Dustre
EN
Customer area

ER308L – wire and rod for 304L stainless

Low-carbon 19Cr-10Ni austenitic filler metal, the standard for welding 304 and 304L stainless steels in process equipment, piping and structures.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER308L
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS30883
GroupAustenitic stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER308L
Solid MIG/MAG wire (GMAW) ER308L / ER308LSi
Covered electrode (SMAW) E308L-16/-17 – AWS A5.4
Flux-cored wire (FCAW) E308LT0-1/-4 – AWS A5.22
Submerged arc wire (SAW) ER308L + flux
Designations and equivalents
DesignationValue
AWS ER308L
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S30883
Others EN ISO 14343-A: W/G 19 9 L; W.Nr. 1.4316

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.03
Cr 19.5 – 22.0
Ni 9.0 – 11.0
Mo ≤ 0.75
Mn 1.0 – 2.5
Si 0.30 – 0.65
P ≤ 0.03
S ≤ 0.03
Cu ≤ 0.75

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 520 MPa (AWS A5.4 minimum for E308L, reference)
Elongation ≥ 35 % (AWS A5.4 minimum for E308L, reference)

Materials welded with ER308L

Why the composition differs from the base metal

The wire has slightly more chromium than 304L to form 3 to 10 % delta ferrite in the bead. That small fraction of ferrite prevents hot cracking during solidification, something a 100 % austenitic deposit with the same chemistry as the plate could not do.

Welding precautions

  • Does not require preheating; keep interpass below 150 °C.
  • Use moderate heat input to limit sensitization and distortion.
  • TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes.
  • Clean with a stainless steel brush dedicated to stainless to avoid iron contamination.

Frequently asked questions

What is ER308L used for?

Low-carbon 19Cr-10Ni austenitic filler metal, the standard for welding 304 and 304L stainless steels in process equipment, piping and structures.

Why is the composition of ER308L different from the material it welds?

The wire has slightly more chromium than 304L to form 3 to 10 % delta ferrite in the bead. That small fraction of ferrite prevents hot cracking during solidification, something a 100 % austenitic deposit with the same chemistry as the plate could not do.

Which covered electrode corresponds to ER308L?

E308L-16/-17 – AWS A5.4.

What precautions apply when welding with ER308L?

Does not require preheating; keep interpass below 150 °C. Use moderate heat input to limit sensitization and distortion. TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes. Clean with a stainless steel brush dedicated to stainless to avoid iron contamination.

Need ER308L?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)