Dustre
EN
Customer area

ER209 – wire and rod for Nitronic 50 (XM-19)

Manganese- and nitrogen-bearing austenitic filler metal (22Cr-11Ni-5Mn-2Mo-N), made to weld the high-strength stainless UNS S20910.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER209
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS20980
GroupAustenitic stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER209
Solid MIG/MAG wire (GMAW) ER209
Covered electrode (SMAW) E209-15/-16 – AWS A5.4
Designations and equivalents
DesignationValue
AWS ER209
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S20980
Trade designation 22-13-5 / XM-19 (designação de material)

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.05
Cr 20.5 – 24.0
Ni 9.5 – 12.0
Mo 1.5 – 3.0
Mn 4.0 – 7.0
N 0.10 – 0.30
V 0.10 – 0.30
Si ≤ 0.90
P ≤ 0.03
S ≤ 0.03
Cu ≤ 0.75

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 690 MPa (AWS A5.4 minimum for E209, reference)
Elongation ≥ 15 % (AWS A5.4 minimum for E209, reference)

Materials welded with ER209

Why the composition differs from the base metal

The wire repeats the concept of the base metal (Mn and N in place of part of the Ni), but with ranges adjusted so that the nitrogen stays in the bead without causing porosity. The deposit thus keeps a mechanical strength close to that of the bar, which a 316L would not give.

Welding precautions

  • No preheating; interpass up to 150 °C.
  • Avoid gases with nitrogen or high CO2; use pure argon in TIG.
  • Moderate heat input to preserve nitrogen and toughness.

Frequently asked questions

What is ER209 used for?

Manganese- and nitrogen-bearing austenitic filler metal (22Cr-11Ni-5Mn-2Mo-N), made to weld the high-strength stainless UNS S20910.

Why is the composition of ER209 different from the material it welds?

The wire repeats the concept of the base metal (Mn and N in place of part of the Ni), but with ranges adjusted so that the nitrogen stays in the bead without causing porosity. The deposit thus keeps a mechanical strength close to that of the bar, which a 316L would not give.

Which covered electrode corresponds to ER209?

E209-15/-16 – AWS A5.4.

What precautions apply when welding with ER209?

No preheating; interpass up to 150 °C. Avoid gases with nitrogen or high CO2; use pure argon in TIG. Moderate heat input to preserve nitrogen and toughness.

Need ER209?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)