Dustre
EN
Customer area

ER383 – wire and rod for Alloy 28 (UNS N08028)

Super-austenitic 27Cr-31Ni-3.5Mo-1Cu filler metal, with a composition close to alloy N08028, for phosphoric and sulfuric acid equipment and well tubing with H2S.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER383
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSN08028
GroupAustenitic stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER383
Solid MIG/MAG wire (GMAW) ER383
Covered electrode (SMAW) E383-16/-17 – AWS A5.4
Designations and equivalents
DesignationValue
AWS ER383
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS N08028
Others EN ISO 14343-A: W/G 27 31 4 Cu L; W.Nr. 1.4563

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.025
Cr 26.5 – 28.5
Ni 30.0 – 33.0
Mo 3.2 – 4.2
Cu 0.70 – 1.5
Mn 1.0 – 2.5
Si ≤ 0.50
P ≤ 0.02
S ≤ 0.03

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 520 MPa (AWS A5.4 minimum for E383, reference)
Elongation ≥ 30 % (AWS A5.4 minimum for E383, reference)

Materials welded with ER383

Dissimilar joints: In very aggressive chloride media, alloy N08028 is also welded with ERNiCrMo-3.

Why the composition differs from the base metal

The chemistry is almost that of the base metal, but with tighter carbon, phosphorus and silicon. As the bead is fully austenitic, those limits reduce the risk of hot cracking, and Mo is kept at the top of the range to compensate for segregation.

Welding precautions

  • No preheating; interpass up to 100 °C.
  • Low heat input and narrow beads.
  • Pure argon for shielding and purging; pickling after welding.

Frequently asked questions

What is ER383 used for?

Super-austenitic 27Cr-31Ni-3.5Mo-1Cu filler metal, with a composition close to alloy N08028, for phosphoric and sulfuric acid equipment and well tubing with H2S.

Why is the composition of ER383 different from the material it welds?

The chemistry is almost that of the base metal, but with tighter carbon, phosphorus and silicon. As the bead is fully austenitic, those limits reduce the risk of hot cracking, and Mo is kept at the top of the range to compensate for segregation.

Which covered electrode corresponds to ER383?

E383-16/-17 – AWS A5.4.

What precautions apply when welding with ER383?

No preheating; interpass up to 100 °C. Low heat input and narrow beads. Pure argon for shielding and purging; pickling after welding.

Need ER383?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)