ER316L – wire and rod for 316L and 316Ti stainless

Austenitic filler metal with 2–3 % molybdenum and low carbon, used on 316, 316L and 316Ti stainless steels where chlorides and organic acids are present.

Technical review Oct 2026 · composition per AWS A5.9/A5.9M; values marked * to be confirmed in the current edition of the standard

ClassificationER316L
StandardAWS A5.9/A5.9M / ASME SFA-5.9
UNSS31683
GroupAustenitic stainless

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ER316L
Solid MIG/MAG wire (GMAW) ER316L / ER316LSi
Covered electrode (SMAW) E316L-16/-17 – AWS A5.4
Flux-cored wire (FCAW) E316LT0-1/-4 – AWS A5.22
Submerged arc wire (SAW) ER316L + flux
Designations and equivalents
DesignationValue
AWS ER316L
Specification AWS A5.9/A5.9M / ASME SFA-5.9
UNS S31683
Others EN ISO 14343-A: W/G 19 12 3 L; W.Nr. 1.4430

Chemical composition (%)

AWS A5.9 (% by mass, filler metal)
Elementwt. %
C ≤ 0.03
Cr 18.0 – 20.0
Ni 11.0 – 14.0
Mo 2.0 – 3.0
Mn 1.0 – 2.5
Si 0.30 – 0.65
P ≤ 0.03
S ≤ 0.03
Cu ≤ 0.75

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 490 MPa (AWS A5.4 minimum for E316L, reference)
Elongation ≥ 30 % (AWS A5.4 minimum for E316L, reference)

Materials welded with ER316L

Dissimilar joints: Can join 316L to 304L when the joint requires the corrosion resistance of the molybdenum-bearing side.

Why the composition differs from the base metal

Chromium and nickel are adjusted to produce a few percent of ferrite in the bead, which reduces the risk of hot cracking. In the case of 316Ti, the titanium of the base metal is not repeated in the wire because it is lost in the arc; it is the low carbon that guarantees intergranular corrosion resistance.

Welding precautions

  • No preheating; interpass up to 150 °C.
  • TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes.
  • For medical-grade 316LVM, confirm with the design whether welding is allowed, since the bead does not have the same purity as the vacuum-remelted material.

Frequently asked questions

What is ER316L used for?

Austenitic filler metal with 2–3 % molybdenum and low carbon, used on 316, 316L and 316Ti stainless steels where chlorides and organic acids are present.

Why is the composition of ER316L different from the material it welds?

Chromium and nickel are adjusted to produce a few percent of ferrite in the bead, which reduces the risk of hot cracking. In the case of 316Ti, the titanium of the base metal is not repeated in the wire because it is lost in the arc; it is the low carbon that guarantees intergranular corrosion resistance.

Which covered electrode corresponds to ER316L?

E316L-16/-17 – AWS A5.4.

What precautions apply when welding with ER316L?

No preheating; interpass up to 150 °C. TIG shielding with pure argon; in MIG/MAG use argon with 1–2 % O2 or 2–3 % CO2. Argon root purge in tubes. For medical-grade 316LVM, confirm with the design whether welding is allowed, since the bead does not have the same purity as the vacuum-remelted material.

Need ER316L?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)