ERNiMo-7 – wire and rod for Hastelloy B-2

Nickel-molybdenum filler metal (28 % Mo) for alloy B-2, used with hydrochloric acid and other strongly reducing media.

Technical review Oct 2026 · composition per AWS A5.14/A5.14M; values marked * to be confirmed in the current edition of the standard

ClassificationERNiMo-7
StandardAWS A5.14/A5.14M / ASME SFA-5.14
UNSN10665
GroupNickel alloy

Product forms and equivalents

ProcessClassification
TIG rod (GTAW) ERNiMo-7
Solid MIG/MAG wire (GMAW) ERNiMo-7
Covered electrode (SMAW) ENiMo-7 – AWS A5.11
Designations and equivalents
DesignationValue
AWS ERNiMo-7
Specification AWS A5.14/A5.14M / ASME SFA-5.14
UNS N10665
Others EN ISO 18274: S Ni 1066 (NiMo28); W.Nr. 2.4615
Trade designation Liga B-2 / Hastelloy B-2 (designação de material)

Chemical composition (%)

AWS A5.14 (% by mass, filler metal)
Elementwt. %
C ≤ 0.02
Mo 26.0 – 30.0
Fe ≤ 2.0
Cr ≤ 1.0
Co ≤ 1.0
W ≤ 1.0
Ni Balance
Mn ≤ 1.0
Si ≤ 0.10
Cu ≤ 0.50
P ≤ 0.04
S ≤ 0.03

Properties of the deposited metal

PropertyValue
Tensile strength of deposited metal ≥ 760 MPa (AWS A5.11 minimum for ENiMo-7, reference)
Elongation ≥ 25 % (AWS A5.11 minimum for ENiMo-7, reference)

Materials welded with ERNiMo-7

Why the composition differs from the base metal

The chemistry follows that of alloy B-2, with very low carbon and silicon and limited iron and chromium. Those limits prevent carbides and brittle Ni-Mo phases in the fusion zone, which would cause preferential corrosion of the bead in hydrochloric acid.

Welding precautions

  • No preheating; interpass below 100 °C.
  • Low heat input; the bead does not tolerate oxidizing media or iron contamination well.
  • TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Frequently asked questions

What is ERNiMo-7 used for?

Nickel-molybdenum filler metal (28 % Mo) for alloy B-2, used with hydrochloric acid and other strongly reducing media.

Why is the composition of ERNiMo-7 different from the material it welds?

The chemistry follows that of alloy B-2, with very low carbon and silicon and limited iron and chromium. Those limits prevent carbides and brittle Ni-Mo phases in the fusion zone, which would cause preferential corrosion of the bead in hydrochloric acid.

Which covered electrode corresponds to ERNiMo-7?

ENiMo-7 – AWS A5.11.

What precautions apply when welding with ERNiMo-7?

No preheating; interpass below 100 °C. Low heat input; the bead does not tolerate oxidizing media or iron contamination well. TIG with pure argon or argon-helium; argon root purge. Rigorous cleaning: oil, paint and markers contaminate the nickel alloy with sulfur and lead.

Need ERNiMo-7?Send the base material, the process and the wire or rod diameter.
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)