ASME B16.5 class 900 (900 lb) flange: dimensions, bolt pattern and weight

All class 900 flange types on one page: weld neck, slip-on, socket weld, threaded, lap joint and blind. Dimensions in millimeters per ASME B16.5 2020 edition, bolts in inches.

Technical review Oct 2026 · Source: ASME B16.5-2020

RangeNPS ½ to 24
Pressure, A105 at 38 °C153.2 bar
Standard raised face (RF)6.4 mm
TypesWN · SO · SW · TH · LJ · BL

Types and range in class 900

ASME B16.5 class 900 flange types and diameter range
TypeCodeRange
Weld neckWNNPS ½ to 24
Slip-onSONPS ½ to 24
Socket weldSWNPS ½ to 2½
ThreadedTHNPS ½ to 24
Lap jointLJNPS ½ to 24
BlindBLNPS ½ to 24
Section of a weld neck flange with dimensions O, tf, R, W, X, Ah, Y and B ORWX tfYAhB pipe axis
Section of the weld neck (WN) flange. O outside diameter · tf thickness · R raised face · W bolt circle · X hub at base · Ah diameter at bevel · Y length · B bore.

Up to NPS 2½, ASME B16.5 requires class 900 to use the same dimensions as class 1500. In the tables these rows appear with "= 1500" next to the NPS.

General dimensions and weld neck (WN) flange

Class 900 flange: dimensions in mm, weight in kg (estimated*)
NPSDNOtfRXAhY WNB WNWN weight*Blind weight*
½" = 15001512122.435.13821.360customer1.91.8
¾" = 15002013025.442.94426.770customer2.62.4
1" = 15002514928.450.85233.573customer3.73.5
1¼" = 15003215928.463.56442.273customer4.34.1
1½" = 15004017831.8737048.383customer65.8
2" = 15005021638.191.910560.5102customer1110.1
2½" = 15006524441.1104.612473.2105customer15.113.9
3"8024138.112712788.9102customer13.613.1
4"10029244.5157.2159114.3114customer22.422.2
5"12534950.8185.7190141.2127customer35.936.5
6"15038155.6215.9235168.4140customer47.447.5
8"20047063.5269.7298219.2162customer80.882.5
10"25054669.8323.8368273.0184customer119.3122.4
12"30061079.2381419323.8200customer158.3173.2
14"35064185.9412.8451355.6213customer181.1206.3
16"40070588.9469.9508406.4216customer218.2259.5
18"450787101.6533.4565457.2229customer294.2366.9
20"500857108.0584.2622508.0248customer365.2463.7
24"6001041139.7692.2749609.6292customer668.9875.7

Slip-on, socket weld, threaded and lap joint

Class 900 flange: lengths and bores by type, in mm
NPS Y SO / SW / TH B SO / SW D socket T threadQ counterbore Y LJB LJr LJ SO weight*
½" = 1500 3222.410 2223.6 3222.93 1.8
¾" = 1500 3527.711 2529.0 3528.23 2.3
1" = 1500 4134.513 2835.8 4135.43 3.4
1¼" = 1500 4143.214 3044.4 4143.75 3.9
1½" = 1500 4449.516 3250.5 4450.06 5.4
2" = 1500 5762.018 3863.5 5762.58 9.8
2½" = 1500 6474.719 4876.2 6475.48 13.5
3" 5490.7– 4192.2 5491.410 11.5
4" 70116.1– 48117.6 70116.811 19.6
5" 79143.8– 54144.5 79144.511 31.6
6" 86170.7– 57171.4 86171.413 40.9
8" 102221.5– 64222.2 114222.213 70.2
10" 108276.4– 71276.4 127277.413 99.6
12" 117327.2– 76328.7 143328.213 131.8
14" 130359.2– 83360.4 155360.213 151.8
16" 133410.5– 86411.2 165411.213 183.3
18" 152461.8– 89462.0 190462.313 255.6
20" 159513.1– 92512.8 210514.413 314.5
24" 203616.0– 102614.4 267616.013 600.2

Y = overall length without raised face · B = minimum bore · D = socket depth · T = minimum thread length · Q = thread counterbore diameter · r = lap joint bore radius. "–" = type not covered by the standard at this diameter.

Bolt pattern and bolting

Class 900 flange: bolt pattern (mm) and bolts (in)
NPSOW (bolt circle)No. of holesHole ØBolt ØStud bolt, RFStud bolt, RTJ
½" = 150012182.64⅞"¾"110110
¾" = 150013088.94⅞"¾"115115
1" = 1500149101.641"⅞"125125
1¼" = 1500159111.141"⅞"125125
1½" = 1500178124.041⅛"1"140140
2" = 1500216165.181"⅞"145145
2½" = 1500244190.581⅛"1"160160
3"241190.581"⅞"145145
4"292235.081¼"1⅛"170170
5"349279.481⅜"1¼"190190
6"381317.5121¼"1⅛"190195
8"470393.7121½"1⅜"220220
10"546469.9161½"1⅜"235235
12"610533.4201½"1⅜"255255
14"641558.8201⅝"1½"275280
16"705616.0201¾"1⅝"285290
18"787685.8202"1⅞"325335
20"857749.3202⅛"2"350360
24"1041901.7202⅝"2½"440455

Stud bolt length in mm, excluding the ends. Ring type joints (RTJ) use a longer stud in almost all diameters.

Allowable pressure of class 900 (bar)

Working pressure of class 900 by material group and temperature
Material (group)−29 to 38 °C100 °C200 °C300 °C400 °C
Carbon steel A105 / A350 LF2 (1.1)153.2139.8131.4119.5104.2
Stainless F304 / F304H (2.1)148.9122.6103.492.785.3
Stainless F316 / F316H (2.2)148.9126.6107.094.988.3
Duplex F51, super duplex F53 / F55 (up to 315 °C), 6Mo F44 (2.8)155.1152.0128.0116.6109.8
Inconel 625, Incoloy 825, Hastelloy C-276 / C-22 (3.8)155.1154.6145.0128.6109.8

Values from ASME B16.5 tables 2-1.1 to 2-3.8. "–" = material outside the standard's temperature range. For other groups and temperatures, consult engineering.

Table notes

  • Dimensions without the raised face: add 6.4 mm to the thickness (tf) and length (Y) of raised-face flanges.
  • "= 1500" next to the NPS: up to NPS 2½, class 900 uses the same dimensions as class 1500, as the standard requires.
  • * Weight estimated from geometry in carbon steel, with STD bore when the customer does not state the schedule. Stainless weighs about 1 % more; nickel alloys 7 % to 13 % more.
  • "customer" = the WN bore follows the pipe schedule stated in the order.

Frequently asked questions

What does class 900 flange (900#, 900 lb) mean?

It is the ASME B16.5 pressure class. It is not the pressure in psi: it defines an allowable pressure vs. temperature curve for each material group. In A105 carbon steel, class 900 allows 153.2 bar from −29 to 38 °C and less as the temperature rises.

Which flange types exist in class 900?

Weld neck (WN): NPS ½ to 24; Slip-on (SO): NPS ½ to 24; Socket weld (SW): NPS ½ to 2½; Threaded (TH): NPS ½ to 24; Lap joint (LJ): NPS ½ to 24; Blind (BL): NPS ½ to 24.

Do the thickness (tf) and length (Y) include the raised face?

No. Since the 2017 edition, tf and Y are measured without the raised face. In class 900 the standard raised face is 6.4 mm, which is added to the table thickness.

What is the bore (B) of the weld neck flange?

The WN bore follows the pipe wall thickness (schedule). The standard gives the standard-wall (STD) bore only for classes 150 and 300 up to NPS 12; in the other cases the customer states the schedule in the order.

Class 900 flange in any alloyA105, F316L, F51, F53/F55, F22, Inconel 625 and others, forged and machined at Dustre, with 3.1 certificate.
Request a quote
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)