ERNiFeCr-2 – wire and rod for Inconel 718

Precipitation-hardenable Ni-19Cr-18Fe-5Nb-3Mo filler metal, for welding alloy 718 in aerospace, oil and gas and high-strength components.

Technical review Oct 2026 · composition per AWS A5.14/A5.14M; values marked * to be confirmed in the current edition of the standard

ClassificationERNiFeCr-2
StandardAWS A5.14/A5.14M / ASME SFA-5.14
UNSN07718
GroupNickel alloy

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ERNiFeCr-2
Solid MIG/MAG wire (GMAW) ERNiFeCr-2
Designations and equivalents
DesignationValue
AWS ERNiFeCr-2
Specification AWS A5.14/A5.14M / ASME SFA-5.14
UNS N07718
Others EN ISO 18274: S Ni 7718 (NiFe19Cr19Nb5Mo3); W.Nr. 2.4667
Trade designation Liga 718 / Inconel 718 (designação de material)

Chemical composition (%)

AWS A5.14 (% by mass, filler metal)
Elementwt. %
C ≤ 0.08
Ni 50.0 – 55.0
Cr 17.0 – 21.0
Nb + Ta 4.75 – 5.50
Mo 2.80 – 3.30
Ti 0.65 – 1.15
Al 0.20 – 0.80
Fe Balance
Mn ≤ 0.35
Si ≤ 0.35
Cu ≤ 0.30*
B ≤ 0.006*
P ≤ 0.015
S ≤ 0.015

Materials welded with ERNiFeCr-2

Why the composition differs from the base metal

It is one of the few cases where the wire has practically the same chemistry as the base metal, because the goal is for the bead to also precipitation harden (gamma double prime) during aging. The limits for C, Si, P, S and B are the same as alloy 718; control of solidification cracking and Laves phase in the bead comes from the procedure (low heat input and controlled interpass), not from a different chemistry.

Welding precautions

  • Weld the part in the solution-treated condition; after welding, solution treat and age per the part specification to obtain strength close to the base metal.
  • Low heat input and fast cooling limit niobium segregation (Laves phase).
  • TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Frequently asked questions

What is ERNiFeCr-2 used for?

Precipitation-hardenable Ni-19Cr-18Fe-5Nb-3Mo filler metal, for welding alloy 718 in aerospace, oil and gas and high-strength components.

Why is the composition of ERNiFeCr-2 different from the material it welds?

It is one of the few cases where the wire has practically the same chemistry as the base metal, because the goal is for the bead to also precipitation harden (gamma double prime) during aging. The limits for C, Si, P, S and B are the same as alloy 718; control of solidification cracking and Laves phase in the bead comes from the procedure (low heat input and controlled interpass), not from a different chemistry.

What precautions apply when welding with ERNiFeCr-2?

Weld the part in the solution-treated condition; after welding, solution treat and age per the part specification to obtain strength close to the base metal. Low heat input and fast cooling limit niobium segregation (Laves phase). TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Need ERNiFeCr-2?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)