A5.14/A5.14M; values marked * to be confirmed in the current edition of the standard

ClassificationERNiCrMo-7
StandardAWS A5.14/A5.14M / ASME SFA-5.14
UNSN06455
GroupNickel alloy

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ERNiCrMo-7
Solid MIG/MAG wire (GMAW) ERNiCrMo-7
Covered electrode (SMAW) ENiCrMo-7 – AWS A5.11
Designations and equivalents
DesignationValue
AWS ERNiCrMo-7
Specification AWS A5.14/A5.14M / ASME SFA-5.14
UNS N06455
Others EN ISO 18274: S Ni 6455 (NiCr16Mo16Ti); W.Nr. 2.4611*
Trade designation Liga C-4 / Hastelloy C-4 (designação de material)

Chemical composition (%)

AWS A5.14 (% by mass, filler metal)
Elementwt. %
C ≤ 0.015
Cr 14.0 – 18.0
Mo 14.0 – 18.0
Ti ≤ 0.70
Fe ≤ 3.0
Co ≤ 2.0
W ≤ 0.50
Ni Balance
Mn ≤ 1.0
Si ≤ 0.08
Cu ≤ 0.50
P ≤ 0.04
S ≤ 0.03

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 690 MPa (AWS A5.11 minimum for ENiCrMo-7, reference)
Elongation ≥ 25 % (AWS A5.11 minimum for ENiCrMo-7, reference)

Materials welded with ERNiCrMo-7

Why the composition differs from the base metal

It follows the chemistry of C-4, but with carbon and silicon as low as possible and no significant tungsten. The idea is the same as in the base metal: remove the elements that form carbides and intermetallic phases, so that the bead stays stable even after exposure to high temperatures.

Welding precautions

  • No preheating; interpass below 100–150 °C.
  • Low heat input and narrow beads.
  • TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Frequently asked questions

What is ERNiCrMo-7 used for?

Ni-16Cr-16Mo filler metal with titanium, for alloy C-4, chosen when the equipment spends long periods at temperatures of 650 to 1040 °C without losing corrosion resistance.

Why is the composition of ERNiCrMo-7 different from the material it welds?

It follows the chemistry of C-4, but with carbon and silicon as low as possible and no significant tungsten. The idea is the same as in the base metal: remove the elements that form carbides and intermetallic phases, so that the bead stays stable even after exposure to high temperatures.

Which covered electrode corresponds to ERNiCrMo-7?

ENiCrMo-7 – AWS A5.11.

What precautions apply when welding with ERNiCrMo-7?

No preheating; interpass below 100–150 °C. Low heat input and narrow beads. TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Need ERNiCrMo-7?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)