Dustre
EN
Customer area

Titanium Grade 5 (Ti-6Al-4V) – UNS R56400

High-strength alpha-beta titanium alloy

Download data sheet (PDF)

Alpha-beta alloy with 6% Al and 4% V, the most used titanium alloy in the world. It combines a tensile strength ≥ 895 MPa with a density of 4.43 g/cm³ and good corrosion and fatigue resistance. It can be used annealed or solution treated and aged (STA); the ELI version (Gr 23) is the reference for implants.

Technical review Oct 2026 · minimum values per the cited standard; physical properties are typical; values marked * to be confirmed in the standard

FamilyTitanium
UNSR56400 (ELI: R56401)
W.Nr. / EN3.7164 / 3.7165 (TiAl6V4)

Designations and equivalents

Designations of Titanium Grade 5 (Ti-6Al-4V) – UNS R56400
SystemDesignation
UNS R56400 (ELI: R56401)
W.Nr./EN 3.7164 / 3.7165 (TiAl6V4)
DIN TiAl6V4
JIS JIS H 4650 Class 60 (Ti-6Al-4V)
Trade names Ti 6-4, Ti64, Ti-6Al-4V
Others GB TC4; BS 2TA10-13 / TA28; AMS 4928 / 4911

Standards by product form

Standards for Titanium Grade 5 (Ti-6Al-4V) – UNS R56400
FormStandard
Bar ASTM B348 Gr 5 / AMS 4928
Plate ASTM B265 Gr 5 / AMS 4911
Forging ASTM B381 F-5 / AMS 4928
Tube ASTM B861 Gr 5
Wire ASTM B863 Gr 5
Implant ASTM F1472 (Gr 5) / F136 (ELI)

Tolerances and HS codes

  • Forged bars (round and square): machining allowance from 2 mm (Ø 6–16 mm) to 24 mm (Ø 400–500 mm) on the diameter. E.g. Ø 100–125 mm finished: +7 mm, tolerance +6 / −0 (length up to 3,500 mm).
  • Forged discs: allowance of 4 to 9 mm on the diameter and 3 to 11 mm on the height, plus-only tolerance.
  • Cutting and machining: band saw −0 / +5 to +15 mm on length; waterjet +10 % of thickness on the diameter (min. 2 mm); machined parts −0 / +2 to +5 mm on the diameter. See the full tables (INF 002 and INF 003, the same for every alloy).
Tariff classification of Titanium Grade 5 (Ti-6Al-4V): NCM, HS, HTS and CN by product form
FormNCM (Brazil, 8 digits)HS (international, 6 digits)HTS (USA, 10 digits)*CN (European Union, 8 digits)*
Forged bar8108.90.008108.908108.90.60318108 90 30
Hot-rolled bar8108.90.008108.908108.90.60318108 90 30
Plate (> 10 mm, width ≥ 600 mm)8108.90.008108.908108.90.60458108 90 50
Seamless pipe8108.90.008108.908108.90.60608108 90 60
Welded pipe8108.90.008108.908108.90.60608108 90 60
Flange and fitting8108.90.008108.908108.90.30608108 90 90

Tariff class: titanium (by chemical composition, under the Chapter 72 Notes and Section XV Note 5).

*: US and EU codes for reference. NCM per current legislation (General Rules of Interpretation, Notes to Chapters 72, 74 and 75 and Section XV Note 5). Confirm the final code with your customs broker according to the item size and finish. HS = first 6 digits of the NCM.

Chemical composition (%)

ASTM B348 Gr 5 (% by mass)

Chemical composition of Titanium Grade 5 (Ti-6Al-4V) – UNS R56400, per ASTM B348 Gr 5 (% by mass)
ElementRange (%)
Al 5.50 – 6.75
V 3.5 – 4.5
Fe ≤ 0.40
O ≤ 0.20
C ≤ 0.08
N ≤ 0.05
H ≤ 0.015
Y ≤ 0.005
Residuals (each / total) ≤ 0.10 / ≤ 0.40
Ti balance

Mechanical properties

annealed (ASTM B348, room temperature)

Mechanical properties of Titanium Grade 5 (Ti-6Al-4V) – UNS R56400
PropertyValue
Yield strength (0.2%) ≥ 828 MPa
Tensile strength ≥ 895 MPa
Elongation (4D) ≥ 10%
Reduction of area ≥ 25%
Hardness ≈ 334 HB / 36 HRC (typical)
STA condition tensile ≈ 1,000 – 1,170 MPa (typical, thin sections)

Typical physical properties

Typical values at 20 °C
PropertyValue
Density 4.43 g/cm³
Melting range 1,604 – 1,660 °C
Modulus of elasticity ≈ 114 GPa
Thermal conductivity (20 °C) ≈ 6.7 W/m·K
Thermal expansion (20–100 °C) ≈ 8.6 µm/m·K
Beta transus ≈ 980 – 995 °C

Calculate the weight of Titanium Grade 5 (Ti-6Al-4V) bar, plate or pipe →

Heat treatment, welding and machining

ItemUsual practice
Service temperature Usual structural use up to ~400 °C; useful creep resistance up to ~300 – 350 °C. ELI version preferred for cryogenic service.
Heat treatment Mill annealing 705 – 790 °C, 1 – 4 h, air. Stress relief 480 – 650 °C, 1 – 4 h. STA: solution treatment 900 – 955 °C (below the beta transus), water quench, aging 480 – 595 °C for 4 – 8 h, air.
Welding Weldable by TIG, plasma, laser and electron beam with AWS A5.16 ERTi-5 or ERTi-23 (ELI, better bead toughness). Same rigorous gas shielding as CP Ti; post-weld stress relief (≈ 540 – 650 °C) recommended on critical parts. Bead ductility is lower than that of the base metal.
Machining Difficult: low conductivity concentrates heat at the cutting edge; use sharp carbide, low cutting speed, constant feed and high-pressure coolant.

Plan an open-die forging in Titanium Grade 5 (Ti-6Al-4V): reduction, slenderness and how much material to send →Simulate the cutting plan of the ingot or bar →

Typical applications

  • Aircraft structures, fasteners and landing gear
  • Compressor discs and blades (cold stages)
  • Orthopedic and dental implants (ELI, ASTM F136)
  • Risers, stress joints and offshore drilling components
  • Racing connecting rods, valves and fasteners
  • Pump and valve shafts and components in corrosive media
  • Additive manufacturing (Ti64 powder)

Alternatives: Gr 23 (ELI) for implants, fatigue and cryogenics; Gr 9 (Ti-3Al-2.5V) when cold forming and tube welding are needed; Gr 2 when corrosion dominates and mechanical strength is secondary; Gr 29 (Ti-6Al-4V-Ru) for severe corrosion in oil and gas.

Compare alloys by corrosive medium, concentration and temperature →

Titanium Grade 5 (Ti-6Al-4V): complete guide

What titanium Grade 5 is

Grade 5 belongs to the family of titanium and its alloys, in the alpha-beta group. Aluminum stabilizes the hexagonal alpha phase and hardens the alloy by solid solution; vanadium stabilizes the cubic beta phase and makes the alloy heat treatable and forgeable. The result is about 90% titanium with nearly three times the strength of Grade 2, with the same lightness and corrosion resistance.

Heat treatment and forming

Annealing is done at 705 – 790 °C and stress relief at 480 – 650 °C; solution treatment at 900 – 955 °C followed by water quenching and aging at 480 – 595 °C gives the high-strength STA condition. Machining requires low speed, continuous feed, a rigid tool and abundant coolant.

Corrosion, biocompatibility and limits of use

Corrosion resistance is similar to CP titanium in seawater, chlorides, oxidizing media and organic acids, slightly lower in reducing acids and hot crevices. The alloy does not resist hydrofluoric acid, hot reducing acids, dry chlorine or anhydrous methanol. Under continuous load, use goes up to about 350 to 400 °C.

Applications

Aircraft engine structures and components, high-strength fasteners and shafts, riser and offshore equipment components, highly loaded seawater valves and pumps, high-performance sporting goods, racing automotive components, and implants and surgical instruments in the ELI version.

Supply forms and Dustre services

Round bars cut to size on a band saw, with rough or finish machining and hardness and tensile testing. All material is supplied with a 3.1 inspection certificate and heat traceability.

Frequently asked questions

What is the chemical composition of Titanium Grade 5 (Ti-6Al-4V)?

Per ASTM B348 Gr 5 (% by mass): Al 5.50 – 6.75; V 3.5 – 4.5; Fe ≤ 0.40; O ≤ 0.20; C ≤ 0.08; N ≤ 0.05.

Which standards cover Titanium Grade 5 (Ti-6Al-4V)?

Bar: ASTM B348 Gr 5 / AMS 4928. Plate: ASTM B265 Gr 5 / AMS 4911. Forging: ASTM B381 F-5 / AMS 4928. Tube: ASTM B861 Gr 5. Wire: ASTM B863 Gr 5. Implant: ASTM F1472 (Gr 5) / F136 (ELI).

Up to what temperature can Titanium Grade 5 (Ti-6Al-4V) be used?

Usual structural use up to ~400 °C; useful creep resistance up to ~300 – 350 °C. ELI version preferred for cryogenic service.

Which materials can replace Titanium Grade 5 (Ti-6Al-4V)?

Gr 23 (ELI) for implants, fatigue and cryogenics; Gr 9 (Ti-3Al-2.5V) when cold forming and tube welding are needed; Gr 2 when corrosion dominates and mechanical strength is secondary; Gr 29 (Ti-6Al-4V-Ru) for severe corrosion in oil and gas.

Where to buy Titanium Grade 5 (Ti-6Al-4V) in Brazil?

Dustre supplies Titanium Grade 5 (Ti-6Al-4V) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

Need Titanium Grade 5 (Ti-6Al-4V)?Bars, forgings and parts with EN 10204 3.1 certificate.

Forms and stock of Titanium Grade 5 (Ti-6Al-4V)

Dustre supplies Titanium Grade 5 (Ti-6Al-4V) as bar, plate, pipe and tube and forgings and flanges, cut to size, with forged and machined parts to drawing (shafts, discs, rings and blocks) and a 3.1 certificate.

In stock in Osasco/SP, Brazil: plate from 60 mm and round bar from Ø 9.5 to 38 mm. List updated on 11/13/2026.

See the full ready-to-ship stock · Request a quote for Titanium Grade 5 (Ti-6Al-4V)

Where to buy Titanium Grade 5 (Ti-6Al-4V) in Brazil?

Dustre supplies Titanium Grade 5 (Ti-6Al-4V) as bar, plate, tube, block and forged or machined parts, subject to availability, with a quality certificate. Head office in Osasco/SP, branches in Joinville/SC and Baixo Guandu/ES, delivery across Brazil and export worldwide (export documents and 3.1 certificate; Incoterm agreed in the quote). For a quote, message Helena, our virtual assistant on WhatsApp +55 11 98649-0075, or write to vendas@dustre.com.br.

See also

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)