ER80S-D2 – Mn-Mo wire and rod for 4140, 4340 and C-½Mo steels

High-strength Mn-Mo filler metal, used in repairs and joints of quenched and tempered steels such as 4140, 4340 and 9315, and on C-½Mo steel (F1).

Technical review Oct 2026 · composition per AWS A5.28/A5.28M; values marked * to be confirmed in the current edition of the standard

ClassificationER80S-D2
StandardAWS A5.28/A5.28M / ASME SFA-5.28
UNSK10945
GroupCarbon and low-alloy steel

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER80S-D2
Solid MIG/MAG wire (GMAW) ER80S-D2
Covered electrode (SMAW) E9018-D1 – AWS A5.5 (approximate)*
Submerged arc wire (SAW) EA3K + flux – AWS A5.23 (approximate)*
Designations and equivalents
DesignationValue
AWS ER80S-D2
Specification AWS A5.28/A5.28M / ASME SFA-5.28
UNS K10945
Others EN ISO 14341-A / 21952-A: G 4Mo / W 4Mo (aproximado)*; AWS A5.28M: ER55S-D2

Chemical composition (%)

AWS A5.28 (% by mass, filler metal)
Elementwt. %
C 0.07 – 0.12
Mn 1.60 – 2.10
Si 0.50 – 0.80
Mo 0.40 – 0.60
Ni ≤ 0.15
P ≤ 0.025
S ≤ 0.025
Cu ≤ 0.50

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 550 MPa (AWS minimum)
Yield strength ≥ 470 MPa (AWS minimum)
Elongation ≥ 17 % (AWS minimum)

Materials welded with ER80S-D2

Dissimilar joints: Can join these steels to carbon steel. On quenched and tempered 4140 and 4340, the bead falls below the strength of the base metal; when matching strength is required, the joint must be qualified with a higher-strength wire and full heat treatment.

Why the composition differs from the base metal

The wire has much less carbon than 4140 or 4340 (about 0.1 % versus 0.4 %). A bead with 0.4 % C would harden to a very high hardness and crack; the wire trades carbon for manganese and molybdenum, which give strength without embrittling the weld.

Welding precautions

  • 4140 and 4340 steels: preheat and interpass of about 250 to 350 °C, with post-heating and slow cooling.
  • Temper or PWHT right after welding when the design allows.
  • Nitriding steel (34CrAlNi7): weld only before nitriding; the nitrided case is not weldable.
  • Use dry, clean wire and bevel to limit hydrogen.

Frequently asked questions

What is ER80S-D2 used for?

High-strength Mn-Mo filler metal, used in repairs and joints of quenched and tempered steels such as 4140, 4340 and 9315, and on C-½Mo steel (F1).

Why is the composition of ER80S-D2 different from the material it welds?

The wire has much less carbon than 4140 or 4340 (about 0.1 % versus 0.4 %). A bead with 0.4 % C would harden to a very high hardness and crack; the wire trades carbon for manganese and molybdenum, which give strength without embrittling the weld.

Which covered electrode corresponds to ER80S-D2?

E9018-D1 – AWS A5.5 (approximate)*.

What precautions apply when welding with ER80S-D2?

4140 and 4340 steels: preheat and interpass of about 250 to 350 °C, with post-heating and slow cooling. Temper or PWHT right after welding when the design allows. Nitriding steel (34CrAlNi7): weld only before nitriding; the nitrided case is not weldable. Use dry, clean wire and bevel to limit hydrogen.

Need ER80S-D2?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)