Dustre
EN
Customer area

ER2209 – wire and rod for duplex 2205

Duplex 22Cr-9Ni-3Mo-N filler metal, used on duplex 2205 steels (UNS S31803/S32205) and in joints of duplex with austenitic stainless or carbon steel.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER2209
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS39209
GroupDuplex stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER2209
Solid MIG/MAG wire (GMAW) ER2209
Covered electrode (SMAW) E2209-16/-17 – AWS A5.4
Flux-cored wire (FCAW) E2209T0-1/-4 – AWS A5.22
Submerged arc wire (SAW) ER2209 + flux
Designations and equivalents
DesignationValue
AWS ER2209
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S39209
Others EN ISO 14343-A: W/G 22 9 3 N L; W.Nr. 1.4462

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.03
Cr 21.5 – 23.5
Ni 7.5 – 9.5
Mo 2.5 – 3.5
N 0.08 – 0.20
Mn 0.50 – 2.0
Si ≤ 0.90
P ≤ 0.03
S ≤ 0.03
Cu ≤ 0.75

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 690 MPa (AWS A5.4 minimum for E2209, reference)
Elongation ≥ 20 % (AWS A5.4 minimum for E2209, reference)

Materials welded with ER2209

Dissimilar joints: Indicated for joining duplex 2205 to 304L/316L stainless and to carbon steel.

Why the composition differs from the base metal

The wire has about 9 % Ni, versus 5–6 % in 2205. As the bead cools quickly, without the plate's solution annealing, it would tend to end up with too much ferrite; the extra nickel favors austenite and brings the balance closer to 50/50 between the phases.

Welding precautions

  • Typical heat input of 0.5 to 2.5 kJ/mm and maximum interpass of 150 °C to avoid intermetallic phases.
  • TIG with pure argon or argon with up to 2 % N2; purge with argon or argon-nitrogen.
  • Do not weld the root autogenously (without wire): the bead becomes excessively ferritic.
  • Normally there is no preheating or PWHT.

Frequently asked questions

What is ER2209 used for?

Duplex 22Cr-9Ni-3Mo-N filler metal, used on duplex 2205 steels (UNS S31803/S32205) and in joints of duplex with austenitic stainless or carbon steel.

Why is the composition of ER2209 different from the material it welds?

The wire has about 9 % Ni, versus 5–6 % in 2205. As the bead cools quickly, without the plate's solution annealing, it would tend to end up with too much ferrite; the extra nickel favors austenite and brings the balance closer to 50/50 between the phases.

Which covered electrode corresponds to ER2209?

E2209-16/-17 – AWS A5.4.

What precautions apply when welding with ER2209?

Typical heat input of 0.5 to 2.5 kJ/mm and maximum interpass of 150 °C to avoid intermetallic phases. TIG with pure argon or argon with up to 2 % N2; purge with argon or argon-nitrogen. Do not weld the root autogenously (without wire): the bead becomes excessively ferritic. Normally there is no preheating or PWHT.

Need ER2209?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)