ASME B16.5 class 1500 (1500 lb) flange: dimensions, bolt pattern and weight

All class 1500 flange types on one page: weld neck, slip-on, socket weld, threaded, lap joint and blind. Dimensions in millimeters per ASME B16.5 2020 edition, bolts in inches.

Technical review Oct 2026 · Source: ASME B16.5-2020

RangeNPS ½ to 24
Pressure, A105 at 38 °C255.3 bar
Standard raised face (RF)6.4 mm
TypesWN · SO · SW · TH · LJ · BL

Types and range in class 1500

ASME B16.5 class 1500 flange types and diameter range
TypeCodeRange
Weld neckWNNPS ½ to 24
Slip-onSONPS ½ to 2½
Socket weldSWNPS ½ to 2½
ThreadedTHNPS ½ to 2½
Lap jointLJNPS ½ to 24
BlindBLNPS ½ to 24
Section of a weld neck flange with dimensions O, tf, R, W, X, Ah, Y and B ORWX tfYAhB pipe axis
Section of the weld neck (WN) flange. O outside diameter · tf thickness · R raised face · W bolt circle · X hub at base · Ah diameter at bevel · Y length · B bore.

General dimensions and weld neck (WN) flange

Class 1500 flange: dimensions in mm, weight in kg (estimated*)
NPSDNOtfRXAhY WNB WNWN weight*Blind weight*
½"1512122.435.13821.360customer1.91.8
¾"2013025.442.94426.770customer2.62.4
1"2514928.450.85233.573customer3.73.5
1¼"3215928.463.56442.273customer4.34.1
1½"4017831.8737048.383customer65.8
2"5021638.191.910560.5102customer1110.1
2½"6524441.1104.612473.2105customer15.113.9
3"8026747.812713388.9117customer2019.3
4"10031153.8157.2162114.3124customer29.729.8
5"12537573.2185.7197141.2155customer56.858.7
6"15039482.6215.9229168.4171customer67.772
8"20048391.9269.7292219.2213customer115.1121.6
10"250584108.0323.8368273.0254customer199.8210.6
12"300673124.0381451323.8282customer298.7316.4
14"350749133.4412.8495355.6298customer392.9420.2
16"400826146.0469.9552406.4311customer500.6558.8
18"450914162.1533.4597457.2327customer650.4760.9
20"500984177.8584.2641508.0356customer794.4964.4
24"6001168203.2692.2762609.6406customer1261.81558.1

Slip-on, socket weld, threaded and lap joint

Class 1500 flange: lengths and bores by type, in mm
NPS Y SO / SW / TH B SO / SW D socket T threadQ counterbore Y LJB LJr LJ SO weight*
½" 3222.410 2223.6 3222.93 1.8
¾" 3527.711 2529.0 3528.23 2.3
1" 4134.513 2835.8 4135.43 3.4
1¼" 4143.214 3044.4 4143.75 3.9
1½" 4449.516 3250.5 4450.06 5.4
2" 5762.018 3863.5 5762.58 9.8
2½" 6474.719 4876.2 6475.48 13.5
3" ––– –– 7391.410 –
4" ––– –– 90116.811 –
5" ––– –– 105144.511 –
6" ––– –– 119171.413 –
8" ––– –– 143222.213 –
10" ––– –– 178277.413 –
12" ––– –– 219328.213 –
14" ––– –– 241360.213 –
16" ––– –– 260411.213 –
18" ––– –– 276462.313 –
20" ––– –– 292514.413 –
24" ––– –– 330616.013 –

Y = overall length without raised face · B = minimum bore · D = socket depth · T = minimum thread length · Q = thread counterbore diameter · r = lap joint bore radius. "–" = type not covered by the standard at this diameter.

Bolt pattern and bolting

Class 1500 flange: bolt pattern (mm) and bolts (in)
NPSOW (bolt circle)No. of holesHole ØBolt ØStud bolt, RFStud bolt, RTJ
½"12182.64⅞"¾"110110
¾"13088.94⅞"¾"115115
1"149101.641"⅞"125125
1¼"159111.141"⅞"125125
1½"178124.041⅛"1"140140
2"216165.181"⅞"145145
2½"244190.581⅛"1"160160
3"267203.281¼"1⅛"180180
4"311241.381⅜"1¼"195195
5"375292.181⅝"1½"250250
6"394317.5121½"1⅜"260265
8"483393.7121¾"1⅝"290300
10"584482.6122"1⅞"335345
12"673571.5162⅛"2"375385
14"749635.0162⅜"2¼"405425
16"826704.8162⅝"2½"445470
18"914774.7162⅞"2¾"495525
20"984831.8163⅛"3"540565
24"1168990.6163⅝"3½"615650

Stud bolt length in mm, excluding the ends. Ring type joints (RTJ) use a longer stud in almost all diameters.

Allowable pressure of class 1500 (bar)

Working pressure of class 1500 by material group and temperature
Material (group)−29 to 38 °C100 °C200 °C300 °C400 °C
Carbon steel A105 / A350 LF2 (1.1)255.3233.0219.0199.1173.6
Stainless F304 / F304H (2.1)248.2204.3172.4154.6142.2
Stainless F316 / F316H (2.2)248.2211.0178.3158.1147.2
Duplex F51, super duplex F53 / F55 (up to 315 °C), 6Mo F44 (2.8)258.6253.3213.3194.3183.1
Inconel 625, Incoloy 825, Hastelloy C-276 / C-22 (3.8)258.6257.6241.7214.4183.1

Values from ASME B16.5 tables 2-1.1 to 2-3.8. "–" = material outside the standard's temperature range. For other groups and temperatures, consult engineering.

Table notes

  • Dimensions without the raised face: add 6.4 mm to the thickness (tf) and length (Y) of raised-face flanges.
  • * Weight estimated from geometry in carbon steel, with STD bore when the customer does not state the schedule. Stainless weighs about 1 % more; nickel alloys 7 % to 13 % more.
  • "customer" = the WN bore follows the pipe schedule stated in the order.

Frequently asked questions

What does class 1500 flange (1500#, 1500 lb) mean?

It is the ASME B16.5 pressure class. It is not the pressure in psi: it defines an allowable pressure vs. temperature curve for each material group. In A105 carbon steel, class 1500 allows 255.3 bar from −29 to 38 °C and less as the temperature rises.

Which flange types exist in class 1500?

Weld neck (WN): NPS ½ to 24; Slip-on (SO): NPS ½ to 2½; Socket weld (SW): NPS ½ to 2½; Threaded (TH): NPS ½ to 2½; Lap joint (LJ): NPS ½ to 24; Blind (BL): NPS ½ to 24.

Do the thickness (tf) and length (Y) include the raised face?

No. Since the 2017 edition, tf and Y are measured without the raised face. In class 1500 the standard raised face is 6.4 mm, which is added to the table thickness.

What is the bore (B) of the weld neck flange?

The WN bore follows the pipe wall thickness (schedule). The standard gives the standard-wall (STD) bore only for classes 150 and 300 up to NPS 12; in the other cases the customer states the schedule in the order.

Class 1500 flange in any alloyA105, F316L, F51, F53/F55, F22, Inconel 625 and others, forged and machined at Dustre, with 3.1 certificate.
Request a quote
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)