ER70S-6 – wire and rod for A105 carbon steel

Carbon steel filler metal with high Si and Mn, the most used for welding carbon steel such as ASTM A105 forged flanges and fittings, plates and structural tubes.

Technical review Oct 2026 · composition per AWS A5.18/A5.18M; values marked * to be confirmed in the current edition of the standard

ClassificationER70S-6
StandardAWS A5.18/A5.18M / ASME SFA-5.18
UNSK11140
GroupCarbon and low-alloy steel

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER70S-6
Solid MIG/MAG wire (GMAW) ER70S-6
Covered electrode (SMAW) E7018 – AWS A5.1 (electrode of the same strength class)
Flux-cored wire (FCAW) E71T-1C/-1M – AWS A5.20
Submerged arc wire (SAW) EM12K + flux – AWS A5.17
Designations and equivalents
DesignationValue
AWS ER70S-6
Specification AWS A5.18/A5.18M / ASME SFA-5.18
UNS K11140
Others EN ISO 14341-A: G 42 x x G3Si1 / G4Si1 (aproximado)*; AWS A5.18M: ER48S-6

Chemical composition (%)

AWS A5.18 (% by mass, filler metal)
Elementwt. %
C 0.06 – 0.15
Mn 1.40 – 1.85
Si 0.80 – 1.15
P ≤ 0.025
S ≤ 0.035
Ni ≤ 0.15
Cr ≤ 0.15
Mo ≤ 0.15
V ≤ 0.03
Cu ≤ 0.50

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 480 MPa (AWS minimum)
Yield strength ≥ 400 MPa (AWS minimum)
Elongation ≥ 22 % (AWS minimum)

Materials welded with ER70S-6

Dissimilar joints: To join A105 to stainless, use ER309L; at elevated temperature, ERNiCr-3.

Why the composition differs from the base metal

The wire has much more silicon and manganese than A105. These elements are deoxidizers: they react with the oxygen from the shielding gas and from a slightly oxidized surface, preventing porosity and leaving the bead with a strength equal to or higher than that of the forging.

Welding precautions

  • Preheat according to thickness and carbon equivalent; on thick A105, typically 80–150 °C.
  • MAG with pure CO2 or argon with 10–25 % CO2; TIG with pure argon.
  • For A105 in H2S service (NACE), control the hardness of the joint.

Frequently asked questions

What is ER70S-6 used for?

Carbon steel filler metal with high Si and Mn, the most used for welding carbon steel such as ASTM A105 forged flanges and fittings, plates and structural tubes.

Why is the composition of ER70S-6 different from the material it welds?

The wire has much more silicon and manganese than A105. These elements are deoxidizers: they react with the oxygen from the shielding gas and from a slightly oxidized surface, preventing porosity and leaving the bead with a strength equal to or higher than that of the forging.

Which covered electrode corresponds to ER70S-6?

E7018 – AWS A5.1 (electrode of the same strength class).

What precautions apply when welding with ER70S-6?

Preheat according to thickness and carbon equivalent; on thick A105, typically 80–150 °C. MAG with pure CO2 or argon with 10–25 % CO2; TIG with pure argon. For A105 in H2S service (NACE), control the hardness of the joint.

Need ER70S-6?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)