ERNiCrCoMo-1 – wire and rod for Incoloy 800HT and Inconel 601 at high temperature

Ni-22Cr-12Co-9Mo-Al filler metal for service above about 760 °C, with high creep and oxidation resistance; indicated for 800HT, alloy 601 and joints between heat-resisting alloys.

Technical review Oct 2026 · composition per AWS A5.14/A5.14M; values marked * to be confirmed in the current edition of the standard

ClassificationERNiCrCoMo-1
StandardAWS A5.14/A5.14M / ASME SFA-5.14
UNSN06617
GroupNickel alloy

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ERNiCrCoMo-1
Solid MIG/MAG wire (GMAW) ERNiCrCoMo-1
Covered electrode (SMAW) ENiCrCoMo-1 – AWS A5.11
Designations and equivalents
DesignationValue
AWS ERNiCrCoMo-1
Specification AWS A5.14/A5.14M / ASME SFA-5.14
UNS N06617
Others EN ISO 18274: S Ni 6617 (NiCr22Co12Mo9); W.Nr. 2.4627
Trade designation Liga 617 (designação genérica)

Chemical composition (%)

AWS A5.14 (% by mass, filler metal)
Elementwt. %
C 0.05 – 0.15
Cr 20.0 – 24.0
Co 10.0 – 15.0
Mo 8.0 – 10.0
Al 0.8 – 1.5
Fe ≤ 3.0
Ti ≤ 0.60
Ni Balance
Mn ≤ 1.0
Si ≤ 1.0
Cu ≤ 0.50
P ≤ 0.03
S ≤ 0.015

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 620 MPa (AWS A5.11 minimum for ENiCrCoMo-1, reference)
Elongation ≥ 25 % (AWS A5.11 minimum for ENiCrCoMo-1, reference)

Materials welded with ERNiCrCoMo-1

Dissimilar joints: Used in joints between 800HT, alloy 601, 310 stainless and heat-resisting steels when the service temperature exceeds about 760 °C.

Why the composition differs from the base metal

The wire does not copy 800HT or alloy 601: it is much richer in nickel and carries cobalt and molybdenum. This gives the bead creep resistance equal to or higher than the base metal at high temperature, since an as-welded deposit of the same chemistry would lose strength and ductility in service.

Welding precautions

  • No preheating; interpass below 150 °C.
  • Moderate heat input; the deposit is sensitive to hot cracking if contaminated.
  • TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Frequently asked questions

What is ERNiCrCoMo-1 used for?

Ni-22Cr-12Co-9Mo-Al filler metal for service above about 760 °C, with high creep and oxidation resistance; indicated for 800HT, alloy 601 and joints between heat-resisting alloys.

Why is the composition of ERNiCrCoMo-1 different from the material it welds?

The wire does not copy 800HT or alloy 601: it is much richer in nickel and carries cobalt and molybdenum. This gives the bead creep resistance equal to or higher than the base metal at high temperature, since an as-welded deposit of the same chemistry would lose strength and ductility in service.

Which covered electrode corresponds to ERNiCrCoMo-1?

ENiCrCoMo-1 – AWS A5.11.

What precautions apply when welding with ERNiCrCoMo-1?

No preheating; interpass below 150 °C. Moderate heat input; the deposit is sensitive to hot cracking if contaminated. TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Need ERNiCrCoMo-1?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)