ASME B16.5 blind flange: dimensions and weight by class

Disc without a central bore that closes the end of lines, nozzles and vessels. Also used as a hydrostatic test point and for future expansion.

Technical review Oct 2026 · Source: ASME B16.5-2020

Blind in section
Blind in section. Bolted to another flange of the same class, with a gasket.
StandardASME B16.5-2020
Classes150, 300, 400, 600, 900, 1,500, 2,500
Range in class 150NPS ½ to 24
Unitsmm, kg; hole and bolt in inches

Dimensions by pressure class

Choose the class and click a row: the drawing changes to the scale and dimensions of that diameter.

Blind, class 150: dimensions in mm · raised face 1.6 mm · all types in class 150
NPSDNOtfRWNo. of holesHole ØBolt ØWeight*
½"15899.735.160.54⅝"½"0.4
¾"209911.242.969.84⅝"½"0.6
1"2510812.750.879.24⅝"½"0.9
1¼"3211714.263.588.94⅝"½"1.1
1½"4012715.97398.64⅝"½"1.5
2"5015217.591.9120.64¾"⅝"2.4
2½"6517820.6104.6139.74¾"⅝"3.9
3"8019022.4127152.44¾"⅝"4.9
3½"9021622.4139.7177.88¾"⅝"6.2
4"10022922.4157.2190.58¾"⅝"7.1
5"12525422.4185.7215.98⅞"¾"8.7
6"15027923.9215.9241.38⅞"¾"11.3
8"20034326.9269.7298.48⅞"¾"19.6
10"25040628.4323.8362.0121"⅞"28.5
12"30048330.2381431.8121"⅞"43.4
14"35053333.3412.8476.2121⅛"1"58
16"40059735.1469.9539.8161⅛"1"76.5
18"45063538.1533.4577.8161¼"1⅛"93.7
20"500698.541.1584.2635.0201¼"1⅛"120
22"55074944.4641.4692.2201⅜"1¼"151
24"60081346.0692.2749.3201⅜"1¼"185.3
Scale drawing

Section drawing, proportional to the table dimensions (mm).

O = outside diameter · tf = thickness without raised face · R = raised face diameter · W = bolt circle. * Weight estimated from geometry in carbon steel.

Frequently asked questions

What is the asme b16.5 blind flange: dimensions and weight by class used for?

Disc without a central bore that closes the end of lines, nozzles and vessels. Also used as a hydrostatic test point and for future expansion.

Do the dimensions include the raised face?

No. Since the 2017 edition, the thickness (tf) and length (Y) in ASME B16.5 are measured without the raised face. Add 1.6 mm for classes 150 and 300 and 6.4 mm from class 400 upward.

In which materials does Dustre supply it?

A105 and A350 LF2 carbon steel, F304L and F316L stainless, F51/F60 duplex, F53/F55 super duplex, F11, F22 and F91 Cr-Mo, nickel alloys and titanium, forged and machined with 3.1 certificate.

Blind in special alloysForged and machined at Dustre, in any class, with 3.1 certificate.
Request a quote
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)