ASME B16.5 class 150 (150 lb) flange: dimensions, bolt pattern and weight

All class 150 flange types on one page: weld neck, slip-on, socket weld, threaded, lap joint and blind. Dimensions in millimeters per ASME B16.5 2020 edition, bolts in inches.

Technical review Oct 2026 · Source: ASME B16.5-2020

RangeNPS ½ to 24
Pressure, A105 at 38 °C19.6 bar
Standard raised face (RF)1.6 mm
TypesWN · SO · SW · TH · LJ · BL

Types and range in class 150

ASME B16.5 class 150 flange types and diameter range
TypeCodeRange
Weld neckWNNPS ½ to 24
Slip-onSONPS ½ to 24
Socket weldSWNPS ½ to 3
ThreadedTHNPS ½ to 24
Lap jointLJNPS ½ to 24
BlindBLNPS ½ to 24
Section of a weld neck flange with dimensions O, tf, R, W, X, Ah, Y and B ORWX tfYAhB pipe axis
Section of the weld neck (WN) flange. O outside diameter · tf thickness · R raised face · W bolt circle · X hub at base · Ah diameter at bevel · Y length · B bore.

General dimensions and weld neck (WN) flange

Class 150 flange: dimensions in mm, weight in kg (estimated*)
NPSDNOtfRXAhY WNB WNWN weight*Blind weight*
½"15899.735.13021.34615.70.50.4
¾"209911.242.93826.75120.80.70.6
1"2510812.750.84933.55426.71.10.9
1¼"3211714.263.55942.25635.11.41.1
1½"4012715.9736548.36040.91.81.5
2"5015217.591.97860.56252.62.72.4
2½"6517820.6104.69073.26862.74.23.9
3"8019022.412710888.96878.05.14.9
3½"9021622.4139.7122101.67090.26.36.2
4"10022922.4157.2135114.375102.47.27.1
5"12525422.4185.7164141.287128.398.7
6"15027923.9215.9192168.487154.21111.3
8"20034326.9269.7246219.2100202.718.219.6
10"25040628.4323.8305273.0100254.524.928.5
12"30048330.2381365323.8113304.838.443.4
14"35053333.3412.8400355.6125customer50.458
16"40059735.1469.9457406.4125customer62.876.5
18"45063538.1533.4505457.2138customer71.293.7
20"500698.541.1584.2559508.0143customer85.8120
22"55074944.4641.4610558.8148customer100.5151
24"60081346.0692.2663609.6151customer119.4185.3

Slip-on, socket weld, threaded and lap joint

Class 150 flange: lengths and bores by type, in mm
NPS Y SO / SW / TH B SO / SW D socket T thread Y LJB LJtf LJr LJ SO weight*
½" 1422.410 16 1622.911.23 0.4
¾" 1427.711 16 1628.212.73 0.6
1" 1634.513 18 1835.114.23 0.8
1¼" 1943.214 21 2143.715.75 1
1½" 2149.516 22 2250.017.56 1.3
2" 2461.918 25 2562.519.08 2.1
2½" 2774.719 28 2875.422.48 3.3
3" 2890.721 30 3091.423.910 3.8
3½" 30103.4– 32 32104.123.910 4.8
4" 32116.1– 33 33116.823.911 5.4
5" 35143.8– 37 37144.523.911 6.1
6" 38170.7– 40 40171.425.413 7.4
8" 43221.5– 44 44222.228.413 12
10" 48276.4– 49 49277.430.213 16.2
12" 54327.2– 56 56328.231.813 26
14" 56359.2– 57 79360.235.113 34.3
16" 62410.5– 64 87411.236.613 44.5
18" 67461.8– 68 97462.339.613 48.3
20" 71513.1– 73 103514.442.913 59
22" 78564.4– – 108565.246.013 70.7
24" 81616.0– 83 111616.047.813 85.7

Y = overall length without raised face · B = minimum bore · D = socket depth · T = minimum thread length · Q = thread counterbore diameter · r = lap joint bore radius. "–" = type not covered by the standard at this diameter.

Bolt pattern and bolting

Class 150 flange: bolt pattern (mm) and bolts (in)
NPSOW (bolt circle)No. of holesHole ØBolt ØStud bolt, RFStud bolt, RTJ
½"8960.54⅝"½"55–
¾"9969.84⅝"½"65–
1"10879.24⅝"½"6575
1¼"11788.94⅝"½"7085
1½"12798.64⅝"½"7085
2"152120.64¾"⅝"8595
2½"178139.74¾"⅝"90100
3"190152.44¾"⅝"90100
3½"216177.88¾"⅝"90100
4"229190.58¾"⅝"90100
5"254215.98⅞"¾"95110
6"279241.38⅞"¾"100115
8"343298.48⅞"¾"110120
10"406362.0121"⅞"115125
12"483431.8121"⅞"120135
14"533476.2121⅛"1"135145
16"597539.8161⅛"1"135145
18"635577.8161¼"1⅛"145160
20"698.5635.0201¼"1⅛"160170
22"749692.2201⅜"1¼"170185
24"813749.3201⅜"1¼"170185

Stud bolt length in mm, excluding the ends. Ring type joints (RTJ) use a longer stud in almost all diameters.

Allowable pressure of class 150 (bar)

Working pressure of class 150 by material group and temperature
Material (group)−29 to 38 °C100 °C200 °C300 °C400 °C
Carbon steel A105 / A350 LF2 (1.1)19.617.713.810.26.5
Stainless F304 / F304H (2.1)19.015.713.210.26.5
Stainless F316 / F316H (2.2)19.016.213.710.26.5
Duplex F51, super duplex F53 / F55 (up to 315 °C), 6Mo F44 (2.8)20.017.713.810.26.5
Inconel 625, Incoloy 825, Hastelloy C-276 / C-22 (3.8)20.017.713.810.26.5

Values from ASME B16.5 tables 2-1.1 to 2-3.8. "–" = material outside the standard's temperature range. For other groups and temperatures, consult engineering.

Table notes

  • Dimensions without the raised face: add 1.6 mm to the thickness (tf) and length (Y) of raised-face flanges.
  • * Weight estimated from geometry in carbon steel, with STD bore when the customer does not state the schedule. Stainless weighs about 1 % more; nickel alloys 7 % to 13 % more.
  • "customer" = the WN bore follows the pipe schedule stated in the order.

Frequently asked questions

What does class 150 flange (150#, 150 lb) mean?

It is the ASME B16.5 pressure class. It is not the pressure in psi: it defines an allowable pressure vs. temperature curve for each material group. In A105 carbon steel, class 150 allows 19.6 bar from −29 to 38 °C and less as the temperature rises.

Which flange types exist in class 150?

Weld neck (WN): NPS ½ to 24; Slip-on (SO): NPS ½ to 24; Socket weld (SW): NPS ½ to 3; Threaded (TH): NPS ½ to 24; Lap joint (LJ): NPS ½ to 24; Blind (BL): NPS ½ to 24.

Do the thickness (tf) and length (Y) include the raised face?

No. Since the 2017 edition, tf and Y are measured without the raised face. In class 150 the standard raised face is 1.6 mm, which is added to the table thickness.

What is the bore (B) of the weld neck flange?

The WN bore follows the pipe wall thickness (schedule). The standard gives the standard-wall (STD) bore only for classes 150 and 300 up to NPS 12; in the other cases the customer states the schedule in the order.

Class 150 flange in any alloyA105, F316L, F51, F53/F55, F22, Inconel 625 and others, forged and machined at Dustre, with 3.1 certificate.
Request a quote
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)